# US 2013/0240895 A1 · Semiconductor element having high breakdown voltage

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240895 A1
- Document ID: US20130240895A1
- Status: Published application
- Kind: A1
- Application number: 13/571,041
- Filed: 2012-08-09
- Published: 2013-09-19
- Earliest claimed: 2012-03-16
- Assignees: National Central University
- Inventors: Jen-Inn CHYI; Geng-Yen Lee; Hsueh-Hsing Liu
- Web page: https://patentgrep.com/patent/US20130240895A1

## CPC

- H10D 8/051: {of Schottky diodes}
- H10D 8/60: Schottky-barrier diodes
- H10D 30/4755: {having wide bandgap charge-carrier supplying layers, e.g. modulation doped HEMTs such as n-AlGaAs/GaAs HEMTs}
- H10D 30/6738: {Schottky barrier electrodes}
- H10D 30/675: {Group III-V materials, Group II-VI materials, Group IV-VI materials, selenium or tellurium}
- H10D 62/85: being Group III-V materials, e.g. GaAs
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D 64/513: {within recesses in the substrate, e.g. trench gates, groove gates or buried gates}
- H10D 64/64: Electrodes comprising a Schottky barrier to a semiconductor
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor element having a high breakdown voltage includes a substrate, a buffer layer, a semiconductor composite layer and a bias electrode. The buffer layer disposed on the substrate includes a high edge dislocation defect density area. The semiconductor composite layer disposed on the buffer layer includes a second high edge dislocation defect density area formed due to the first high edge dislocation defect density area. The bias electrode is disposed on the semiconductor composite layer. A virtual gate effect of defect energy level capturing electrons is generated due to the first and second high edge dislocation defect density areas, such that an extended depletion region expanded from the bias electrode is formed at the semiconductor composite layer. When the bias electrode receives a reverse bias, the extended depletion region reduces a leakage current and increases the breakdown voltage of the semiconductor element.

## Claims

### Claim 1

A semiconductor element having a high breakdown voltage, comprising:
a substrate;
a buffer layer, disposed on the substrate, comprising a first high edge dislocation defect density area;
a semiconductor composite layer, disposed on the buffer layer, comprising a second high edge dislocation defect density area formed due to the first high edge dislocation defect density area; and
a bias electrode, disposed on the semiconductor composite layer;
wherein, the first and second high edge dislocation defect density areas generating a virtual gate effect of defect energy level capturing electrons to form an extended depletion region expanded from the bias electrode at the semiconductor composite layer.

### Claim 2 (depends on 1)

The semiconductor element of claim 1, wherein the semiconductor composite layer comprises a barrier layer located away from the buffer layer, and a channel layer located adjacent to the barrier layer and between the barrier layer and the buffer layer, and the barrier layer has an energy level greater than that of the channel layer.

### Claim 3 (depends on 2)

The semiconductor element of claim 2, wherein the channel layer is formed from a material selected from the group consisting of GaN, AlGaN and InAlGaN.

### Claim 4 (depends on 2)

The semiconductor element of claim 2, wherein a full-width at half-maximum (FWHM) value of an X-ray rocking curve (XRC) at a (0002) plane of the second high edge dislocation defect density area is smaller than 250 arc seconds, and the FWHM value of the XRC at a (1-102) plane of the second high edge dislocation defect density area is between 500 and 2500 arc seconds.

### Claim 5 (depends on 2)

The semiconductor element of claim 2, wherein the barrier layer is formed from a material selected from the group consisting of AlGaN, AlInN and AlGaInN.

### Claim 6 (depends on 1)

The semiconductor element of claim 1, wherein the buffer layer is formed from a material of AlN.

### Claim 7 (depends on 1)

The semiconductor element of claim 1, wherein an FWHM value of an XRC at a (0002) plane of the first high edge dislocation defect density area is smaller than 150 arc seconds, and the FWHM value of the XRC at a (1-102) plane of the first high edge dislocation defect density area is between 1000 and 5000 arc seconds.

### Claim 8 (depends on 1)

The semiconductor element of claim 1, wherein a temperature for developing the buffer layer is between 1100° C. and 1200° C.

### Claim 9 (depends on 1)

The semiconductor element of claim 1, further comprising an intermediate layer disposed between the buffer layer and the semiconductor composite layer.

### Claim 10 (depends on 9)

The semiconductor element of claim 9, wherein the intermediate layer is formed from a material selected from the group consisting of GaN, AlGaN and AlInN.

### Claim 11 (depends on 1)

The semiconductor element of claim 1, further comprising a cladding layer disposed between the bias electrode and the semiconductor composite layer.

### Claim 12 (depends on 11)

The semiconductor element of claim 11, wherein the cladding layer is formed from a material of GaN or GaInN.