# US 2013/0252365 A1 · Solid state lighting devices grown on semi-polar facets and associated methods of manufacturing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252365 A1
- Document ID: US20130252365A1
- Status: Published application
- Kind: A1
- Application number: 13/897,922
- Filed: 2013-05-20
- Published: 2013-09-26
- Earliest claimed: 2010-03-09
- Assignees: Micron Technology, Inc.
- Applicants: Micron Technology, Inc.
- Inventors: Lifang Xu; Zaiyuan Ren
- Web page: https://patentgrep.com/patent/US20130252365A1

## CPC

- H10H 20/825: containing nitrogen, e.g. GaN
- H10H 20/817: characterised by the crystal structures or orientations, e.g. polycrystalline, amorphous or porous
- H10H 20/821: of the light-emitting regions, e.g. non-planar junctions
- H10H 20/819: characterised by their shape, e.g. curved or truncated substrates
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

Solid state lighting devices grown on semi-polar facets and associated methods of manufacturing are disclosed herein. In one embodiment, a solid state light device includes a light emitting diode with an N-type gallium nitride (“GaN”) material, a P-type GaN material spaced apart from the N-type GaN material, and an indium gallium nitride (“InGaN”)/GaN multi quantum well (“MQW”) active region directly between the N-type GaN material and the P-type GaN material. At least one of the N-type GaN, InGaN/GaN MQW, and P-type GaN materials is grown a semi-polar sidewall.

## Claims

### Claim 1

A method for forming a light emitting diode, comprising:
forming a foundation on a support surface of a microelectronic substrate;
initiating a deposition of a semiconductor material on the microelectronic substrate, the semiconductor material having a semiconductor surface spaced apart from the support surface;
adjusting an operating parameter during the deposition the semiconductor material;
forming a sidewall along a semi-polar crystal plane of the semiconductor material with the adjusted operating parameter; and
forming an active region in direct contact with the sidewall of the semiconductor material.

### Claim 2 (depends on 1)

The method of claim 1 wherein:
forming the foundation includes forming a plurality of foundations containing SiO2 on the support surface, two of the adjacent foundations being spaced apart from each other by an open region; and
initiating the deposition includes depositing an N-type GaN material in the open region between two of the adjacent foundations.

### Claim 3 (depends on 1)

The method of claim 1 wherein:
forming the foundation includes forming a plurality of foundations containing SiO2 on the support surface, two of the adjacent foundations being spaced apart from each other by an open region;
initiating the deposition includes depositing an N-type GaN material in the open region between two of the adjacent foundations; and
adjusting the operating parameter includes adjusting at least one of a size of the foundations, a direction of the foundations, a material of the foundations, a fill factor of the foundations, a deposition ambient condition, a depositing temperature, a deposition pressure, and a deposition time period.

### Claim 4 (depends on 1)

The method of claim 1 wherein:
forming the foundation includes forming a plurality of foundations containing SiO2 on the support surface, two of the adjacent foundations being spaced apart from each other by an open region;
initiating the deposition includes:
depositing an N-type GaN material in the open region between two of the adjacent foundations; and
forming a first portion of the N-type GaN material with a triangular shape; and
adjusting the operating parameter includes:
adjusting at least one of a deposition ambient condition, a depositing temperature, a deposition pressure, and a deposition time period to promote lateral growth; and
forming a second portion of the N-type GaN material via lateral growth.

### Claim 5 (depends on 1)

The method of claim 1 wherein:
forming the foundation includes forming a plurality of foundations containing SiO2 on the support surface, two of the adjacent foundations being spaced apart from each other by an open region;
initiating the deposition includes:
depositing an N-type GaN material in the open region between two of the adjacent foundations; and
forming a first portion of the N-type GaN material with a triangular shape with a first semi-polar plane;
adjusting the operating parameter includes:
adjusting at least one of a deposition ambient condition, a depositing temperature, a deposition pressure, and a deposition time period to promote lateral growth; and
forming a second portion of the N-type GaN material via lateral growth, thereby forming a second semi-polar plane generally parallel to the first semi-polar plane; and
forming the active region includes depositing InGaN/GaN MQW on the second semi-polar plane.

### Claim 6 (depends on 1)

The method of claim 1 wherein:
forming the foundation includes forming a plurality of foundations containing SiO2 on the support surface, two of the adjacent foundations being spaced apart from each other by an open region;
initiating the deposition includes:
depositing an N-type GaN material in the open region between two of the adjacent foundations; and
forming a first portion of the N-type GaN material with a triangular shape with a first semi-polar plane;
adjusting the operating parameter includes:
adjusting at least one of a deposition ambient condition, a depositing temperature, a deposition pressure, and a deposition time period to promote lateral growth; and
forming a second portion of the N-type GaN material via lateral growth, thereby forming a second semi-polar plane generally parallel to the first semi-polar plane and covering at least a portion of the foundations; and
forming the active region includes depositing InGaN/GaN MQW on the second semi-polar plane.