# US 2013/0240805 A1 · Uranium Dioxide Nuclear Fuel Containing Mn and Al as Additives and Method of Fabricating the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240805 A1
- Document ID: US20130240805A1
- Status: Published application
- Kind: A1
- Application number: 12/544,497
- Filed: 2009-08-20
- Published: 2013-09-19
- Earliest claimed: 2008-11-11
- Assignees: Korea Hydro & Nuclear Power Co., Ltd.; Korea Atomic Energy Research Institute
- Inventors: Ki Won Kang; Jae Ho Yang; Keon Sik Kim; Young Woo Rhee; Jong Hun Kim; Kun Woo Song
- Web page: https://patentgrep.com/patent/US20130240805A1

## CPC

- G21C 3/04: Constructional details
- G21C 3/623: {Oxide fuels}
- G21C 3/17: Means for storage or immobilisation of gases in fuel elements
- G21C 3/18: Internal spacers or other non-active material within the casing, e.g. compensating for expansion of fuel rods or for compensating excess reactivity (interlayers G21C3/20)
- G21C 3/58: Solid reactor fuel {Pellets made of fissile material}
- G21C 21/00: Apparatus or processes specially adapted to the manufacture of reactors or parts thereof (in general section B, e.g. B23)
- Y02E 30/30: Nuclear fission reactors
- G21C: NUCLEAR REACTORS (fusion reactors, hybrid fission-fusion reactors G21B; nuclear explosives G21J)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

UO2 nuclear fuel pellets are fabricated by adding additive powder comprising Mn compound and Al compound into UO2 powder.

## Claims

### Claim 1

Nuclear fuel pellets comprising:
UO2;
MnO as an additive; and
Al2O3 as an additive,
wherein Mn/Al ratio of the additives in the nuclear fuel pellets is 1 to 100 by weight, and (Mn+Al)/U ratio of the additives to UO2 in the nuclear fuel pellets is 50 μg/g to 3000 μg/g.

### Claim 2

(canceled)

### Claim 3

A method for fabricating nuclear fuel pellets, the method comprising:
preparing mixture powder by mixing additive powder comprising MnO and Al2O3 with UO2 powder;
compacting the mixture powder to produce green pellets; and
sintering the green pellets at a temperature of 1,600° C. to 1,800° C. under a reducing gas atmosphere,
wherein when the mixture powder of the additive powder and the UO2 powder is prepared, the additive powder is mixed with UO2 powder in such a way that (Mn+Al)/U ratio in the mixture powder is 50 μg/g to 3,000 μg/g, and Mn/Al ratio of the additive powder is 1 to 100 by weight.

### Claim at position 4

4-6. (canceled)

### Claim 7 (depends on 3)

The method of claim 3, wherein, in sintering the green pellets, the reducing gas atmosphere is a hydrogen-containing gas atmosphere.

### Claim 8 (depends on 7)

The method of claim 7, wherein the hydrogen-containing gas is hydrogen-containing mixture gas, which contains hydrogen gas and at least one selected from the group consisting of carbon dioxide, water vapor and inert gas.

### Claim 9 (depends on 7)

The method of claim 7, wherein the hydrogen-containing gas is hydrogen gas.