# US 2013/0252167 A1 · Toner

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252167 A1
- Document ID: US20130252167A1
- Status: Published application
- Kind: A1
- Application number: 13/991,348
- Filed: 2011-12-13
- Published: 2013-09-26
- Earliest claimed: 2010-12-28
- Assignees: Canon Kabushiki Kaisha
- Inventors: Shuhei Moribe; Katsuhisa Yamazaki; Daisuke Yoshiba; Toru Takahashi; Daisuke Tsujimoto; Masami Fujimoto
- Web page: https://patentgrep.com/patent/US20130252167A1

## CPC

- G03G 9/08755: {Polyesters}
- G03G 9/08702: {comprising macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds}
- G03G 9/08788: {Block polymers}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A toner comprising toner particles, each of which contains a binder resin and a colorant, wherein the binder resin includes a resin having an endothermic peak at a temperature of 55° C. to 120° C. in a DSC curve; the toner has a softening point Tm of 90° C. to 140° C.; in the viscoelastic characteristic of the toner measured at a frequency of 6.28 rad/sec, the storage elastic modulus at a temperature of 180° C. is 1.0×102 Pa to 1.0×104 Pa; in a chart with the temperature on the x-axis and tan δ on the y-axis, tan δ has a peak having a peak top in the range of 50° C. to 70° C.; tan δ (P) at the peak top temperature is 2.0 to 10.0; the ratio of the tan δ (P) at the peak top temperature to tan δ (Tm) at a temperature of Tm (tan δ (P)/tan δ (Tm)) is in the range of 2.5 to 8.0.

## Claims

### Claim 1

A toner comprising toner particles, each of which contains a binder resin and a colorant, wherein
the binder resin comprises a resin having an endothermic peak at a temperature of not less than 55° C. but not more than 120° C. in a DSC curve measured by a differential scanning calorimeter,
a softening point Tm of the toner is not less than 90° C. but not more than 140° C., and wherein
in a viscoelastic characteristic of the toner measured at a frequency of 6.28 rad/sec,
i) a storage elastic modulus at a temperature of 180° C. (G′180) is not less than 1.0×102 Pa but not more than 1.0×104 Pa,
ii) in a chart with a temperature on an x-axis and a loss tangent tan δ on a y-axis,
a) tan δ has at least one peak having a peak top in the temperature range of not less than 50° C. but not more than 70° C.,
b) tan δ (P) is not less than 2.0 but not more than 10.0 wherein a loss tangent at a peak top temperature that gives the peak top of the peak is tan δ (P), and
c) a ratio of tan δ (P) to tan δ (Tm) (tan δ (P)/tan δ (Tm)) is in the range of not less than 2.5 but not more than 8.0 wherein a loss tangent at a softening point Tm of the toner is tan δ (Tm).

### Claim 2 (depends on 1)

The toner according to claim 1, wherein the binder resin has a binder resin (A) and a binder resin (B) each having a different softening point,
the binder resin (A) has a softening point TA (° C.), the binder resin (B) has a softening point TB (° C.),
the softening point TA (° C.) is lower than the softening point TB (° C.), and the softening point TA (° C.) is not less than 70° C. but not more than 100° C., and
the binder resin (A) has an endothermic peak at a temperature not less than 55° C. but not more than 120° C. in a DSC curve measured by a differential scanning calorimeter.

### Claim 3 (depends on 1)

The toner according to claim 1, wherein the binder resin (B) is a hybrid resin of a polyester unit chemically bonded to a vinyl copolymerization unit.

### Claim 4 (depends on 2)

The toner according to claim 2, wherein the binder resin (B) is a hybrid resin of a polyester unit chemically bonded to a vinyl copolymerization unit.