# US 2013/0252369 A1 · Enhanced lift-off techniques for use when fabricating light sensors including dielectric optical coating filters

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252369 A1
- Document ID: US20130252369A1
- Status: Published application
- Kind: A1
- Application number: 13/530,675
- Filed: 2012-06-22
- Published: 2013-09-26
- Earliest claimed: 2012-03-20
- Assignees: Intersil Americas Inc.
- Inventors: Eric S. Lee; Michael I-Shan Sun; Francois Hebert
- Web page: https://patentgrep.com/patent/US20130252369A1

## CPC

- H10F 77/413: {directly associated or integrated with the devices, e.g. back reflectors (directly associated or integrated with photovoltaic cells H10F77/42)}
- H10F 30/21: the devices being sensitive to infrared, visible or ultraviolet radiation
- H10F 30/221: the potential barrier being a PN homojunction
- H10F 71/134: {Irradiation with electromagnetic or particle radiation}
- H10F 77/331: {for filtering or shielding light, e.g. multicolour filters for photodetectors}
- H10P 76/202: {for lift-off processes}
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Light sensors including dielectric optical coatings to shape their spectral responses, and methods for fabricating such light sensors in a manner that accelerates lift-off processes and increases process margins, are described herein. In certain embodiments, a short duration soft bake is performed. Alternatively, or additionally, temperature cycling is performed. Alternatively, or additionally, photolithography is performed using a photomask that includes one or more dummy corners, dummy islands and/or dummy rings. Each of the aforementioned embodiments form and/or increase a number of micro-cracks in the dielectric optical coating not covering the photodetector sensor region, thereby enabling an accelerated lift-off process and an increased process margin. Alternatively, or additionally, a portion of the photomask can include chamfered corners so that the dielectric optical coating includes chamfered corners, which improves the thermal reliability of the dielectric optical coating.

## Claims

### Claim 1

A method for fabricating a light sensor, comprising:
(a) covering a surface of a semiconductor substrate, which includes a photodetector sensor region, with photoresist having a softening point (Tsoft);
(b) using photolithography to define a pattern in the photoresist;
(c) using a developer, removing a portion of the photoresist that covered the photodetector sensor region and covered a circumferential region surrounding the photodetector sensor region;
(d) depositing a dielectric optical coating over the photodetector sensor region, over the circumferential region, and over the photoresist not covering the photodetector sensor region that remained after the removing at step (c);
(e) performing a short duration soft bake at a temperature (Tsoft—bake) within a predetermined range of the softening point (Tsoft) of the photoresist to thereby form and/or increase a number of micro-cracks in the dielectric optical coating not covering the photodetector sensor region; and
(f) lifting off a portion of the dielectric optical coating that is over the remaining photoresist not covering the photodetector sensor region, so that a remaining portion of the dielectric optical coating covers the photodetector sensor region and the circumferential region.

### Claim 2 (depends on 1)

The method of claim 1, wherein the short duration soft bake performed at step (e) is performed for 15 minutes or less.

### Claim 3 (depends on 1)

The method of claim 1, wherein the short duration soft bake performed at step (e) is performed for between about 30 and 60 seconds.

### Claim 4 (depends on 1)

The method of claim 1, wherein the predetermined range of the softening point (Tsoft) of the photoresist is +/−10 degrees Celsius of the softening point (Tsoft).

### Claim 5 (depends on 1)

The method of claim 1, wherein the predetermined range of the softening point (Tsoft) of the photoresist includes the softening point (Tsoft) and temperatures that are up to 10 degrees Celsius greater than the softening point (Tsoft), inclusive.

### Claim 6 (depends on 1)

The method of claim 1, wherein step (f) comprises performing a chemical solvent soak for no more than one hour.

### Claim 7 (depends on 1)

The method of claim 1, wherein step (f) comprises performing a chemical solvent soak for between about 15 to 30 minutes.

### Claim 8

A method for fabricating a light sensor, comprising:
(a) covering a surface of a semiconductor substrate, which includes a photodetector sensor region;
(b) using photolithography to define a pattern in the photoresist;
(c) using a developer, removing a portion of the photoresist that covered the photodetector sensor region and covered a circumferential region surrounding the photodetector sensor region;
(d) depositing a dielectric optical coating over the photodetector sensor region, over the circumferential region, and over the photoresist not covering the photodetector sensor region that remained after the removing at step (c);
(e) repetitively cycling back and forth between at least two temperatures T1 and T2, where the temperature T2 is between about 50 and 150 degrees Celsius greater than the temperature T1, to thereby form and/or increase a number of micro-cracks in the dielectric optical coating not covering the photodetector sensor region; and
(f) lifting off a portion of the dielectric optical coating that is over the remaining photoresist not covering the photodetector sensor region, so that a remaining portion of the dielectric optical coating covers the photodetector sensor region and the circumferential region.

### Claim 9 (depends on 8)

The method of claim 8, wherein:
the temperature T1 is within the range of about 0 to 50 degrees Celsius; and
the temperature T2 is within the range of about 100 to 150 degrees Celsius.

### Claim 10 (depends on 8)

The method of claim 8, wherein the temperature T2 is at least 90 degrees Celsius greater than the temperature T2.

### Claim 11 (depends on 8)

The method of claim 8, wherein the temperature T2 between about 90 and 120 degrees Celsius greater than the temperature T1.

### Claim 12 (depends on 8)

The method of claim 8, wherein:
step (e) is performed within an oven; and
during the repetitively cycling back and forth between the at least two temperatures T1 and T2 at step (e), the temperature of the oven remains at one of the two temperatures T1 and T2 for at least 10 seconds before transitioning to another one of the temperatures T1 and T2.

### Claim 13 (depends on 8)

The method of claim 8, wherein the repetitively cycling back and forth between the at least two temperatures T1 and T2 at step (e) is performed for 15 minutes or less.

### Claim 14 (depends on 8)

The method of claim 8, wherein the repetitively cycling back and forth between the at least two temperatures T1 and T2 at step (e) is performed for between about 1 and 2 minutes.

### Claim 15 (depends on 8)

The method of claim 8, wherein step (f) comprises performing a chemical solvent soak for no more than one hour.

### Claim 16 (depends on 8)

The method of claim 8, wherein step (f) comprises performing a chemical solvent soak for between about 15 to 30 minutes.