# US 2013/0252138 A1 · Pt/graphene catalyst, preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252138 A1
- Document ID: US20130252138A1
- Status: Published application
- Kind: A1
- Application number: 13/990,154
- Filed: 2010-12-29
- Published: 2013-09-26
- Earliest claimed: 2010-12-29
- Assignees: Ocean's King Lighting Science & Technology Co., Ltd.
- Inventors: Mingjie Zhou; Linglong Zhong; Yaobing Wang
- Web page: https://patentgrep.com/patent/US20130252138A1

## CPC

- H01M 4/926: {on carbon or graphite}
- B01J 21/18: Carbon
- B01J 23/42: Platinum
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/0207: {Pretreatment of the support}
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A Pt/graphene catalyst comprises graphene as carrier, and Pt loaded on the graphene. The use of graphene as carrier for the catalyst takes advantage of the ion effect and two-dimensional ductility of graphene, which increases the stability of the catalyst. The catalyst is prepared by a reverse micelles system method which provides a micro-environment (i.e. water-in-oil microemulsion), so that the particle size of the resulting nano-particles can be regulated easily and is more uniformly distributed. The use of the catalyst in electrochemostry is also disclosed.

## Claims

### Claim 1

A preparation method of a Pt/graphene catalyst, comprising the steps of:
performing an oxidation reaction with graphite power according to a Hummers method to obtain graphite oxide;
adding the graphite into water and then ultrasonically dispersing to form a graphene oxide solution with uniformly dispersed monolithic layer;
preparing a reverse micellar system containing surfactant, co-surfactant, oil phase, and chloroplatinic acid aqueous solution at room temperature;
adding the graphite oxide solution into the reverse micellar system dropwise, and adding catalyst dropwise to perform a reduction reaction under a water bath heating condition to obtain an emulsion containing Pt and graphene;
adding demulsifier into the emulsion dropwise to load Pt on the graphene carrier; and
filtering, washing, and drying the graphene loaded with the Pt to obtain the Pt/graphene catalyst.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein the steps of preparing the graphite oxide comprises:
adding graphite powder, potassium persulfate and phosphrous pentoxide into a concentrated sulfuric acid at a temperature of 80° C., stirring uniformly and cooling for more than six hours, washing to neutral, drying to obtain a sample;
adding the dried sample into 200 to 250 mL of concentrated sulfuric acid, then adding potassium permanganate, heat preserving at a temperature of 0 to 20° C. for 5 to 60 minutes, maintaining at a temperature of 35° C. in an oil bath for 1 to 2 hours, slowly adding deionized water containing hydrogen peroxide to obtain a mixture; and
hot filtrating the mixture when the color of the mixture becomes bright yellow, washing with hydrochloric acid and then filtering, drying under vacuum condition at a temperature of 60° C. for 48 hours to obtain the graphite oxide.

### Claim 3 (depends on 2)

The preparation method according to claim 2, wherein the mass ratio of the graphite powder, the potassium persulfate and the phosphrous pentoxide is 2:1:1.

### Claim 4 (depends on 2)

The preparation method according to claim 2, wherein an adding amount of the potassium permanganate is 3 times of the adding amount of the graphite powder, the concentration of the hydrogen peroxide is wt. 30%.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein the surfactant is selected from the group consisting of methyl benzene sulfonate, sodium dodecylbenzene sulfonate, aliphatic sulfate and aliphatic quaternary ammonium salts; the co-surfactant is selected from the group consisting of n-octanol, n-nonyl alcohol, n-heptanol, and n-hexyl alcohol; the oil phase is cyclohexane; the molar concentration of the chloroplatinic acid aqueous solution is 0.04 mol/L; the mass ratio of the surface active agent, the cosurfactant, and the oil phase is 10:7:1.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein in the emulsion containing Pt and graphene, the mass ratio of Pt to graphene is 1:10.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein the reducing agent is hydrazine hydrate or sodium borohydride, the using amount of reducing agent is 3 to 10 times of the amount of chloroplatinic acid.

### Claim 8 (depends on 1)

The preparation method according to claim 1, wherein the demulsifier is acetone or ethanol.

### Claim 9 (depends on 1)

A Pt/graphene catalyst, being prepared according to claim 1, wherein graphene is a carrier, and Pt is loaded on the graphene.

### Claim 10 (depends on 9)

A proton exchange membrane fuel cell, comprising the Pt/graphene catalyst according to claim 9.