# US 2013/0252135 A1 · Pt-ru nano-alloy/graphene catalyst, preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252135 A1
- Document ID: US20130252135A1
- Status: Published application
- Kind: A1
- Application number: 13/990,129
- Filed: 2010-12-29
- Published: 2013-09-26
- Earliest claimed: 2010-12-29
- Inventors: Mingjie Zhou; Linglong Zhong; Yaobing Wang
- Web page: https://patentgrep.com/patent/US20130252135A1

## CPC

- H01M 4/8657: {layered}
- H01M 4/88: Processes of manufacture
- H01M 4/921: {Alloys or mixtures with metallic elements}
- H01M 4/926: {on carbon or graphite}
- H01M 8/1018: Polymeric electrolyte materials
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/10: Energy storage using batteries
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A Pt—Ru nano-alloy/graphene catalyst comprises graphene as a support, and a Pt—Ru nano-alloy loaded on the graphene. The use of graphene as support for the catalyst takes advantage of the ion effect and tow-dimensional ductility of graphene, which increase the stability of the catalyst. The catalyst is prepared by a reverse micelles system method which provides a micro-environment (i.e. water-in-oil microemulsion), so that the particle size of the resulting nano-alloy particles can be regulated easily and is more uniformly distributed. The use of the catalyst in electrochemistry is also disclosed.

## Claims

### Claim 1

A preparation method of a Pt—Ru nano-alloy/graphene catalyst, comprising the following steps:
oxidizing graphite powder to obtain a graphite oxide according to a Hummers method;
adding the graphite oxide to water, forming a graphene oxide solution with uniform dispersion of monolithic layer after ultrasonic dispersion;
preparing a reverse micellar system containing a surfactant, a cosurfactant, an oil phase, a chloroplatinic acid, and a ruthenium chloride aqueous solution at room temperature;
adding the graphene oxide solution to the reverse micelle system dropwise, and adding a reducing agent dropwise in a water bath, performing a reduction reaction to obtain an emulsion containing Pt—Ru nano-alloy and graphene;
adding a demulsifier to the emulsion dropwise, and loading the Pt—Ru nano-alloy on a carrier of the graphene; and
filtering, washing, drying the graphene loaded with Pt—Ru nano-alloy to obtain the Pt—Ru nano-alloy/graphene catalyst.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein in the step of preparing the graphite oxide, comprising the following steps:
adding the graphite powder, a potassium persulfate and a phosphorus pentoxide to a concentrated sulfuric acid at a temperature of 80° C., and stirring uniformly, cooling, washing to neutral, and drying to obtain a sample;
adding the dried sample to 200 mL to 250 mL of concentrated sulfuric acid at a temperature of 0° C., and then adding a potassium permanganate, and heat preserving for 5 to 60 minutes at a temperature from 0° C. to 20° C., then maintaining for 1 to 2 hours in an oil bath at a temperature of 35° C., then slowly adding to deionized water containing a hydrogen peroxide to obtain a mixed solution; and
hot filtering the mixed solution when the color of the mixed solution becomes bright yellow, washing with hydrochloric acid, filtering, drying to obtain the graphite oxide.

### Claim 3 (depends on 2)

The preparation method according to claim 2, wherein a mass ratio of the graphite powder, the potassium persulfate and the phosphorus pentoxide is 2:1:1.

### Claim 4 (depends on 2)

The preparation method according to claim 2, wherein a mass of the potassium permanganate is 3 times of a mass of the graphite powder; a mass percentage concentration of the hydrogen peroxide is 30%.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein the surfactant is selected from the group consisting of sodium benzenesulfonate, sodium dodecyl benzenesulfonate, aliphatic sulfate and aliphatic quaternary ammonium salt; the cosurfactant is selected from the group consisting n-octanol, n-nonyl alcohol, n-heptanol and n-hexyl alcohol; the oil phase is cyclohexane; a molar concentration of the chloroplatinic acid is 0.04 mol/L, a molar concentration of the ruthenium chloride aqueous solution is 0.04 mol/L; a mass ratio of the surfactant, the cosurfactant and the oil phase is 10:7:1.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein a mass ratio of the Pt—Ru nano-alloy and the graphene in the emulsion containing Pt—Ru nano-alloy and graphene is 1:10.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein the reducing agent is hydrazine hydrate or sodium borohydride, a molar amount of the reducing agent is 3 to 10 times of a molar amount of the chloroplatinic acid.

### Claim 8 (depends on 1)

The preparation method according to claim 1, wherein the demulsifier is acetone or anhydrous ethanol.

### Claim 9 (depends on 1)

A Pt—Ru nano-alloy/graphene catalyst, prepared according to the preparation method of claim 1, wherein the graphene is a carrier, the Pt—Ru nano-alloy is loaded on the graphene.

### Claim 10 (depends on 9)

A proton exchange membrane fuel cell, comprising the Pt—Ru nano-alloy/graphene catalyst provided according to claim 9.