# US 2013/0240976 A1 · Nonvolatile semiconductor memory device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240976 A1
- Document ID: US20130240976A1
- Status: Published application
- Kind: A1
- Application number: 13/601,266
- Filed: 2012-08-31
- Published: 2013-09-19
- Earliest claimed: 2012-03-19
- Assignees: Kabushiki Kaisha Toshiba
- Inventors: Masayuki TANAKA
- Web page: https://patentgrep.com/patent/US20130240976A1

## CPC

- H10P 14/6524: {the substance being nitrogen}
- H10B 41/30: characterised by the memory core region
- H10D 30/69: IGFETs having charge trapping gate insulators, e.g. MNOS transistors
- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

In accordance with an embodiment, a nonvolatile semiconductor memory device includes a substrate including a semiconductor layer including an active region, a first insulating film on the active region, a charge storage layer on the first insulating film, an element isolation insulating film defining the active region, a second insulating film, and a control electrode on the second insulating film. The top surface of the element isolation insulating film is placed at a height between the top surface and the bottom surface of the charge storage layer, thereby forming a step constituted of the charge storage layer and the element isolation insulating film. The second insulating film covers the step and the charge storage layer. The second insulating film includes a first silicon oxide film and a first silicon nitride film on the first silicon oxide film. Nitrogen concentration in the first silicon nitride film is non-uniform.

## Claims

### Claim 1

A nonvolatile semiconductor memory device comprising:
a substrate comprising a semiconductor layer thereon, the semiconductor layer comprising an active region;
a first insulating film on the active region of the semiconductor layer;
a charge storage layer on the first insulating film;
an element isolation insulating film defining the active region in the semiconductor layer, a top surface of the element isolation insulating film being placed at a height between a top surface and a bottom surface of the charge storage layer, thereby forming a step constituted of the charge storage layer and the element isolation insulating film;
a second insulating film covering the step and the charge storage layer; and
a control electrode on the second insulating film,
wherein the second insulating film comprises a first silicon oxide film and a first silicon nitride film on the first silicon oxide film, and
nitrogen concentration in the first silicon nitride film is non-uniform.

### Claim 2 (depends on 1)

The device of claim 1,
wherein the nitrogen concentration in the first silicon nitride film is higher in corner portions of an upper region covering the charge storage layer and corner portions of a lower region on the element isolation insulating film than any other regions.

### Claim 3 (depends on 1)

The device of claim 1,
wherein the nitrogen concentration in the first silicon nitride film is higher in an upper region covering the charge storage layer and a lower region on the element isolation insulating film than any other regions.

### Claim 4 (depends on 2)

The device of claim 2,
wherein, in addition to the corner portions of the upper region covering the charge storage layer and the corner portions of the lower region on the element isolation insulating film, the nitrogen concentration in the first silicon nitride film is also higher in a region along a side surface of the charge storage layer than any other regions.

### Claim 5 (depends on 4)

The device of claim 4,
wherein, in addition to the corner portions of the upper region covering the charge storage layer, the lower region on the element isolation insulating film, and the region along the side surface of the charge storage layer, the nitrogen concentration in the first silicon nitride film is higher in a region on the top surface of the charge storage layer than any other regions.

### Claim 6 (depends on 1)

The device of claim 1,
wherein the second insulating film further comprises a second silicon oxide film on the first silicon nitride film.

### Claim 7 (depends on 6)

The device of claim 6,
wherein the second insulating film further comprises a second silicon nitride film on the second silicon oxide film.

### Claim 8 (depends on 6)

The device of claim 6,
wherein the second insulating film further comprises a third silicon nitride film on the first silicon oxide film.

### Claim 9 (depends on 8)

The device of claim 8,
wherein the second insulating film further comprises a fourth silicon nitride film on the second silicon oxide film.

### Claim 10

A manufacturing method of a nonvolatile semiconductor memory device comprising:
forming a first insulating film on an active region of a semiconductor layer on a substrate;
forming a charge storage layer on the first insulating film;
forming an element isolation insulating film defining the active region in the semiconductor layer in such a manner that its top surface is placed at a height between a top surface and a bottom surface of the charge storage layer;
forming a second insulating film so as to cover a step constituted of the charge storage layer and the element isolation insulating film and cover the charge storage layer; and
forming a control electrode on the second insulating film,
wherein forming the second insulating film comprises:
sequentially forming a first silicon oxide film and a first silicon nitride film; and
introducing nitrogen to the first silicon nitride film so as to provide non-uniform nitrogen concentration.

### Claim 11 (depends on 10)

The method of claim 10,
wherein the nitrogen is introduced to the first silicon nitride film by an anisotropic nitriding method using a nitrogen radical.

### Claim 12 (depends on 11)

The method of claim 11,
wherein introducing the nitrogen comprises applying a bias voltage to the substrate;

### Claim 13 (depends on 10)

The method of claim 10,
wherein the nitrogen is introduced by an ion implantation method using an injection angle of 15 degrees or above.

### Claim 14 (depends on 10)

The method of claim 10, further comprising forming a mask with which an edge region of an upper surface of the first silicon nitride film on the charge storage layer and an edge region of a step bottom portion between cells are exposed in the first silicon nitride film before introducing the nitrogen.

### Claim 15 (depends on 14)

The method of claim 14,
wherein introducing the nitrogen further comprises applying a bias voltage to the substrate.

### Claim 16 (depends on 14)

The method of claim 14,
wherein the nitrogen is uniformly introduced in a sidewall region of the first silicon nitride film along a side surface of the charge storage layer, an edge region of an upper surface of the first silicon nitride film on the charge storage layer, and an edge region of a step bottom portion between cells in the first silicon nitride film.

### Claim 17 (depends on 10)

The method of claim 10, further comprising forming a second silicon oxide film on the first silicon nitride film.

### Claim 18 (depends on 17)

The method of claim 17, further comprising forming a second silicon nitride film between the charge storage layer and the first silicon oxide film.

### Claim 19 (depends on 18)

The method of claim 18, further comprising forming a third silicon nitride film on the second silicon oxide film.

### Claim 20 (depends on 17)