# US 2013/0241015 A1 · Magnetoresistive element and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0241015 A1
- Document ID: US20130241015A1
- Status: Published application
- Kind: A1
- Application number: 13/604,457
- Filed: 2012-09-05
- Published: 2013-09-19
- Earliest claimed: 2012-01-05
- Assignees: Kabushiki Kaisha Toshiba
- Inventors: Akiko NOMACHI
- Web page: https://patentgrep.com/patent/US20130241015A1

## CPC

- H10N 50/01: Manufacture or treatment
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10N 30/01: Manufacture or treatment
- H10N 30/05: Manufacture of multilayered piezoelectric or electrostrictive devices, or parts thereof, e.g. by stacking piezoelectric bodies and electrodes
- H10N 30/067: Forming single-layered electrodes of multilayered piezoelectric or electrostrictive parts
- H10N 30/082: by etching, e.g. lithography
- H10N 35/00: Magnetostrictive devices (integrated devices or assemblies of multiple devices H10N39/00)
- H10N 35/01: Manufacture or treatment
- H10N 35/80: Constructional details
- H10N 35/85: Magnetostrictive active materials
- H10N 39/00: Integrated devices, or assemblies of multiple devices, comprising at least one piezoelectric, electrostrictive or magnetostrictive element covered by groups H10N30/00 – H10N35/00
- H10N 50/10: Magnetoresistive devices
- H10N 50/80: Constructional details
- H10B 61/22: {of the field-effect transistor [FET] type}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

According to one embodiment, a magnetoresistive element manufacturing method is provided. In this magnetoresistive element manufacturing method, a first ferromagnetic layer, tunnel barrier layer, and second ferromagnetic layer are sequentially formed on a substrate. A conductive hard mask is formed on the second ferromagnetic layer. The hard mask is patterned. A hard layer is formed on the side surface of the hard mask. The second ferromagnetic layer, tunnel barrier layer, and first ferromagnetic layer are processed by IBE in an oblique direction by using the hard mask and hard layer as masks. The IBE etching rate of the hard layer is lower than that of the hard mask.

## Claims

### Claim 1

A magnetoresistive element manufacturing method comprising:
sequentially forming a first ferromagnetic layer, a tunnel barrier layer, and a second ferromagnetic layer on a substrate;
forming a conductive hard mask on the second ferromagnetic layer;
patterning the hard mask;
forming a hard layer on a side surface of the hard mask; and
processing the second ferromagnetic layer, the tunnel barrier layer, and the first ferromagnetic layer by IBE in an oblique direction by using the hard mask and the hard layer as masks,
wherein the hard layer has an IBE etching rate lower than that of the hard mask.

### Claim 2 (depends on 1)

The method of claim 1, wherein a Vickers hardness of the hard layer is higher than that of the hard mask.

### Claim 3 (depends on 1)

The method of claim 1, wherein the hard layer comprises one of DLC, Al2O3, BN, and SiC.

### Claim 4 (depends on 1)

The method of claim 1, wherein the hard mask comprises one of TiN, Ta, and W.

### Claim 5 (depends on 1)

The method of claim 1, wherein the hard layer and the hard mask comprise the same material, and a density of the hard layer is higher than that of the hard mask.

### Claim 6 (depends on 5)

The method of claim 5, wherein the hard layer and the hard mask comprise one of TiN, Ta, and W.

### Claim 7 (depends on 1)

The method of claim 1, wherein the forming the hard layer on the side surface of the hard mask comprises:
forming the hard layer on an entire surface; and
removing the hard layer from an upper surface of the second ferromagnetic layer and an upper surface of the hard mask by RIE.

### Claim 8 (depends on 7)

The method of claim 7, wherein the hard layer comprises DLC, and RIE of the hard layer uses an O2-based gas.

### Claim 9 (depends on 7)

The method of claim 7, wherein the hard layer comprises Al2O3, and RIE of the hard layer uses a BCl3-based gas.

### Claim 10

A magnetoresistive element manufacturing method comprising:
sequentially forming a first ferromagnetic layer, a tunnel barrier layer, and a second ferromagnetic layer on a substrate;
forming a sacrificial layer on the second ferromagnetic layer;
forming a hole extending through the sacrificial layer;
forming a hard layer on the sacrificial layer in the hole;
forming a conductive hard mask on the hard layer in the hole so as to fill the hole;
removing the sacrificial layer; and
processing the second ferromagnetic layer, the tunnel barrier layer, and the first ferromagnetic layer by IBE in an oblique direction by using the hard mask and the hard layer as masks,
wherein the hard layer has an IBE etching rate lower than that of the hard mask.

### Claim 11 (depends on 10)

The method of claim 10, wherein a Vickers hardness of the hard layer is higher than that of the hard mask.

### Claim 12 (depends on 10)

The method of claim 10, wherein the hard layer comprises one of DLC, Al2O3, BN, and SiC.

### Claim 13 (depends on 10)

The method of claim 10, wherein the hard mask comprises one of TiN, Ta, and W.

### Claim 14 (depends on 10)

The method of claim 10, wherein the hard layer and the hard mask comprises the same material, and a density of the hard layer is higher than that of the hard mask.

### Claim 15 (depends on 14)

The method of claim 14, wherein the hard layer and the hard mask comprise one of TiN, Ta, and W.

### Claim 16 (depends on 10)

The method of claim 10, wherein the forming the hard layer on the sacrificial layer in the hole comprises:
forming the hard layer on an entire surface; and
removing the hard layer from an upper surface of the second ferromagnetic layer and an upper surface of the sacrificial layer by RIE.

### Claim 17

A magnetoresistive element comprising:
a first ferromagnetic layer, a tunnel barrier layer, and a second ferromagnetic layer sequentially formed on a substrate;
a conductive hard mask formed on the second ferromagnetic layer; and
a hard layer formed on a side surface of the hard mask.

### Claim 18 (depends on 17)

The element of claim 17, wherein a Vickers hardness of the hard layer is higher than that of the hard mask.

### Claim 19 (depends on 17)

The element of claim 17, wherein the hard layer comprises one of DLC, Al2O3, BN, and SiC.

### Claim 20 (depends on 17)

The element of claim 17, wherein the hard mask comprises one of TiN, Ta, and W.