# US 2013/0252105 A1 · Positive electrode active material, method of preparing positive electrode active material, and lithium secondary battery using positive electrode active material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252105 A1
- Document ID: US20130252105A1
- Status: Published application
- Kind: A1
- Application number: 13/730,045
- Filed: 2012-12-28
- Published: 2013-09-26
- Earliest claimed: 2012-03-23
- Assignees: Samsung Corning Precision Materials Co., Ltd.
- Applicants: Samsung Corning Precision Materials Co., Ltd.
- Inventors: Mi Sun LEE; Yun Ju Cho; Se Won Kim; Pil Sang Yun; Doo Kyun Lee; Ha Yeon Lee; Shin Jung Choi
- Web page: https://patentgrep.com/patent/US20130252105A1

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/0402: {Methods of deposition of the material}
- H01M 4/366: {as layered products}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/624: {Electric conductive fillers}
- H01M 10/052: Li-accumulators
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided are a positive electrode active material, a method of preparing the same, and a lithium secondary battery using the positive electrode active material, and more particularly, a positive electrode active material in which a surface of layer-structured lithium transition metal composite oxide is coated with one or more indium-based compounds selected from the group consisting of indium oxides and alloys including indium, a method of preparing the positive electrode active material, and a lithium secondary battery using the positive electrode active material. According to the present disclosure, degradation of cycle characteristics according to repetitive discharge of a battery may be prevented and thermal stability and rate characteristics may be improved.

## Claims

### Claim 1

A positive electrode active material comprising layer-structured lithium transition metal composite oxide expressed by the following Chemical Formula 1,
wherein a surface of the lithium transition metal composite oxide is coated with one or more indium (In)-based compounds selected from the group consisting of indium oxides and alloys including indium:
xLiMO2.(1−x)Li2MnO3 [Chemical Formula 1]
where M is one or more selected from the group consisting of magnesium (Mg), nickel (Ni), cobalt (Co), chromium (Cr), aluminum (Al), vanadium (V), iron (Fe), copper (Cu), zinc (Zn), titanium (Ti), strontium (Sr), manganese (Mn), boron (B), and lanthanum (La), and 0<x<1.

### Claim 2 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the indium-based compound is one or more selected from the group consisting of In2O3, ITO (tin (Sn)-doped In2O3), IZO (Zn-doped In2O3), ITZO (Sn/Zn co-doped In2O3), IAO (antimony (Sb)-doped In2O3), ZnIn2O5, Zn3In2O6, Zn5In2O8, CdIn2O4, MgIn2O4, AgInO2, and an alloy of indium oxide and one or more of Zn oxide, Sn oxide, gallium (Ga) oxide, thallium (TI) oxide, Mg oxide, tungsten (W) oxide, and Al oxide.

### Claim 3 (depends on 2)

The positive electrode active material as claimed in claim 2, wherein the alloy of indium oxide is one or more selected from the group consisting of ZnO—In2O3, SnO2—In2O3, MgO—In2O3, Ga2O—In2O3, and Al2O3—In2O3.

### Claim 4 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein the indium-based compound is coated in an amount range of 0.2 wt % to 6 wt % based on the lithium transition metal composite oxide.

### Claim 5 (depends on 1)

The positive electrode active material as claimed in claim 1, wherein a particle diameter of the indium-based compound is in a range of 10 nm to 50 μm.

### Claim 6 (depends on 1)

A lithium secondary battery comprising the positive electrode active material of claim 1.

### Claim 7

A method of preparing a positive electrode active material, the method comprising:
coating lithium transition metal composite oxide expressed by the following Chemical Formula 1 by adding and stirring one or more indium (In)-based compounds selected from the group consisting of indium oxides and alloys including indium; and
heat treating powder obtained after the coating:
xLiMO2.(1−x)Li2MnO3 [Chemical Formula 1]
where M is one or more selected from the group consisting of magnesium (Mg), nickel (Ni), cobalt (Co), chromium (Cr), aluminum (Al), vanadium (V), iron (Fe), copper (Cu), zinc (Zn), titanium (Ti), strontium (Sr), manganese (Mn), boron (B), and lanthanum (La), and 0<x<1.

### Claim 8 (depends on 7)

The method as claimed in claim 7, wherein the coating is performed by using a dry coating method or wet coating method.

### Claim 9 (depends on 8)

The method as claimed in claim 8, wherein the wet coating method further comprises preparing a coating solution in which an indium-based compound is mixed with a solvent.

### Claim 10 (depends on 9)

The method as claimed in claim 9, wherein the solvent is one or more selected from the group consisting of alcohol having a carbon number of 1 to 6, toluene, hexane, acetone, ether, tetrahydrofuran, dichloromethane, dichloroethane, ethyl acetate, xylene, benzene, ethylbenzene, methylethylketone, dimethyl sulfoxide, dimethylformamide, hexamethylphosphoramide, and methylisobutylketone.

### Claim 11 (depends on 7)

The method as claimed in claim 7, wherein the indium-based compound is added in an amount range of 0.2 wt % to 6 wt % based on the lithium transition metal composite oxide.

### Claim 12 (depends on 7)

The method as claimed in claim 7, wherein the heat treating is performed at a temperature in a range of 300° C. to 700° C. for 1 hour to 12 hours.

### Claim 13 (depends on 2)

A lithium secondary battery comprising the positive electrode active material of claim 2.

### Claim 14 (depends on 3)

A lithium secondary battery comprising the positive electrode active material of claim 3.

### Claim 15 (depends on 4)

A lithium secondary battery comprising the positive electrode active material of claim 4.

### Claim 16 (depends on 5)