# US 2013/0252108 A1 · Metal-doped nickel oxide active materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252108 A1
- Document ID: US20130252108A1
- Status: Published application
- Kind: A1
- Application number: 13/425,587
- Filed: 2012-03-21
- Published: 2013-09-26
- Earliest claimed: 2012-03-21
- Assignees: The Gillette Company
- Inventors: Thomas C. Richards; Paul Christian; Jennifer A. Nelson; Kirakodu S. Nanjundaswamy; Fan Zhang
- Web page: https://patentgrep.com/patent/US20130252108A1

## CPC

- H01M 4/06: Electrodes for primary cells
- H01M 4/0445: {Forming after manufacture of the electrode, e.g. first charge, cycling}
- H01M 4/52: of nickel, cobalt or iron
- H01M 6/5088: {Initial activation; predischarge; Stabilisation of initial voltage}
- H01M 2300/0014: Alkaline electrolytes
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 29/49108: Electric battery cell making
- Y10T 29/53135: Storage cell or battery
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A primary alkaline battery includes a cathode having an alkali-deficient nickel (IV)-containing oxide including metals such as Ni, Co, Mg, Al, Ca, Y, Mn, and/or non-metals such as B, Si, Ge or a combination of metal and/or non-metal ions as stabilizing dopants; a combination of metal ions as dopants; an anode; a separator between the cathode and the anode; and an alkaline electrolyte. The battery can be pre-discharged within one hour after assembly to decrease the open circuit voltage.

## Claims

### Claim 1

A method of making a primary alkaline battery, comprising:
partially discharging an assembled battery at a continuous drain rate within about one hour of cell closure;
maintaining the partially discharged battery for a period of time ranging from 1 to 24 hours at a temperature in the range of 25 to 70° C. to provide a pre-discharged primary alkaline battery;
wherein the pre-discharged battery has an open circuit voltage value of less than or equal to 1.75 V at 25° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the pre-discharged battery has a capacity retention of at least 95 percent of the capacity of a battery discharged within 24 hours after manufacture, after storage for at least one week at 25° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the pre-discharged battery has a capacity retention of at least 90 percent of the capacity of a battery discharged within 24 hours after manufacture, after storage for at least one week at 45° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the pre-discharged battery has a capacity retention of at least 85 percent of the capacity of a battery discharged within 24 hours after manufacture, after storage for at least one week at 60° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the pre-discharged battery has a decrease in oxygen evolution of at least 50% compared to a freshly assembled battery.

### Claim 6 (depends on 1)

The method of claim 1, wherein the pre-discharged battery has an open circuit voltage value of from 1.65 to 1.75 V at 25° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the battery is partially discharged by 15 percent or less of a total battery design capacity within 24 hours after manufacture.

### Claim 8 (depends on 1)

The method of claim 1, wherein the battery is partially discharged by 10 percent or less of a total battery design capacity within 24 hours after manufacture.

### Claim 9 (depends on 1)

The method of claim 1, wherein the battery is partially discharged by 7.5 percent or less of a total battery design capacity within 24 hours after manufacture.

### Claim 10 (depends on 1)

The method of claim 1, wherein the battery is partially discharged by five percent or less of a total battery design capacity within 24 hours after manufacture.

### Claim 11

(canceled)

### Claim 12 (depends on 1)

The method of claim 1, wherein the battery is partially discharged at a low rate of 5 to 10 mA/g of active material within 24 hours after manufacture.

### Claim 13 (depends on 1)

The method of claim 1, wherein the freshly assembled battery is partially discharged at a high rate of 10 to 100 mA/g of active material within 24 hours after manufacture.

### Claim 14 (depends on 1)

The method of claim 1, wherein partially discharging the battery comprises a step-wise discharge process.

### Claim 15 (depends on 1)

The method of claim 1, wherein partially discharging the battery is performed at 25° C.

### Claim 16 (depends on 1)

The method of claim 1, wherein partially discharging the battery is performed at a temperature of from 20 to 30° C.

### Claim 17 (depends on 1)

The method of claim 1, wherein the battery comprises:
a cathode comprising an oxide having a formula AxNi1-y-z-wCoyMazMbwO2;
an anode;
a separator between the cathode and the anode; and
an alkaline electrolyte, wherein
A is an alkali metal,
Ma is a metal dopant,
Mb is a non-metal dopant,
0≦x≦0.2,
w is 0, or 0≦w≦0.02 and
0.02≦y+z≦0.25.

### Claim 18

A battery, comprising:
a cathode comprising an oxide having a formula AxNi1-y-z-wCoyMazMbwO2;
an anode;
a separator between the cathode and the anode; and
an alkaline electrolyte, wherein
A is an alkali metal,
Ma is a metal dopant,
Mb is a non-metal dopant,
0≦x≦0.2,
w is 0, or 0≦w≦0.02 and
0.02≦y+z≦0.25,
wherein the battery has an open circuit voltage value of from 1.65 to 1.75 V.

### Claim 19 (depends on 18)

The battery of claim 18, wherein the capacity retention is more than 95 percent after one week at 25° C.

### Claim 20 (depends on 18)

The battery of claim 18, wherein the capacity retention is more than 90 percent after one week at 45° C.

### Claim 21 (depends on 18)

The battery of claim 18, wherein the capacity retention is more than 85 percent after one week at 60° C.