# US 2013/0252436 A1 · Dielectric thin film, method of manufacturing same, and applications thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252436 A1
- Document ID: US20130252436A1
- Status: Published application
- Kind: A1
- Application number: 13/899,927
- Filed: 2013-05-22
- Published: 2013-09-26
- Earliest claimed: 2007-12-28
- Assignees: Mitsubishi Materials Corporation
- Applicants: Mitsubishi Materials Corporation
- Inventors: Jun Fujii; Hideaki Sakurai; Nobuyuki Soyama
- Web page: https://patentgrep.com/patent/US20130252436A1

## CPC

- H10P 14/69398: {the material having a perovskite structure, e.g. BaTiO3}
- C04B 35/4682: {based on BaTiO3 perovskite phase}
- C23C 18/1216: {Metal oxides (C23C18/1212 takes precedence)}
- H01G 4/1227: {based on alkaline earth titanates}
- H01G 4/33: Thin- or thick-film capacitors {(thin- or thick-film circuits; capacitors without a potential-jump or surface barrier specially adapted for integrated circuits, details thereof, multistep manufacturing processes therefor)}
- H10N 30/077: by liquid phase deposition
- C04B 2235/3213: Strontium oxides or oxide-forming salts thereof
- C04B 2235/6562: Heating rate
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/79: Non-stoichiometric products, e.g. perovskites (ABO3) with an A/B-ratio other than 1
- H10D 1/682: {having dielectrics comprising perovskite structures}
- H10N 30/8536: {Alkaline earth metal based oxides, e.g. barium titanates}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- Y10T 428/268: Monolayer with structurally defined element
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A dielectric thin film and a method of manufacturing the same, wherein the manufacture of a dielectric thin film having a composition represented by Ba1-xSrxTiyO3 (wherein 0≦x≦1 and 0.9≦y≦1.1) includes applying a precursor to the thin film to a substrate and performing drying, and subsequently performing calcination by raising the temperature of the dried thin film at a rate of not more than 30° C./minute, thereby forming a dielectric thin film having an average primary particle size of not less than 70 nm, for which no cracks with a continuous linear length of 1.5 μm or greater exist at the surface of the thin film.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

A method for manufacturing a dielectric thin film having a composition represented by Ba1-xSrxTiyO3 (wherein 0.1≦x≦0.5 and 0.9≦y≦1.1), comprising the steps of:
preparing a precursor solution by dissolving an organic barium compound, an organic strontium compound, and a titanium alkoxide dissolved in an organic solvent such that a molar ratio of Ba:Sr:Ti is (1−x):x:y (wherein 0.1≦x≦0.5 and 0.9≦y≦1.1), and the organic barium compound and the organic strontium compound being metal salts of carboxylic acids represented by a formula CnH2n+1COOH (3≦n≦7);
applying the precursor solution to a substrate to form a coating and drying the coating at a temperature of 150° C. to 400° C.;
repeating the step of applying and drying to form a dried coating; and
performing calcination treatment by heating the dried coating to a temperature of not less than 450° C. and not more than 800° C. at a rate of temperature increase of 5 to 20° C./minute to form the dielectric thin film, which is formed by dielectric crystal particles having an average primary particle size of not less than 70 nm and not more than 300 nm, and
the dielectric thin film having no cracks which have a width of not less than 5 nm and not more than 60 nm and a continuous linear length of 1.5 μm or greater at a surface of the dielectric thin film, and the dielectric thin film having a thickness of not less than 30 nm and not more than 800 nm and a leakage current density of less than 10−1 A/cm2 at a voltage of 20V.

### Claim 14 (depends on 13)

A method for manufacturing a dielectric thin film according to claim 13, further comprising the steps of providing a passivation film on a top of the dielectric thin film.