# US 2013/0252370 A1 · Method of manufacturing semiconductor light-receiving element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252370 A1
- Document ID: US20130252370A1
- Status: Published application
- Kind: A1
- Application number: 13/838,241
- Filed: 2013-03-15
- Published: 2013-09-26
- Earliest claimed: 2012-03-22
- Assignees: Sumitomo Electric Device Innovations, Inc.
- Applicants: Sumitomo Electric Device Innovations, Inc.
- Inventors: Yuji Koyama
- Web page: https://patentgrep.com/patent/US20130252370A1

## CPC

- H10H 20/856: Reflecting means
- H10F 10/17: Photovoltaic cells having only PIN junction potential barriers
- H10F 30/223: the potential barrier being a PIN barrier
- H10F 77/241: {comprising ring electrodes}
- H10F 77/413: {directly associated or integrated with the devices, e.g. back reflectors (directly associated or integrated with photovoltaic cells H10F77/42)}
- H10F 77/48: Back surface reflectors [BSR]
- H10F 77/484: {Refractive light-concentrating means, e.g. lenses}
- H10F 77/63: Arrangements for cooling directly associated or integrated with photovoltaic cells, e.g. heat sinks directly associated with the photovoltaic cells or integrated Peltier elements for active cooling
- H10F 77/90: Energy storage means directly associated or integrated with photovoltaic cells, e.g. capacitors integrated with photovoltaic cells
- Y02E 10/52: PV systems with concentrators
- Y02E 10/548: Amorphous silicon PV cells
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of manufacturing a semiconductor light-receiving element includes: forming a semiconductor layer structure having a one-conductivity-type semiconductor layer having a first conduction type located on a side of light incidence, an opposite-conductivity-type semiconductor layer having a second conduction type opposite to the first conduction type, and a light-absorbing layer between the one-conductivity-type semiconductor layer and the opposite-conductivity type semiconductor layer, the opposite-conductivity-type semiconductor layer having a structure in which a first semiconductor layer comprised of a binary mixed crystal, a second semiconductor layer comprised of a three-or-more-element mixed crystal, and a third semiconductor layer comprised of a three-or-more-element mixed crystal having an energy gap smaller than that of the second semiconductor layer are laminated in this order from the light incidence side; forming a metal film that is in contact with the third semiconductor layer; and performing a thermal process after the forming of the metal film.

## Claims

### Claim 1

A method of manufacturing a semiconductor light-receiving element comprising:
forming a semiconductor layer structure having a one-conductivity-type semiconductor layer having a first conduction type located on a side of light incidence, an opposite-conductivity-type semiconductor layer having a second conduction type opposite to the first conduction type, and a light-absorbing layer between the one-conductivity-type semiconductor layer and the opposite-conductivity type semiconductor layer,
the opposite-conductivity-type semiconductor layer having a structure in which a first semiconductor layer comprised of a binary mixed crystal, a second semiconductor layer comprised of a three-or-more-element mixed crystal, and a third semiconductor layer comprised of a three-or-more-element mixed crystal having an energy gap smaller than that of the second semiconductor layer are laminated in this order from the light incidence side;
forming a metal film that is in contact with the third semiconductor layer; and
performing a thermal process after the forming of the metal film.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein:
the first semiconductor layer is comprised of InP;
the second semiconductor layer is comprised of InGaAsP; and
the third semiconductor layer is comprised of InGaAs.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein the metal layer is formed by laminating gold, zinc and gold in this order from the third semiconductor layer side.

### Claim 4 (depends on 3)

The method as claimed in claim 3, wherein a temperature range of the thermal process is 350 degrees C. to 400 degrees C.

### Claim 5

A method of manufacturing a semiconductor light-receiving element comprising:
growing a one-conductivity-type semiconductor layer having a first conduction type, a light-absorbing layer and an opposite-conductivity type semiconductor layer having a second conduction type opposite to the first conduction type, in this order from a light incidence side;
forming an insulating film on the opposite-conductivity-type semiconductor layer;
forming a selective etching mask on a face of the insulating film;
forming a concave and convex portion on the face of the insulating film by performing an etching against a part or all of a thickness of the insulating film exposed through the selective etching mask; and
forming a metal film on the face of the insulating film including the concave and convex portion.

### Claim 6

A method of manufacturing a semiconductor light-receiving element comprising:
growing a one-conductivity-type semiconductor layer having a first conduction type, a light-absorbing layer, and an opposite-conductivity-type semiconductor layer having a second conduction type opposite to the first conduction type, in this order;
forming an insulating film on the opposite-conductivity-type semiconductor layer;
enlarging a concave and convex portion of the insulating film in a face subjected to an etching compared to before the etching, by performing the etching to the insulating film; and
forming a metal film on a face of the insulating film including the concave and convex portion.

### Claim 7 (depends on 5)

The method as claimed in claim 5 wherein the insulating film is silicon nitride.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the semiconductor light-receiving element is a back-face-incident-type light-receiving element.

### Claim 9 (depends on 6)

The method as claimed in claim 6 wherein the insulating film is silicon nitride.

### Claim 10 (depends on 5)

The method as claimed in claim 5, wherein the semiconductor light-receiving element is a back-face-incident-type light-receiving element.

### Claim 11 (depends on 6)

The method as claimed in claim 6, wherein the semiconductor light-receiving element is a back-face-incident-type light-receiving element.

### Claim 12 (depends on 1)

The method as claimed in claim 1 further comprising forming an extracting electrode on the metal film and on a dummy mesa.

### Claim 13 (depends on 5)

The method as claimed in claim 5 further comprising forming an extracting electrode on the metal film and on a dummy mesa.

### Claim 14 (depends on 6)

The method as claimed in claim 6 further comprising forming an extracting electrode on the metal film and on a dummy mesa.

### Claim 15 (depends on 8)

The method as claimed in claim 8, wherein:
the one-conductivity-type semiconductor layer is formed on a one-conductivity-type semiconductor substrate; and
the method further comprises forming a lens by performing a milling against the one-conductivity-type semiconductor substrate.

### Claim 16 (depends on 10)

The method as claimed in claim 10, wherein:
the one-conductivity-type semiconductor layer is formed on a one-conductivity-type semiconductor substrate; and
the method further comprises forming a lens by performing a milling against the one-conductivity-type semiconductor substrate.

### Claim 17 (depends on 11)

The method as claimed in claim 11, wherein:
the one-conductivity-type semiconductor layer is formed on a one-conductivity-type semiconductor substrate; and
the method further comprises forming a lens by performing a milling against the one-conductivity-type semiconductor substrate.

### Claim 18 (depends on 5)

The method as claimed in claim 5, wherein at least one of faces of the concave and convex portion is formed so as to be inclined with respect to the light incidence, in the forming of the concave and convex portion.

### Claim 19 (depends on 6)

The method as claimed in claim 6, wherein at least one of faces of the concave and convex portion is formed so as to be inclined with respect to the light incidence, in the forming of the concave and convex portion.