# US 2013/0251883 A1 · Method of manufacturing porous granules

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0251883 A1
- Document ID: US20130251883A1
- Status: Published application
- Kind: A1
- Application number: 13/752,389
- Filed: 2013-01-29
- Published: 2013-09-26
- Earliest claimed: 2012-03-23
- Assignees: Ikeda Food Research Co., Ltd.
- Applicants: Ikeda Food and Research Co., Ltd.
- Inventors: Ken OHSUMI
- Web page: https://patentgrep.com/patent/US20130251883A1

## CPC

- A23D 9/05: Forming free-flowing pieces
- A23D 9/007: characterised by ingredients other than fatty acid triglycerides
- A23D: EDIBLE OILS OR FATS, e.g. MARGARINES, SHORTENINGS OR COOKING OILS (preservation thereof A23B20/00; production, refinement or preservation of animal or vegetable fats or oils C11B, C11C)

## Abstract

The present invention discloses a method of manufacturing porous granules, a porous granule obtained by the method, a lipid-containing granule and a method of manufacturing thereof, and a food containing the lipid-containing granules and a method of manufacturing thereof. The porous granule of the present invention is bigger than the granule manufactured by the spray drying method, has high solubility, is easily obtained (porous structure can be easily formed), and has enough hardness. In addition, drying time and drying cost can be reduced because an amount of water to be dried can be reduced. The porous granule can be obtained by mixing a powder whose solubility is at most 100 g per 100 mL of water at 20° C., with water and drying a mixture under reduced pressure to obtain the porous granules having loose bulk density of at least 0.30 g/mL, having porous structure, and capable of absorbing lipids.

## Claims

### Claim 1

A method of manufacturing porous granules comprising the steps of:
mixing a powder with water; and
drying a mixture under reduced pressure, wherein
the powder contains at least one of ingredients selected from a group consisting of monosaccharide, disaccharide, salt, amino acid and amino acid salt,
solubility of the powder is at most 100 g per 100 mL of water at 20° C., and
loose bulk density of the porous granules is at least 0.30 g/mL.

### Claim 2 (depends on 1)

The method according to claim 1, wherein
the percentage of at least one of ingredients selected from a group consisting of monosaccharide, disaccharide, salt, amino acid and amino acid salt is at least 80 wt. % in the powder.

### Claim 3 (depends on 1)

The method according to claim 1, wherein
the mixture contains at least 40 wt. % of the powder when the mixture of the powder and water is assumed to be 100 wt. %.

### Claim 4 (depends on 1)

A porous granule for absorbing lipid obtained from the manufacturing method according to claim 1.

### Claim 5 (depends on 4)

The porous granule for absorbing lipid according to claim 4, wherein
a compressive stress of a test piece of the porous granule prepared in 16 mm×16 mm×10 mm is at least 1.0 N/mm2 when the compressive stress is measured by a creep meter by applying pressure to the test piece by a cylindrical plunger of 3 mm diameter at a speed of 0.5 mm/sec.

### Claim 6 (depends on 4)

A lipid-containing granule obtained from the porous granule according to claim 4, wherein
the lipid is absorbed in the porous granule.

### Claim 7 (depends on 6)

The lipid-containing granule according to claim 6, wherein
compressibility of the lipid-containing granule is at most 25 and
Hausner ratio of the lipid-containing granule is 1.00 to 1.34.