# US 2013/0252392 A1 · Performing Enhanced Cleaning in the Formation of MOS Devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252392 A1
- Document ID: US20130252392A1
- Status: Published application
- Kind: A1
- Application number: 13/427,628
- Filed: 2012-03-22
- Published: 2013-09-26
- Earliest claimed: 2012-03-22
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Yu-Hung Cheng; Wu-Ping Huang; Chii-Horng Li; Tze-Liang Lee
- Web page: https://patentgrep.com/patent/US20130252392A1

## CPC

- H10P 70/20: {Cleaning during device manufacture}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 84/0128: {Manufacturing their channels}
- H10D 84/0133: {Manufacturing common source or drain regions between multiple IGFETs}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/2925: {Surface structures}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3602: {In-situ cleaning}
- H10P 50/242: {of Group IV materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method includes etching a semiconductor substrate to form a recess, wherein the recess extends from a top surface of the semiconductor substrate into the semiconductor substrate. An enhanced cleaning is then performed to etch exposed portions of the semiconductor substrate. The exposed portions are in the recess. The enhanced cleaning is performed using process gases including hydrochloride (HCl) and germane (GeH4). After the enhanced cleaning, an epitaxy is performed to grow a semiconductor region in the recess.

## Claims

### Claim 1

A method comprising:
etching a semiconductor substrate to form a recess, wherein the recess extends from a top surface of the semiconductor substrate into the semiconductor substrate;
performing an enhanced cleaning to etch exposed portions of the semiconductor substrate, wherein the exposed portions are in the recess, and wherein the enhanced cleaning is performed using process gases comprising hydrochloride (HCl) and germane (GeH4); and
after the enhanced cleaning, performing an epitaxy to grow a semiconductor region in the recess.

### Claim 2 (depends on 1)

The method of claim 1, wherein the enhanced cleaning comprises an etching and a deposition simultaneously, and wherein the enhanced cleaning has a net effect of etching.

### Claim 3 (depends on 1)

The method of claim 1, wherein after the step of etching the semiconductor substrate and before the enhanced cleaning, the semiconductor substrate has a (111) surface in the recess, and wherein after the enhanced cleaning, a portion of the semiconductor substrate having the (111) surface is etched to generate a surface parallel to the top surface of the semiconductor substrate.

### Claim 4 (depends on 1)

The method of claim 1, wherein the enhanced cleaning and the epitaxy are in-situ performed in a same process chamber.

### Claim 5 (depends on 1)

The method of claim 1, wherein the process gases for the enhanced cleaning further comprises a process gas selected from the group consisting essentially of Dichloro-Silane (DCS), silane (SiH4), methylsilane (SiCH6), and combinations thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the recess is adjacent to a gate electrode and a gate dielectric under the gate electrode, wherein the gate dielectric is over the semiconductor substrate, and wherein after the enhanced cleaning, a top point of a surface of the semiconductor substrate in the recess is substantially aligned to an edge of the gate electrode, and wherein the top point is substantially level with a bottom surface of the gate dielectric.

### Claim 7 (depends on 1)

The method of claim 1, wherein the recess is between opposite sidewalls of two Shallow Trench Isolation (STI) Regions, and wherein before the enhanced cleaning, the recess comprises a (111) bottom surface not parallel to the top surface of the semiconductor substrate, and wherein after the enhanced cleaning, substantially an entirety of bottom surface of the recess is planar, and is parallel to the top surface of the semiconductor substrate.

### Claim 8

A method comprising:
forming a gate stack over a top surface of a semiconductor substrate;
etching a portion of the semiconductor substrate adjacent to the gate stack to form a recess, wherein the recess comprises a (111) bottom surface contacting a Shallow Trench Isolation (STI) region, with the (111) bottom surface being a surface of a portion of the semiconductor substrate;
after the step of etching, performing an enhanced cleaning on the semiconductor substrate, wherein during the enhanced cleaning, a portion of the semiconductor substrate having the (111) bottom surface is removed to generate a surface parallel to the top surface of a semiconductor substrate; and
after the enhanced cleaning, performing an epitaxy to grow a semiconductor region in the recess.

### Claim 9 (depends on 8)

The method of claim 8, wherein the enhanced cleaning is performed using process gases comprising hydrochloride (HCl) and germane (GeH4).

### Claim 10 (depends on 9)

The method of claim 9, wherein the process gases for the enhanced cleaning further comprises a process gas selected from the group consisting essentially of Dichloro-Silane (DCS), silane (SiH4), methylsilane (SiCH6), and combinations thereof.

### Claim 11 (depends on 8)

The method of claim 8, wherein the enhanced cleaning and the epitaxy are in-situ performed in a same process chamber.

### Claim 12 (depends on 8)

The method of claim 8 further comprises:
during the step of etching the portion of the semiconductor substrate, simultaneously etching an addition portion of the semiconductor substrate between opposite sidewalls of two Shallow Trench Isolation (STI) regions to form an additional recess, wherein the opposite sidewalls are exposed to the additional recess, wherein the semiconductor substrate comprises a (111) bottom surface in the additional recess, and wherein after the enhanced cleaning, substantially an entirety of the bottom surface of the additional recess is planar and parallel to the top surface of the semiconductor substrate.

### Claim 13 (depends on 8)

The method of claim 8, wherein the enhanced cleaning is performed in a process chamber configured to perform a Low-Pressure Chemical Vapor Deposition (LPCVD).

### Claim 14

A method comprising:
etching a semiconductor substrate having a top surface to form a recess in the semiconductor substrate;
performing an enhanced cleaning in a process chamber to etch a portion of the semiconductor substrate, wherein the portion of the semiconductor substrate is in the recess, and wherein the enhanced cleaning is performed using process gases comprising hydrochloride (HCl) and germane (GeH4); and
after the enhanced cleaning, performing an epitaxy to grow a semiconductor region in the recess, wherein the epitaxy is in-situ performed in the process chamber.

### Claim 15 (depends on 14)

The method of claim 14, wherein the process gases for the enhanced cleaning further comprises a process gas selected from the group consisting essentially of Dichloro-Silane (DCS), silane (SiH4), methylsilane (SiCH6), and combinations thereof.

### Claim 16 (depends on 15)

The method of claim 15, wherein the enhanced cleaning is performed with a first Etching-to-Growth (E/G) ratio, wherein the epitaxy is performed with a second E/G ratio, and wherein the first and the second E/G ratios are calculated using an equation:
E/G=FRHCl/(FRDCS+100×FRGeH4)
wherein FRHCl, FRDCS, and FRGeH4 are flow rates of HCl, DCS, and GeH4, respectively, and wherein the first E/G ratio is greater than 1, and the second E/G ratio is lower than 1.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first E/G ratio is greater than about 1.5.

### Claim 18 (depends on 14)

The method of claim 14, wherein after the step of etching the semiconductor substrate and before the enhanced cleaning, the semiconductor substrate has a (111) bottom surface in the recess, and wherein after the enhanced cleaning, a portion of the semiconductor substrate having the (111) surface is etched to generate a surface parallel to the top surface of the semiconductor substrate.

### Claim 19 (depends on 14)

The method of claim 14, wherein the enhanced cleaning and the epitaxy are performed with no vacuum break therebetween.

### Claim 20 (depends on 14)

The method of claim 14, wherein the recess is adjacent to a gate electrode and a gate dielectric under the gate electrode, wherein the gate dielectric is over the semiconductor substrate, and wherein after the enhanced cleaning, a top point of a surface of the semiconductor substrate in the recess is substantially aligned to an edge of the gate electrode, and wherein the top point is substantially level with a bottom surface of the gate dielectric.