# US 2013/0251919 A1 · Front plate of tn liquid crystal panel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0251919 A1
- Document ID: US20130251919A1
- Status: Published application
- Kind: A1
- Application number: 13/824,157
- Filed: 2011-08-08
- Published: 2013-09-26
- Earliest claimed: 2010-09-17
- Assignees: Mgc Filsheet Co., Ltd.; Mitsubishi Gas Chemical Company, Inc.
- Inventors: Koshi Koide; Osamu Kakinoki
- Web page: https://patentgrep.com/patent/US20130251919A1

## CPC

- G02F 1/1335: Structural association of cells with optical devices, e.g. polarisers or reflectors
- G02F 1/133308: {Support structures for LCD panels, e.g. frames or bezels}
- B32B 2457/202: LCD, i.e. liquid crystal displays
- C09K 2323/035: Ester polymer, e.g. polycarbonate, polyacrylate or polyester
- G02F 1/133331: {Cover glasses}
- G02F 1/13363: Birefringent elements, e.g. for optical compensation
- G02F 1/1396: {the liquid crystal being selectively controlled between a twisted state and a non-twisted state, e.g. TN-LC cell (G02F1/141 takes precedence)}
- G02F 2201/50: Protective arrangements
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

The problem is to provide a front plate of a TN liquid crystal panel capable of inhibiting occurrence of color unevenness caused by retardation of a polycarbonate resin sheet, even when a liquid crystal panel is observed through polarizing glasses or liquid crystal shutter glasses for 3D, while having excellent impact resistance, heat resistance and transparency. The solution means is the front plate 1 of a TN liquid crystal panel provided with the polycarbonate resin sheet 10, wherein the direction of the slow axis X or the fast axis Y of the polycarbonate resin sheet 10 is inclined by 45° with respect to the lengthwise direction L of a liquid crystal panel.

## Claims

### Claim 1

A front plate of a TN liquid crystal panel comprising a polycarbonate resin sheet, wherein the direction of the slow axis or the fast axis of the polycarbonate resin sheet is inclined by 45° with respect to the lengthwise direction of a TN liquid crystal panel.

### Claim 2 (depends on 1)

A front plate of a TN liquid crystal panel according to claim 1, wherein a polycarbonate resin constituting the polycarbonate resin sheet has 2,2-bis(4-hydroxyphenyl)propane as a main raw material monomer, the viscosity average molecular weight within a range of 20,000 to 30,000, and the glass transition temperature within a range of 130 to 160° C.

### Claim 3 (depends on 1)

A front plate of a TN liquid crystal panel according to claim 1, wherein the thickness of the polycarbonate resin sheet is within a range of 0.3 to 2 mm.

### Claim 4 (depends on 1)

A front plate of a TN liquid crystal panel according to claim 1, further comprising a hard resin layer with a thickness within a range of 30 to 100 μm and the pencil hardness at a laminated state measured according to JIS5600-5-4 of at least F or more, the hard resin layer is obtained by coextrusion molding with the polycarbonate resin provided on the front surface or the back surface of the polycarbonate resin sheet.

### Claim 5 (depends on 4)

A front plate of a TN liquid crystal panel according to claim 4, wherein the hard resin layer consists of an acryl resin, a resin (nuclear hydrogenated MS resin) obtained by hydrogenating an aromatic ring of a copolymer obtained by polymerizing at least one kind of (meth)acrylate ester monomer and at least one kind of aromatic vinyl monomer, or a modified polycarbonate resin having 2,2-bis(4-hydroxy-3-methylphenyl)propane or 2,2-bis(4-hydroxy-3-methylphenyl)cyclohexane as a main raw material monomer.

### Claim 6 (depends on 5)

A front plate of a TN liquid crystal panel according to claim 5, wherein the acryl resin is methyl methacrylate as a main raw material monomer and the glass transition temperature of not less than 95° C.

### Claim 7 (depends on 5)

A front plate of a TN liquid crystal panel according to claim 5, wherein the nuclear hydrogenated MS resin is a resin obtained by hydrogenating an aromatic ring of a copolymer obtained by polymerizing methyl methacrylate and styrene hydrogenated, a copolymerization ratio of them is within a range of 60:40 to 90:10, and the hydrogenation ratio of an aromatic ring is not less than 70%.

### Claim 8 (depends on 5)

A front plate of a TN liquid crystal panel according to claim 5, wherein the modified polycarbonate resin is a copolymer of 2,2-bis(4-hydroxy-3-methylphenyl)propane and 2,2-bis(4-hydroxyphenyl)propane, and a copolymerization ratio of them is 50:50 to 100:0.

### Claim 9 (depends on 5)

A front plate of a TN liquid crystal panel according to claim 5, wherein the modified polycarbonate resin is a copolymer of 2,2-bis(4-hydroxy-3-methylphenyl)cyclohexane and 2,2-bis(4-hydroxyphenyl)propane, and a copolymerization ratio of them is 50:50 to 100:0.

### Claim 10 (depends on 5)

A front plate of a TN liquid crystal panel according claim 5, further comprising a hard coat membrane formed on the top front surface or the top back surface of the TN liquid crystal panel.

### Claim 11 (depends on 10)

A front plate of a TN liquid crystal panel according to claim 10, wherein the hard coat membrane consists of an ultraviolet curable acryl based resin composition, the thickness is within a range of 1 to 20 μm, and the pencil hardness at a laminated state measured according to JIS5600-5-4 is 3H or more.