# US 2013/0240990 A1 · Semiconductor structure and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240990 A1
- Document ID: US20130240990A1
- Status: Published application
- Kind: A1
- Application number: 13/989,808
- Filed: 2011-12-02
- Published: 2013-09-19
- Earliest claimed: 2011-11-15
- Inventors: Haizhou Yin; Wei Jiang; Gaobo Xu
- Web page: https://patentgrep.com/patent/US20130240990A1

## CPC

- H10D 64/01: Manufacture or treatment
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 62/83: being Group IV materials, e.g. B-doped Si or undoped Ge
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/0113: {the conductive layers comprising highly doped semiconductor materials, e.g. polysilicon layers or amorphous silicon layers}
- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/258: {characterised by the relative positions of the source or drain electrodes with respect to the gate electrode}
- H10D 64/259: {Source or drain electrodes being self-aligned with the gate electrode and having bottom surfaces higher than the interface between the channel and the gate dielectric}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10D 30/608: {having non-planar bodies, e.g. having recessed gate electrodes}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for manufacturing a semiconductor structure and a semiconductor device manufactured using the same are disclosed. In replacement gate process, the present invention is capable of reducing contact resistance at source/drain regions through forming doped amorphous Si layers above source/drain regions, forming contact holes (310) penetrating through the interlayer dielectric layer (300) and amorphous Si layers (251); wherein the contact holes (310) at least expose part of the source/drain regions (110), and contact layers are formed at the exposed area of the source/drain regions and sidewalls of the contact holes in the amorphous Si layer. Since contact layers are formed after high-k dielectric layer has been annealed, metal silicide layers are protected from damages at high temperatures.

## Claims

### Claim 1

A method for manufacturing a semiconductor structure, comprising:
a) providing a substrate (100);
b) forming a dummy gate stack on the substrate (100), spacers (240) located on sidewalls of the dummy gate stack, and source/drain regions (110) located on both sides of the dummy gate stack, wherein the dummy gate stack at least comprises a first gate dielectric layer and a dummy gate (220):
c) forming an amorphous Si layer (251), which has the same doping type as the source/drain regions, on surfaces of the source/drain regions (110):
d) forming an interlayer dielectric layer (300) to cover the doped amorphous Si layer (251) and the dummy gate stack;
e) removing part of the interlayer dielectric layer (300) to expose the dummy gate stack;
f) removing the dummy gate stack to form an opening, filling the opening (260) with a second gate dielectric layer and a first conductive material (280) to form a gate stack structure; or removing part of the dummy gate stack that is located on the first gate dielectric layer to form an opening, and filling the opening (260) with a first conductive material (280) to form a gate stack structure;
g) forming contact holes (310) that penetrate through the interlayer dielectric layer (300) and the amorphous Si layer (251), wherein the contact holes (310) at least expose part of the source/drain regions (110):
h) forming a contact layer (111) on the exposed area of the source/drain regions (110) and on sidewalls of the contact holes (310) in the amorphous Si layer (251); and
i) filling the contact holes with a second conductive material to form contact vias (320).

### Claim 2 (depends on 1)

The method of claim 1, wherein
at step c), the step for forming the doped amorphous Si layer (251) comprises:
forming an amorphous Si layer (250) to cover the dummy gate stack, spacers (240) located on sidewalls of the dummy gate stack, and source/drain regions (110) located on both sides of the dummy gate stack;
doping the amorphous Si layer (250), wherein the doping type thereof is the same as that of the source/drain regions; and
patterning the amorphous Si layer (250) to keep the amorphous Si layer on the source/drain regions and remove the remaining amorphous Si layer, so as to form the doped amorphous Si layer (251).

### Claim 3 (depends on 1)

The method of claim 1, wherein between the step f) and the step g), the method further comprises:
j) forming a cap layer (400) to cover the gate stack structure and the interlayer dielectric layer (300), wherein the material of the cap layer (400) is different from the material of the interlayer dielectric layer (300).

### Claim 4 (depends on 1)

The method of claim 1, wherein the contact layer (111) comprises one of NiSi and Ni(Pt)Si2-y.

### Claim 5 (depends on 1)

The method of claim 1, wherein the step h) comprises:
forming a metal layer to cover the exposed area of the source/drain regions (110) and sidewalls of the contact holes (310);
implementing a first annealing such that the metal layer reacts with the exposed area of the source/drain regions (110) and with sidewalls of the contact holes (310) in the amorphous Si layer (251) so as to form a contact layer (111); and
removing the unreacted metal layer.

### Claim 6 (depends on 5)

The method of claim 5, wherein
the metal layer comprises one of Ni and NiPt.

### Claim 7 (depends on 5)

The method of claim 5, wherein
if the material of the metal layer is NiPt, the content of Pt therein is less than 5%.

### Claim 8 (depends on 5)

The method of claim 5, wherein the metal layer has a thickness that ranges from 10 nm to 25 nm.

### Claim 9 (depends on 5)

The method of claim 5, wherein
the annealing is performed at a temperature between 500° C. to 600° C.

### Claim 10 (depends on 5)

The method of claim 5, wherein the contact layer (111) has a thickness that ranges from 15 nm to 35 nm.

### Claim 11 (depends on 1)

The method of claim 1, wherein prior to filling the first conductive material (280), the step f) further comprises:
implementing a second annealing to repair the structure that has been formed before filling the first conductive material.

### Claim 12

A semiconductor structure, which comprises:
a substrate (100);
a gate stack structure formed on the substrate (100);
source/drain regions formed within the substrate (100) and located on both sides of the gate stack structure;
a doped amorphous Si layer (251) that covers the source/drain regions (110);
an interlayer dielectric layer (300) that covers the doped amorphous Si layer (251) and the gate stack structure;
contact vias (320), which are made of a second conductive material, penetrating through the interlayer dielectric layer (300) and the amorphous Si layer (251) and being electrically connected with the source/drain regions (110); wherein
a contact layer (111) is formed between the contact vias (320) and the source/drain regions (110), and between the contact vias (320) and the amorphous Si layer (251).

### Claim 13 (depends on 12)

The semiconductor structure of claim 12, wherein
the contact layer (111) comprises one of NiSi and Ni(Pt)Si2-y.

### Claim 14 (depends on 12)

The semiconductor structure of claim 12, wherein
the contact layer (111) has a thickness that ranges from 15 nm to 35 nm.

### Claim 15 (depends on 12)

The semiconductor structure of claim 12, wherein
the contact vias (320) penetrate into the source/drain regions (110).

### Claim 16 (depends on 6)

The method of claim 6, wherein
the metal layer has a thickness that ranges from 10 nm to 25 nm.

### Claim 17 (depends on 6)

The method of claim 6, wherein
the annealing is performed at a temperature between 500° C. to 600° C.