# US 2013/0252068 A1 · Manufacturing method of high-performance silicon based electrode using polymer pattern on current collector and manufacturing method of negative electrode of rechargeable lithium battery including same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0252068 A1
- Document ID: US20130252068A1
- Status: Published application
- Kind: A1
- Application number: 13/593,985
- Filed: 2012-08-24
- Published: 2013-09-26
- Earliest claimed: 2012-03-20
- Assignees: Korea Institute of Science and Technology
- Inventors: Joong Kee LEE; Won Chang CHOI; Joo Man WOO; Ho Suk CHOI; Jung Sub KIM; Hieu Si NGUYEN; Chairul HUDAYA; A Young KIM; Ji Hun PARK; Sang Ok KIM; Xuyan LIU
- Web page: https://patentgrep.com/patent/US20130252068A1

## CPC

- H01M 4/0421: {involving vapour deposition}
- C25D 5/022: {using masking means}
- C25D 5/38: of refractory metals or nickel
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are a silicon nanostructured material with theoretical storage capacity of energy resulting from electrochemical reaction with lithium improved more than 10 times as compared to the existing graphite material and having superior output characteristics, an electrode including the same, and a secondary battery and an electrochemical capacitor including the electrode as a negative electrode. The physical stability of the electrode active material is improved and an electrode with high performance can be obtained. Since more energy can be stored as compared to the graphite material of the same thickness and high-output performance can be achieved through the nanostructure, energy density can be remarkably improved as compared to the existing lithium-ion battery by about 2 times. An asymmetric lithium-ion secondary battery including the electrode active material is applicable to storage of renewable energy, ubiquitous power source, power supply for machinery and vehicles, or the like.

## Claims

### Claim 1

A method for manufacturing a micropolymer-patterned current collector, comprising:
(a) preparing a solution in which a polymer resin is dissolved in a solvent;
(b) coating the polymer solution on a current collector and drying the same;
(c) preparing a mixture solvent by diluting the solvent in step (a) with a nonsolvent; and
(d) treating a substrate on which the polymer solution is coated with the mixture solvent and drying the same.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, in said preparing the polymer solution, the polymer resin is one or more selected from a group consisting of polyethylene, polystyrene, polypropylene, polyethylene and poly(methyl methacrylate).

### Claim 3 (depends on 1)

The method according to claim 1, wherein, in said preparing the polymer solution, the solvent is one or more selected from a group consisting of acetone, acetic acid, aniline, allylamine, benzene, bromobenzene, chloroform, chloroethane, chlorobenzene, chlorohexanol, ethylbenzene, ethoxyethane and hexane.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, in said preparing the polymer solution, the polymer resin is included in the polymer solution in an amount of 0.01-50 wt %.

### Claim 5 (depends on 1)

The method according to claim 1, wherein, in said preparing the polymer solution, the current collector is a porous copper current collector.

### Claim 6 (depends on 1)

The method according to claim 1, wherein, in said coating the polymer solution, the coating is doctor blade coating, bar coating, dip coating or spin coating.

### Claim 7 (depends on 1)

The method according to claim 1, wherein, in said drying the polymer solution, the drying is performed at 0-100° C. for 1-24 hours.

### Claim 8 (depends on 1)

The method according to claim 1, wherein, in said preparing the mixture solvent, the nonsolvent is one or more selected from a group consisting of butanol, 1-butoxybutane, 1,3-butanediol, cyclohexanol, ethanol, ethylene glycol, formamide, 1-pentanol, 2-isopropoxypropane, isopropyl alcohol, methanol and water.

### Claim 9 (depends on 1)

The method according to claim 1, wherein, in said preparing the mixture solvent, the mixture solvent is prepared by diluting the solvent which is acetone, acetic acid, aniline, allylamine, benzene, bromobenzene, chloroform, chloroethane, chlorobenzene, chlorohexanol, ethylbenzene, ethoxyethane or hexane with the nonsolvent which is butanol, 1-butoxybutane, 1,3-butanediol, cyclohexanol, ethanol, ethylene glycol, formamide, 1-pentanol, 2-isopropoxypropane, isopropyl alcohol, methanol or water to 1-100 vol %.

### Claim 10 (depends on 1)

The method according to claim 1, wherein, in said drying the mixture solvent, the drying is performed at 0-100° C. for 1-24 hours.

### Claim 11

A method for manufacturing a negative electrode for a lithium secondary battery, comprising:
performing electroless copper plating on a micropolymer pattern formed on a micropolymer-patterned current collector;
removing the polymer pattern and forming an electrode active material on the current collector by chemical deposition or physical deposition; and
modifying the surface of the electrode active material.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the current collector is a porous copper current collector.

### Claim 13 (depends on 11)

The method according to claim 11, wherein, in said performing the electroless copper plating, the plating is performed at 20-30° C. for 10-30 seconds under a current density of current density of 10-20 A/cm2 using a mixture of 60 g/L CuSO4H2O, 150 g/L H2S04 and 50 ppm HCl.

### Claim 14 (depends on 11)

The method according to claim 11, wherein, in said removing the polymer pattern, the micropolymer pattern is removed by immersing the current collector in a solvent.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the solvent is chloroform.

### Claim 16 (depends on 11)

The method according to claim 11, wherein, in said forming the electrode active material, the electrode active material is a phosphorus-doped silicon thick film comprising silane and phosphine.

### Claim 17 (depends on 11)

The method according to claim 11, wherein, in said modifying the surface of the electrode active material, the surface modification comprises connecting a copper plate to a positive electrode and an electrode to a negative electrode in a plating solution and flowing electrical current or placing the electrode active material in a vacuum chamber and coating copper on the electrode active material under vacuum to a thickness of 0.1-20 nm.

### Claim 18 (depends on 10, 11, 12, 13, 14, 15)

A single-cell battery comprising one lithiated negative electrode manufactured by the method according to any one of claims 10 to 15 and one positive electrode comprising activated carbon.

### Claim 19 (depends on 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15)

A multiple-cell battery comprising 2-10 lithiated negative electrodes manufactured by the method according to any one of claims 10 to 15 and 2-10 positive electrodes comprising activated carbon stacked alternatingly.