# US 2013/0240606 A1 · Tool for ultrasonic welding device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240606 A1
- Document ID: US20130240606A1
- Status: Published application
- Kind: A1
- Application number: 13/796,623
- Filed: 2013-03-12
- Published: 2013-09-19
- Earliest claimed: 2012-03-14
- Assignees: Telsonic Holding AG; Friedrich-Alexander-Universitaet Erlangen-Nuernberg
- Inventors: Georg LANG; Stefan ROSIWAL; Matthias LODES; Katharina NEUERER
- Web page: https://patentgrep.com/patent/US20130240606A1

## CPC

- B23K 20/106: {Features related to sonotrodes}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

The invention relates to a tool for an ultrasonic welding device, wherein a contact face of a carrier body (1) produced from a metal facing a component to be welded is provided with a diamond coating (3). To improve the durability, it is proposed in accordance with the invention for the diamond coating to be produced by means of CVD methods and to have a thickness (D2) in the range from 0.5 to 20 μm.

## Claims

### Claim 1

A tool for an ultrasonic welding device, wherein a contact face of a carrier body (1) produced from a metal facing a component part to be welded is provided with a diamond coating (3),
characterised in that
the diamond coating (3) is produced by means of a CVD method and has a thickness (D2) in the range from 0.5 to 20 μm.

### Claim 2 (depends on 1)

The tool according to claim 1, wherein the diamond coating (3) has a thickness in the range from 1 to 15 μm, preferably 1.5 to 5.0 μm.

### Claim 3 (depends on 1)

The tool according to claim 1, wherein, in the Raman spectrum, the diamond coating (3) has a first peak in the range from 1335 to 1345 l/cm and a second peak in the range from 1345 to 1355 l/cm.

### Claim 4 (depends on 1)

The tool according to claim 1, wherein the thickness (D2) of the diamond coating (3) deviates by at most 10% compared to an average thickness of the diamond coating (D3).

### Claim 5 (depends on 1)

The tool according to claim 1, wherein an average diameter of the diamond crystal (4) forming the diamond coating (3) is 0.05 μm to 20 μm, preferably 0.5 to 3.0 μm, at a surface (O) of the diamond coating (3).

### Claim 6 (depends on 1)

The tool according to claim 1, wherein a thermal conductivity of the diamond coating (3) is 2 to 2000 W/mk.

### Claim 7 (depends on 1)

The tool according to claim 1, wherein the diamond crystals (4) contain 50 to 100000 ppm of boron.

### Claim 8 (depends on 1)

The tool according to claim 1, wherein an electrical resistivity of the diamond coating (3) is 10−3 to 104 S/m.

### Claim 9 (depends on 1)

The tool according to claim 1, wherein the carrier body (1) is produced from titanium, titanium alloy, molybdenum, molybdenum alloy, tungsten, tungsten alloy or hard metal.

### Claim 10 (depends on 9)

The tool according to claim 9, wherein a TiC coating (2) having a further thickness (D1) in the range from 10 nm to 2.0 μm, preferably 0.5 to 2.0 μm, is incorporated between the carrier body (1) produced from titanium or the titanium alloy and the diamond coating (3).

### Claim 11 (depends on 9)

The tool according to claim 9, wherein an intermediate coating (2) consisting of chromium carbide or TiN is incorporated between the carrier body (1), produced from steel, and the diamond coating (3).

### Claim 12 (depends on 11)

The tool according to claim 11, wherein the intermediate coating (2) has a further thickness (D2) in the range from 1 to 50 μm.

### Claim 13 (depends on 1)

The tool according to claim 1, comprising at least one of the following elements: sonotrode, anvil, lateral slide.

### Claim 14 (depends on 1)

The tool according to claim 1, wherein the carrier body (1) is formed as an insert for insertion into a corresponding recess on the anvil.