# US 2013/0251982 A1 · Synthetic nano-sized crystalline calcium phosphate and method of production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0251982 A1
- Document ID: US20130251982A1
- Status: Published application
- Kind: A1
- Application number: 13/892,423
- Filed: 2013-05-13
- Published: 2013-09-26
- Earliest claimed: 2004-06-15
- Assignees: Promimic AB
- Applicants: Promimic AB
- Inventors: Per Kjellin; Martin Andersson
- Web page: https://patentgrep.com/patent/US20130251982A1

## CPC

- C09D 1/00: Coating compositions, e.g. paints, varnishes or lacquers, based on inorganic substances
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C01B 25/32: Phosphates of magnesium, calcium, strontium, or barium
- C01B 25/322: {Preparation by neutralisation of orthophosphoric acid}
- Y10T 428/258: Alkali metal or alkaline earth metal or compound thereof
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Synthetic nano-sized crystalline calcium phosphate, particularly hydroxyapatite, having a specific surface area in the range of 150 m2/g to 300 m2/g, is described. The nano-sized crystalline calcium phosphate may be in the form of a powder or in the form of a coating on a surface. A method of producing a nano-sized crystalline calcium phosphate powder or coating is also described.

## Claims

### Claim 1

A synthetic nano-sized crystalline calcium phosphate having a specific surface area in the range of 50 m2/g to 300 m2/g.

### Claim 2 (depends on 1)

The synthetic nano-sized crystalline calcium phosphate of claim 1, wherein the calcium phosphate is hydroxyapatite.

### Claim 3 (depends on 1)

The synthetic nano-sized crystalline calcium phosphate of claim 1, wherein the specific surface is selected from the group consisting of 180 m2/g, 220 m2/g and 280 m2/g.

### Claim 4 (depends on 1)

The synthetic nano-sized crystalline calcium phosphate of claim 1, wherein the calcium phosphate is in the form of a powder.

### Claim 5 (depends on 1)

The synthetic nano-sized crystalline calcium phosphate of claim 1, wherein the calcium phosphate is in the form of a coating on a surface.

### Claim 6 (depends on 1)

The synthetic nano-sized crystalline calcium phosphate of claim 1, wherein the surface is a metal surface.

### Claim 7 (depends on 6)

The synthetic nano-sized crystalline calcium phosphate of claim 6, wherein the metal surface is a titanium surface.

### Claim 8 (depends on 1)

The synthetic nano-sized crystalline calcium phosphate of claim 1, wherein the coating has a thickness of less than or equal to 100 nm.

### Claim 9 (depends on 1)

The synthetic nano-sized crystalline calcium phosphate of claim 1, wherein the calcium to phosphor ratio is 1.67.

### Claim 10

A method of producing a powder or coating of nano-sized crystalline calcium phosphate comprising the steps of
a) providing a solution of water and stoichiometric solved amounts of a phosphor precursor and of a calcium salt precursor,
b) adding a surfactant, and optionally a hydrophobic organic solvent, to the solution of a) to create a liquid crystalline phase,
c) allowing the liquid crystalline phase to equilibrate, and
d) placing the equilibrated liquid crystalline phase in an ammonia atmosphere to raise the pH so that nano-sized crystals of calcium phosphate are formed in the water domains of the liquid crystalline phase, the steps a)-d) being performed at ambient temperature, followed by either
e1) removing the surfactant from the ammonia-treated liquid crystalline phase of d) with a solvent and
f1) filtering, washing and drying the nano-sized crystals of calcium phosphate to obtain the powder, or
e2) diluting the ammonia-treated liquid crystalline phase of d) with a hydrophobic organic solvent to create a microemulsion of the nano-sized crystals of calcium phosphate in water,
f2) dipping an oxide layer-coated surface of an object into the microemulsion of e2) to deposit the microemulsion onto the surface,
g2) evaporating the organic solvent from the surface of f2) to obtain the coating of nano-sized crystalline calcium phosphate, and
h2) heating under inert atmosphere in order to remove the surfactant, or alternatively omitting step d) and
e3) diluting the liquid crystalline phase of c) with a hydrophobic organic solvent to create a microemulsion,
f3) dipping an oxide layer-coated surface of an object into the microemulsion of e3) to deposit the microemulsion onto the surface,
g3) evaporating the organic solvent from the surface of f3) to form a liquid crystalline phase, and
h3) placing the surface of g3) in an ammonia atmosphere to raise the pH so that nano-sized crystals of calcium phosphate are formed in the water domains of the liquid crystalline phase and are deposited on the surface, followed by
i2) heating under inert atmosphere in order to remove the surfactant.

### Claim 11 (depends on 10)

The method of claim 10, wherein the surfactant in b) is a non-ionic surfactant.

### Claim 12 (depends on 10)

The method of claim 10, wherein the oxide layer-coated surface of f2) or f3) is a metal surface.

### Claim 13 (depends on 12)

The method of claim 12, wherein the metal surface is a titanium surface.

### Claim 14 (depends on 10)

The method of claim 10, wherein the object of f2) or f3) is a body implant.

### Claim 15 (depends on 14)

The method of claim 14, wherein the body implant is a dental implant.

### Claim 16 (depends on 10)

The method of claim 10, wherein the calcium phosphate is hydroxyapatite.

### Claim 17 (depends on 10)

The method of claim 10, wherein the phosphor precursor is phosphoric acid.

### Claim 18 (depends on 10)

The method of claim 10, wherein the calcium salt precursor is calcium nitrate.

### Claim 19 (depends on 10)

The method of claim 10, wherein the calcium to phosphor ratio is 1.67.