# US 2013/0240785 A1 · Halo-borate luminescent materials and preparation methods thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240785 A1
- Document ID: US20130240785A1
- Status: Published application
- Kind: A1
- Application number: 13/885,275
- Filed: 2010-12-14
- Published: 2013-09-19
- Earliest claimed: 2010-12-14
- Assignees: Ocean's King Lighting Science & Technology Co., Ltd.
- Inventors: Mingjie Zhou; Qiurong Liao; Wenbo Ma
- Web page: https://patentgrep.com/patent/US20130240785A1

## CPC

- C09K 11/87: containing platina group metals
- C09K 11/774: {Borates}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

Halo-borate luminescent materials and preparation methods thereof are provided. The said luminescent materials are represented by the following general formula: Ca2-xBO3Cl1-yFy:xEu2+, zM0, wherein M0 is selected from one of Ag, Au, Pt, Pd or Cu metal nano-particles; 0.001≦x≦0.1, 0≦y≦0.2, 0≦z≦0.01. The said luminescent materials have excellent chemical stability and high luminous intensity. The said preparation methods have simple technique, no pollution, manageable process conditions and low equipment requirement, and are beneficial to industry production.

## Claims

### Claim 1

A halogen borate phosphor, represented by the following general formula:
Ca2-xBO3Cl1-yFy:xEu2+,zM0;
wherein M0 represents metal nano-particles selected from the group consisting of Ag, Au, Pt, Pd and Cu; 0.001≦x≦0.1, 0≦y≦0.2, 0≦z≦0.01.

### Claim 2 (depends on 1)

The halogen borate phosphor according to claim 1, wherein 1×10−4≦z≦1×10−3.

### Claim 3

A method of preparing a halogen borate phosphor, comprising the following steps:
step S1, weighing and dissolving calcium source compound, boron source compound, chlorine source compound, fluorine source compound, and europium source compound in water according to a composition of a formula of Ca2-xBO3Cl1-yFy:xEu2+, zM0 to prepare a mixed solution, wherein 0.001≦x≦0.1, 0≦y≦0.2;
step S2, adding chelating agent and crosslinking agent successively to the mixed solution obtained in the step S1 to prepare a chelate solution;
step S3, adding surface-treated nano-particle sol of M0 to the chelate solution prepared in step S2, stirring and heating in a water bath, drying to obtain a precursor, wherein M0 represents metal nano-particles selected from the group consisting of Ag, Au, Pt, Pd and Cu; and
step S4, pre-sintering, cooling, grinding, and then calcining the precursor obtained in step S3 in a reducing atmosphere, cooling, grinding to obtain the halogen borate phosphor represented by the following general formula: Ca2-xBO3Cl1-yFy:xEu2+, zM0.

### Claim 4 (depends on 3)

The method according to claim 3, wherein in step S1, the calcium source compound is calcium nitrate, calcium chloride, or calcium fluoride; the boron source compound is boric acid or tributyl borate; the chlorine source compound is calcium chloride or ammonium chloride; the fluorine source compound is calcium fluoride or ammonium fluoride; the europium source compound is europium nitrate, europium chloride, fluoride, or europium.

### Claim 5 (depends on 3)

The method according to claim 3, wherein in step S2, the chelating agent is citric acid, and a molar ratio of the chelating agent to the total metal ions in the mixed solution is 1:1 to 3:1; the crosslinking agent is polyethylene glycol with a molecular weight of 10,000, and a molar ratio of the crosslinking agent to the total metal ions in the mixed solution is 0.5% to 1%.

### Claim 6 (depends on 3)

The method according to claim 3, wherein in step S3, the surface-treated nano-particle sol of M0 is prepared according to the following steps:
step S31, weighing and dissolving an M0 source compound in water to prepare and dilute a solution with a molar concentration of M0 ion of 1×10−4 mol/L to 1×10−2 mol/L; wherein M0 represents metal nano-particles selected from the group consisting of Ag, Au, Pt, Pd and Cu;
step S32, adding an additive and a reducing agent solution successively to the solution prepared in step S31, stirring and obtaining an M0 nanoparticles sol; and
step S33, adding a surface treatment agent to the M0 nanoparticles sol obtained in step S32, stirring to obtain the surface-treated M0 nanoparticles sol.

### Claim 7 (depends on 6)

The preparation method according to claim 6, wherein in step S32,
the additive is at least one selected from the group consisting of polyvinylpyrrolidone, sodium citrate, cetyl trimethyl ammonium bromide, sodium lauryl sulfate, and sodium dodecyl sulfate; and the concentration of the additive in the M0 nanoparticles sol is from 1.5×10−4 g/mL to 2.1×10−3 g/mL;
a molar concentration of the reducing agent solution is from 1×10−3 mol/L to 1×10−2 mol/L;
a reducing agent in the reducing agent solution is at least one selected from the group consisting of hydrazine, ascorbic acid, and sodium borohydride; a molar ratio of the reducing agent and the M0 ion is 1.2:1 to 4.8:1.

### Claim 8 (depends on 6)

The preparation method according to claim 6, wherein in step S33, the surface treatment agent is polyvinylpyrrolidone; the content of the surface treatment agent in the M0 nanoparticles sol is from 0.001 g/mL to 0.1 g/mL.

### Claim 9 (depends on 3)

The preparation method according to claim 3, wherein in step S3, the process of stirring and heating in a water bath comprises: stirring and heating in a 70° C. to 90° C. water bath for 2 hours to 6 hours; a temperature of the drying process is 80° C. to 150° C.

### Claim 10 (depends on 3)

The preparation method according to claim 3, wherein in step S4, the process of pre-sintering comprises: pre-sintering at a temperature of 500° C. to 800° C. for 2 hours to 7 hours; the process of calcining comprises: calcining the precursor at a temperature of 800° C. to 1200° C. for 2 hours to 6 hours.