# US 2013/0240874 A1 · Layered film including heteroepitaxial pn junction oxide thin film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240874 A1
- Document ID: US20130240874A1
- Status: Published application
- Kind: A1
- Application number: 13/790,398
- Filed: 2013-03-08
- Published: 2013-09-19
- Earliest claimed: 2012-03-14
- Assignees: TDK Corporation
- Applicants: TDK Corporation
- Inventors: Kazuya MAEKAWA; Kunihiro UEDA
- Web page: https://patentgrep.com/patent/US20130240874A1

## CPC

- H10D 8/045: {of PN junction diodes}
- H10D 8/00: Diodes (variable-capacitance diodes H10D1/64; gated diodes H10D12/00)
- H10D 62/80: characterised by the materials
- H10D 62/81: of structures exhibiting quantum-confinement effects, e.g. single quantum wells; of structures having periodic or quasi-periodic potential variation
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3234: {being oxide semiconducting materials (Group IIB-VIA semiconductors H10P14/3224)}
- H10P 14/3238: {being insulating materials}
- H10P 14/3241: {being conductive materials}
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3434: {being oxide semiconductor materials (Group IIB-VIA semiconductor materials H10P14/3424)}
- H10P 14/3442: {N-type}
- H10P 14/3444: {P-type}
- H10P 14/3446: {Transition metal elements; Rare earth elements}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Semiconductors of different types are formed by a crystal growth technique and joined at the interface at which rapid atomic-layer-level compositional changes occur while maintaining high crystallinity of the semiconductor layers so as to form a heterogeneous PN junction. A layered film that includes a PN junction oxide thin film is formed on a single crystal substrate. The PN junction oxide thin film is constituted by an N-type semiconductor oxide thin film and a P-type semiconductor oxide thin film that are epitaxially grown to have c-axis orientation represented by (00k).

## Claims

### Claim 1

A layered film formed on a single crystal substrate, comprising:
a heteroepitaxial PN junction oxide thin film including an N-type semiconductor oxide thin film and a P-type semiconductor oxide thin film that are each epitaxially grown to have c-axis orientation represented by (00k).

### Claim 2 (depends on 1)

The layered film according to claim 1, further comprising:
an epitaxially grown buffer layer containing ZrO2 and Y2O3 and serving as an underlayer for the heteroepitaxial PN junction oxide thin film; and
an epitaxially grown metal thin film disposed between the heteroepitaxial PN junction oxide thin film and the buffer layer, the metal thin film containing at least one element selected from the group consisting of Pt, Ir, Pd, Ru, and Rh.

### Claim 3 (depends on 1)

The layered film according to claim 1 wherein the N-type semiconductor oxide thin film is composed of a doped perovskite-type compound represented by R(Mx,Dy)O3 or (Rx,Dy)MO3 obtained by doping a perovskite-type compound represented by general formula RMO3 with a metal D other than R and M, and the amount of the metal D is adjusted to x+y=1 and 0.03≦y≦0.3 to control epitaxial growth of the P-type semiconductor oxide thin film on the N-type semiconductor oxide thin film so that the P-type semiconductor oxide thin film has c-axis orientation represented by (00k).

### Claim 4 (depends on 3)

The layered film according to claim 3, wherein, in the doped perovskite-type compound represented by R(Mx,Dy)O3 or (Rx,Dy)MO3, R is selected from the group consisting of Ba, Ca, Fe, K, La, Li, Mg, Mn, Na, Sr, and Zn, M is selected from the group consisting of Co, Fe, Hf, La, Mn, Nb, Ni, Si, Sn, Ta, Ti, and Zr, and D is selected from the group consisting of Al, Ba, Ca, Ce, Co, Cr, Fe, Hf, K, La, Mg, Mn, Na, Nb, Ni, Sn, Sr, V, Y, Zn, and Zr.

### Claim 5 (depends on 1)

The layered film according to claim 1, wherein the P-type semiconductor oxide thin film is composed of a material selected from the group consisting of SnO, NiO, and Cu2O.

### Claim 6 (depends on 1)

The layered film according to claim 1, wherein, when an oriented surface of a stack constituted by the N-type semiconductor oxide thin film and the P-type semiconductor oxide thin film is subjected to x-ray diffraction, the highest intensity of a reflection peak of a plane other than a c-axis-oriented plane represented by (00k) is 10% or less of the intensity of a reflection peak of the c-axis-oriented plane.

### Claim 7 (depends on 1)

The layered film according to claim 1, wherein, when the N-type semiconductor oxide thin film and the P-type semiconductor oxide thin film are analyzed by x-ray diffraction through rocking curve scan of a c-axis-oriented plane represented by (00k), at least one of the N-type semiconductor oxide thin film and the P-type semiconductor oxide thin film exhibits a full-width half-maximum of 0.8° or less.

### Claim 8 (depends on 1)

The layered film according to claim 1, wherein the differences in rotation angle between the in-plane surface orientation of the single crystal substrate and the in-plane surface orientation of the N-type semiconductor oxide thin film and between the in-plane surface orientation of the single crystal substrate and the in-plane surface orientation of the P-type semiconductor oxide thin film are 1° or less.

### Claim 9 (depends on 1)

The layered thin film according to claim 1, wherein the single crystal substrate is composed of a material selected from the group consisting of Si, MgO, SrTiO3, and LiNbO3.

### Claim 10 (depends on 2)

The layered film according to claim 2, wherein the N-type semiconductor oxide thin film is composed of a doped perovskite-type compound represented by R(Mx,Dy)O3 or (Rx,Dy)MO3 obtained by doping a perovskite-type compound represented by general formula RMO3 with a metal D other than R and M, and the amount of the metal D is adjusted to x+y=1 and 0.03≦y≦0.3 to control epitaxial growth of the P-type semiconductor oxide thin film on the N-type semiconductor oxide thin film so that the P-type semiconductor oxide thin film has c-axis orientation represented by (00k).