# US 2013/0252101 A1 · Nanoporous silicon and lithium ion battery anodes formed therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252101 A1
- Document ID: US20130252101A1
- Status: Published application
- Kind: A1
- Application number: 13/831,210
- Filed: 2013-03-14
- Published: 2013-09-26
- Earliest claimed: 2012-03-21
- Assignees: University of Southern California
- Applicants: University of Southern California
- Inventors: Chongwu Zhou; Mingyuan Ge; Jiepeng Rong; Xin Fang
- Web page: https://patentgrep.com/patent/US20130252101A1

## CPC

- H01M 4/049: {Manufacturing of an active layer by chemical means}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/621: {Binders}
- H01M 4/625: {Carbon or graphite}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An electrode for a lithium ion battery, the electrode including nanoporous silicon structures, each nanoporous silicon structure defining a multiplicity of pores, a binder, and a conductive substrate. The nanoporous silicon structures are mixed with the binder to form a composition, and the composition is adhered to the conductive substrate to form the electrode. The nanoporous silicon may be, for example, nanoporous silicon nanowires or nanoporous silicon formed by etching a silicon wafer, metallurgical grade silicon, silicon nanoparticles, or silicon prepared from silicon precursors in a plasma or chemical vapor deposition process. The nanoporous silicon structures may be coated or combined with a carbon-containing compound, such as reduced graphene oxide. The electrode has a high specific capacity (e.g., above 1000 mAh/g at current rate of 0.4 A/g, above 1000 mAh/g at a current rate of 2.0 A/g, or above 1400 mAh/g at a current rate of 1.0 A/g).

## Claims

### Claim 1

An electrode for a lithium ion battery, the electrode comprising:
nanoporous silicon structures, each nanoporous silicon structure defining a multiplicity of pores;
a binder; and
a conductive substrate,
wherein the nanoporous silicon structures are mixed with the binder to form a composition, and the composition is adhered to the conductive substrate to form the electrode.

### Claim 2 (depends on 1)

The electrode of claim 1, wherein the nanoporous silicon structures are nanoporous silicon nanowires.

### Claim 3 (depends on 1)

The electrode of claim 1, wherein the nanoporous silicon structures are nanoporous silicon particles having a mean diameter of 10 μm or less, between 1 μm and 10 μm, between 1 and 100 nm, between 50 and 150 nm, or between 50 and 500 nm.

### Claim 4 (depends on 3)

The electrode of claim 3, wherein the nanoporous silicon structures are nanoporous silicon particles formed from powder silicon nanoparticles, bulk metallurgical grade silicon, or from silicon precursors through a plasma or chemical vapor deposition process.

### Claim 5 (depends on 1)

The electrode of claim 1, further comprising carbon black, wherein the carbon black is mixed with the nanoporous silicon structures and the binder to form the composition.

### Claim 6 (depends on 1)

The electrode of claim 1, wherein a mean diameter of the pores in the nanoporous silicon structures is in a range between 1 nm and 200 nm, and a distance between adjacent pores in the nanoporous silicon structures is in a range between 1 nm and 200 nm.

### Claim 7 (depends on 1)

The electrode of claim 1, wherein the nanoporous silicon structures are coated with carbon, reduced graphene oxide, or a combination thereof.

### Claim 8 (depends on 1)

The electrode of claim 1, wherein the nanoporous silicon structures are doped with boron, arsenic, phosphorus, iron, chromium, aluminum, or a combination thereof.

### Claim 9 (depends on 1)

The electrode of claim 1, wherein the viscosity of the binder is in a range between 100 cP to 2000 cP at room temperature.

### Claim 10 (depends on 9)

The electrode of claim 9, wherein the binder comprises an alginic acid salt.

### Claim 11 (depends on 1)

The electrode of claim 1, wherein the specific capacity of the electrode exceeds 1000 mAh/g after 100 cycles at a charge/discharge rate of 0.4 A/g.

### Claim 12 (depends on 1)

A lithium ion battery comprising the electrode of claim 1.

### Claim 13

A method comprising:
combining nanoporous silicon structures, each nanoporous silicon structure defining a multiplicity of pores, with a binder to form a mixture; and
forming the mixture to yield an electrode for a lithium ion battery, wherein the specific capacity of the electrode exceeds 1000 mAh/g after 100 cycles at a charge/discharge rate of 0.4 A/g electrode.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
etching solid silicon structures with a first etchant solution comprising a metal salt and strong acid to yield the nanoporous silicon structures before combining the nanoporous silicon structures with the binder; or
etching solid silicon structures with a first etchant solution comprising a metal salt and strong acid to yield the nanoporous silicon structures and then etching the nanoporous silicon structures with a second etchant solution comprising a strong acid and an oxidizing agent before combining the nanoporous silicon structures with the binder.

### Claim 15 (depends on 14)

The method of claim 14, wherein the solid silicon structures are selected from the group consisting of silicon wafers, silicon nanoparticles, metallurgical grade silicon particles, and silicon particles prepared from silicon precursors in a plasma or chemical vapor deposition process.

### Claim 16 (depends on 14)

The method of claim 14, wherein the solid silicon structures are metallurgical grade silicon particles having a purity of at least 95% and less than 99.9%, less than 99.8%, less than 99.5%, less than 99%, less than 98%, or less than 96%, and further comprising ball-milling the metallurgical grade silicon particles before etching the solid silicon structures.

### Claim 17 (depends on 14)

The method of claim 14, wherein the solid silicon structures are doped with boron, arsenic, phosphorus, iron, chromium, aluminum, or a combination thereof.

### Claim 18 (depends on 14)

The method of claim 14, wherein the metal salt is silver nitrate.

### Claim 19 (depends on 18)

The method of claim 18, wherein the metal salt comprises iron nitrate, chloroauric acid, copper nitrate, copper chloride, cobalt (III) nitrate, cobalt (III) chloride, or a combination thereof.

### Claim 20 (depends on 13)

The method of claim 13, further comprising:
coating the nanoporous silicon structures with carbon by decomposition of a carbon-containing compound before combining the nanoporous silicon structures with the binder; or
coating the nanoporous silicon structures with carbon by decomposition of a carbon-containing compound before combining the nanoporous silicon structures with the binder, and coating the carbon-coated nanoporous silicon structures with reduced graphene oxide before combining the nanoporous silicon structures with the binder.