# US 2013/0251966 A1 · Low temperature sintering conductive metal film and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0251966 A1
- Document ID: US20130251966A1
- Status: Published application
- Kind: A1
- Application number: 13/991,130
- Filed: 2011-10-20
- Published: 2013-09-26
- Earliest claimed: 2010-12-02
- Assignees: Korea Institute of Machinery & Materials
- Inventors: Ji-Hun Yu; Sangsun Yang; Yong-Jin Kim
- Web page: https://patentgrep.com/patent/US20130251966A1

## CPC

- C09D 11/52: Electrically conductive inks
- B22F 1/0545: Dispersions or suspensions of nanosized particles
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- H05K 3/1283: {After-treatment of the printed patterns, e.g. sintering or curing methods}
- B22F 1/105: containing inorganic lubricating or binding agents, e.g. metal salts
- B22F 1/107: containing organic material comprising solvents, e.g. for slip casting
- H05K 3/12: using {thick film techniques, e.g.} printing techniques to apply the conductive material {or similar techniques for applying conductive paste or ink patterns}
- Y10T 428/24909: Free metal or mineral containing
- Y10T 428/24917: including metal layer
- Y10T 428/256: Heavy metal or aluminum or compound thereof
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A low-temperature sintered conductive metal ink and a method for preparing the same are provided. To be specific, the preparation method includes the following steps of: preparing the conductive film or pattern by printing a conductive metal ink including metal nanocolloids, metal salts, and polymers reacted with the metal salts and preparing the metal nanocolloids (step 1); preparing a mixture by mixing the metal salts and polymers (step 2); preparing the metal ink by stirring the metal nanocolloids and the metal salt/polymer mixture prepared at steps 1 and 2 (step 3); printing the metal ink prepared at step 3 (step 4); and drying and thermally treating a product printed at step 4 (step 5).

## Claims

### Claim 1

A conductive metal film or pattern prepared by printing a conductive metal ink, the conductive metal ink comprising metal nanocolloids, metal salts, and polymers reacted with the metal salts.

### Claim 2 (depends on 1)

The conductive metal film or pattern as set forth in claim 1, wherein the metal nanocolloids comprise conductive metal particles of copper or aluminum.

### Claim 3 (depends on 2)

The conductive metal film or pattern as set forth in claim 2, wherein a size of the conductive metal particles is in a range of 1 to 500 nm.

### Claim 4 (depends on 1)

The conductive metal film or pattern as set forth in claim 1, wherein a metal content of the metal nanocolloids is in a range of 0.1 to 80 wt %.

### Claim 5 (depends on 1)

The conductive metal film or pattern as set forth in claim 1, wherein the metal salts are selected from the group consisting of metal organics, metal nitrides, and metal chlorides.

### Claim 6 (depends on 1)

The conductive metal film or pattern as set forth in claim 1, wherein the polymers reacted with the metal salts are selected from the group consisting of polyvinyl pyrrolidone, ethylene diamine, and diethyleneamine.

### Claim 7 (depends on 1)

The conductive metal film or pattern as set forth in claim 1, wherein the conductive metal ink further comprises a viscosity controlling agent.

### Claim 8 (depends on 1)

The conductive metal film or pattern as set forth in claim 1, wherein the conductive metal ink is printed by a method selected from the group consisting of gravure printing, offset printing, inkjet printing, screen printing, imprint, and spin coating.

### Claim 9

A method for preparing a conductive metal film or pattern, the method comprising the following steps of:
preparing the metal nanocolloids (step 1);
preparing a mixture of metal salts and polymers (step 2);
preparing a metal ink by stirring metal nanocolloids and the mixture of the metal salts and polymers prepared at steps 1 and 2 (step 3);
printing the metal ink prepared at step 3 (step 4); and
thermally treating a product printed at step 4.

### Claim 10 (depends on 9)

The method for preparing the conductive metal film or pattern as set forth in claim 9, wherein the metal nanocolloids at step 1 are prepared by means of an electrical wire explosion method.

### Claim 11 (depends on 9)

The method for preparing the conductive metal film or pattern as set forth in claim 9, wherein a concentration for mixing the metal salts and polymers at step 2 is in a range of 0.01 to 1 mol.

### Claim 12 (depends on 9)

The method for preparing the conductive metal film or pattern as set forth in claim 9, wherein the printing at step 4 is performed by a method selected from the group consisting of gravure printing, offset printing, inkjet printing, screen printing, imprint, and spin coating.

### Claim 13 (depends on 9)

The method for preparing the conductive metal film or pattern as set forth in claim 9, wherein the printing at step 4 is performed in an atmosphere of gas selected from the group consisting of argon, hydrogen, and air.

### Claim 14 (depends on 9)

The method for preparing the conductive metal film or pattern as set forth in claim 9, wherein the thermal treatment at step 5 is performed at a temperature of 100 to 500° C.