# US 2013/0252408 A1 · Method for fabricating schottky device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252408 A1
- Document ID: US20130252408A1
- Status: Published application
- Kind: A1
- Application number: 13/894,439
- Filed: 2013-05-15
- Published: 2013-09-26
- Earliest claimed: 2011-11-18
- Assignees: Anpec Electronics Corporation
- Applicants: Anpec Electronics Corporation
- Inventors: Yung-Fa Lin; Shou-Yi Hsu; Meng-Wei Wu; Chia-Hao Chang
- Web page: https://patentgrep.com/patent/US20130252408A1

## CPC

- H10P 32/00: Diffusion of dopants within, into or out of wafers, substrates or parts of devices (during formation of materials H10P14/00)
- H10D 8/051: {of Schottky diodes}
- H10D 8/60: Schottky-barrier diodes
- H10D 64/011: {of electrodes ohmically coupled to a semiconductor}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/212: {Through-implantation}
- H10P 32/1408: {from or through or into an external applied layer, e.g. photoresist or nitride layers}
- H10P 32/1412: {through the applied layer}
- H10P 32/1414: {the applied layer being silicon, silicide or SIPOS, e.g. polysilicon or porous silicon}
- H10P 32/171: {being group IV material}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for fabricating a Schottky device includes the following sequences. First, a substrate with a first conductivity type is provided and an epitaxial layer with the first conductivity type is grown on the substrate. Then, a patterned dielectric layer is formed on the epitaxial layer, and a metal silicide layer is formed on a surface of the epitaxial layer. A dopant source layer with a second conductivity type is formed on the metal silicide layer, followed by applying a thermal drive-in process to diffuse the dopants inside the dopant source layer into the epitaxial layer. Finally, a conductive layer is formed on the metal silicide layer.

## Claims

### Claim 1

A fabricating method of a Schottky device, comprising:
providing a substrate having a first conductivity type;
forming an epitaxial layer on the substrate, wherein the epitaxial layer has the first conductivity type;
forming a patterned dielectric layer on the epitaxial layer;
forming a guard ring of a second conductivity type in the epitaxial layer;
forming a silicide layer on a surface of the epitaxial layer, wherein the silicide layer covers the guard ring;
forming a dopant source layer on the silicide layer, wherein the dopant source layer has a plurality of dopants with the second conductivity type;
performing a thermal drive-in process to diffuse the dopants from the dopant source layer into the epitaxial layer through the silicide layer, thereby forming a doped region of the second conductivity type; and
forming a conductive layer on the silicide layer.

### Claim 2 (depends on 1)

The fabricating method of the Schottky device according to claim 1, wherein the surface of the epitaxial layer comprises at least a lattice defect structure.

### Claim 3 (depends on 2)

The fabricating method of the Schottky device according to claim 2, wherein the lattice defect structure comprises seam defects, void defects, or lattice dislocations.

### Claim 4 (depends on 2)

The fabricating method of the Schottky device according to claim 2, wherein the doped region encompasses the lattice defect structure.

### Claim 5 (depends on 4)

The fabricating method of the Schottky device according to claim 4, wherein a doping concentration of dopants with the second conductivity type in the doped region ranges from 1e14 atoms/cm3 to 1e19 atoms/cm3.

### Claim 6 (depends on 1)

The fabricating method of the Schottky device according to claim 1, further comprising:
forming a buffer layer on the silicide layer before forming the dopant source layer.

### Claim 7 (depends on 6)

The fabricating method of the Schottky device according to claim 6, further comprising:
removing the dopant source layer and the buffer layer after performing the thermal drive-in process.

### Claim 8 (depends on 7)

The fabricating method of the Schottky device according to claim 7, wherein the buffer layer comprises silicon oxide.

### Claim 9 (depends on 1)

The fabricating method of the Schottky device according to claim 1, wherein the first conductivity type is N-type and the second conductivity type is P-type.

### Claim 10 (depends on 1)

The fabricating method of the Schottky device according to claim 1, wherein the silicide layer comprises titanium silicide (TiSi2), nickel silicide (NiSi), platinum silicide (PtSi), molybdenum silicide (MoSi2), or cobalt silicide (CoSi2).

### Claim 11 (depends on 1)

The fabricating method of the Schottky device according to claim 1, wherein the dopant source layer comprises monocrystalline silicon, polycrystalline silicon, amorphous silicon, or borosilicate glass (BSG).

### Claim 12 (depends on 1)

The fabricating method of the Schottky device according to claim 1, wherein the dopants of the second conductivity type comprises boron atoms.

### Claim 13 (depends on 1)

The fabricating method of the Schottky device according to claim 1, wherein the thermal drive-in process comprises rapid thermal process (RTP), spike thermal annealing, laser thermal annealing (LTA), or laser spike annealing, (LSA).

### Claim 14 (depends on 1)

The fabricating method of the Schottky device according to claim 1, wherein the conductive layer comprises titanium, nickel, gold, aluminum, or a combination thereof.