# US 2013/0252090 A1 · Non-aqueous electrolyte battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252090 A1
- Document ID: US20130252090A1
- Status: Published application
- Kind: A1
- Application number: 13/820,817
- Filed: 2011-09-05
- Published: 2013-09-26
- Earliest claimed: 2010-09-06
- Assignees: Ntt Facilities, Inc.; Hitachi Chemical Company, Ltd.
- Inventors: Tomonobu Tsujikawa; Masayasu Arakawa; Kenji Kurita; Masayuki Terada
- Web page: https://patentgrep.com/patent/US20130252090A1

## CPC

- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A non-aqueous electrolyte battery capable of securing safety at a time of battery abnormality and restricting a drop in capacity or output at a time of battery use is provided. In a lithium-ion secondary battery 20, an electrode group 6 that positive and negative electrode plates are wound via a separator is accommodated into a battery container 7 into which a non-aqueous electrolyte is injected. In the positive electrode plate, a positive electrode mixture layer W2 including a lithium transition metal complex oxide is formed at both surfaces of an aluminum foil W1. A flame retardant layer W6 containing a phosphazene compound of a flame retardant and a polyethylene oxide of a binder having ionic conductivity is formed at a surface of the positive electrode mixture layer W2. In the negative electrode plate, a negative electrode mixture layer W6 including a carbon material of a negative electrode active material is formed at both surfaces of rolled copper foil W3. Ionic conductivity is secured by the polyethylene oxide and the phosphazene compound decomposes when a battery temperature goes up due to battery abnormality.

## Claims

### Claim 1

A non-aqueous electrolyte battery that a positive electrode plate in which a positive electrode mixture including a positive electrode active material is applied to a collector and a negative electrode plate in which a negative electrode mixture including a negative electrode active material is applied to a collector are disposed via a porous separator, wherein a flame retardant layer containing a phosphazene compound of a flame retardant and a binder having ionic conductivity is placed at one side or both sides of at least one kind of the positive electrode plate, the negative electrode plate and the separator.

### Claim 2 (depends on 1)

The non-aqueous electrolyte battery according to claim 1, wherein the flame retardant decomposes thermally under a thermal environment of from 60 deg. C. to 400 deg. C.

### Claim 3 (depends on 1)

The non-aqueous electrolyte battery according to claim 1, wherein the flame retardant is contained at a percentage of 10 wt % or more to the positive electrode mixture.

### Claim 4 (depends on 1)

The non-aqueous electrolyte battery according to claim 1, wherein the binder is a polyether-based polymer compound.

### Claim 5 (depends on 4)

The non-aqueous electrolyte battery according to claim 4, wherein the polyether-based polymer compound includes a polyethylene oxide.

### Claim 6 (depends on 1)

The non-aqueous electrolyte battery according to claim 1, wherein the flame retardant layer contains the flame retardant at a percentage of ranging from 50 wt % to 91 wt % and the binder at a percentage of ranging from 9 wt % to 50 wt %, respectively.