# US 2013/0240448 A1 · Method for separating water by separation membrane, separation membrane for dehydrating aqueous organic acid solution and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240448 A1
- Document ID: US20130240448A1
- Status: Published application
- Kind: A1
- Application number: 13/782,076
- Filed: 2013-03-01
- Published: 2013-09-19
- Earliest claimed: 2012-03-14
- Assignees: Hitachi Zosen Corporation
- Applicants: Hitachi Zosen Corporation
- Inventors: Kenichi Sawamura; Masanobu Aizawa; Kentaro Shinoya; Yoshinobu Takaki; Kazuhiro Yano
- Web page: https://patentgrep.com/patent/US20130240448A1

## CPC

- C02F 1/44: by dialysis, osmosis or reverse osmosis {(general membrane separation processes B01D61/00, membrane modules B01D63/00, electrodialysis C02F1/4693, combination of membrane modules and bioreactors C02F3/1268)}
- B01D 67/0051: {by controlled crystallisation, e,.g. hydrothermal growth}
- B01D 71/0281: {Zeolites}
- B01D 2323/08: Specific temperatures applied
- B01D 2323/48: Influencing the pH
- B01D 2325/02831: less than 1 nm
- B01D 2325/28: Degradation or stability over time
- B01D 2325/42: Ion-exchange membranes
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)

## Abstract

The method for separating water by a separation membrane is a method for separating water from an aqueous organic acid solution by the separation membrane, and the separation membrane consists of polycrystalline membrane of mordenite (the chemical composition of the frame: AlnSi40-nO96, 2≦n≦, further, a major component of exchangeable cations present in ion exchange sites of the mordenite is protons (H+). The separation membrane for dehydrating an aqueous organic acid solution exhibits unexpectedly remarkable water permeability and has excellent acid resistance, without damaging water separation selectivity. The method for separating water using this separation membrane enables, for example, realizing the process of dehydrating acetic acid by the separation membrane, and a great energy saving. There are provided the above-described separation membrane for dehydrating an aqueous organic acid solution, and the method for manufacturing it.

## Claims

### Claim 1

A method for separating water from an aqueous organic acid solution by a separation membrane, wherein the separation membrane consists of mordenite (the chemical composition of the frame: AlnSi40-nO96, 2≦n≦8) polycrystalline membrane and further, a major component of exchangeable cations present in ion exchange sites of the mordenite is protons (H+).

### Claim 2 (depends on 1)

The method for separating water by the separation membrane according to claim 1 wherein the organic acid is acetic acid.

### Claim 3 (depends on 1)

The separation membrane for dehydrating an aqueous organic acid solution used in the method for separating water according to claim 1, wherein the membrane consists of mordenite (the chemical composition of the frame AlnSi40-nO96, 2≦n≦8) polycrystalline membrane, and further wherein a major component of exchangeable cations present in ion exchange sites of the mordenite is protons (H+), and the mordenite polycrystalline membrane is obstructed by the connection of pore paths parallel to the c-axes with pores oriented in the different direction, the pore paths parallel to the c-axes being formed by at least 12-membered rings, that is, the largest pore among pores consisting of 4, 5, 6, 8, and 12-membered oxygen rings.

### Claim 4 (depends on 3)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according to claim 3, wherein the suspension of the mordenite species crystal powder is applied to the surface of a porous support and dried, then the porous support having the mordenite species crystal powder on the surface is subjected to hydrothermal synthesis in a synthesis solution containing SiO2 and Al2O3 to form the mordenite polycrystalline membrane, after that, cation species present in the ion exchange sites are ion-exchanged with protons (H+) using an acidic solution.

### Claim 5 (depends on 4)

A method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according to claim 4, wherein the porous support is comprised of at least one porous body selected from the group consisting of alumina, silica and zirconia.

### Claim 6 (depends on 4)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according to claim 4, wherein the synthesis solution in hydrothermal synthesis has a molar composition (100≦SiO2/Al2O3≦400).

### Claim 7 (depends on 4)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according to claim 4, wherein the synthesis solution in hydrothermal synthesis contains further Na2O, and has a molar composition (40≦H2O/Na2O≦120, 0.1≦Na2O/SiO2≦0.4, 100≦SiO2/Al2O3≦400).

### Claim 8 (depends on 4)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 4, wherein the reaction temperature in hydrothermal synthesis is 100-200° C. and the reaction time is 4-48 hours.

### Claim 9 (depends on 4)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 4, wherein the acidic solution used in the treatment of ion exchange with protons is an acidic solution with pH 1-3 comprised of at least one of hydrochloric acid, nitric acid and acetic acid.

### Claim 10 (depends on 5)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according to claim 5, wherein the synthesis solution in hydrothermal synthesis has a molar composition (100≦SiO2/Al2O3≦400).

### Claim 11 (depends on 5)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according to claim 5, wherein the synthesis solution in hydrothermal synthesis contains further Na2O, and has a molar composition (40≦H2O/Na2O≦120, 0.1≦Na2O/SiO2≦0.4, 100≦SiO2/Al2O3≦400).

### Claim 12 (depends on 5)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 5, wherein the reaction temperature in hydrothermal synthesis is 100-200° C. and the reaction time is 4-48 hours.

### Claim 13 (depends on 6)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 6, wherein the reaction temperature in hydrothermal synthesis is 100-200° C. and the reaction time is 4-48 hours.

### Claim 14 (depends on 7)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 7, wherein the reaction temperature in hydrothermal synthesis is 100-200° C. and the reaction time is 4-48 hours.

### Claim 15 (depends on 10)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 10, wherein the reaction temperature in hydrothermal synthesis is 100-200° C. and the reaction time is 4-48 hours.

### Claim 16 (depends on 11)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 11, wherein the reaction temperature in hydrothermal synthesis is 100-200° C. and the reaction time is 4-48 hours.

### Claim 17 (depends on 5)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 5, wherein the acidic solution used in the treatment of ion exchange with protons is an acidic solution with pH 1-3 comprised of at least one of hydrochloric acid, nitric acid and acetic acid.

### Claim 18 (depends on 6)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 6, wherein the acidic solution used in the treatment of ion exchange with protons is an acidic solution with pH 1-3 comprised of at least one of hydrochloric acid, nitric acid and acetic acid.

### Claim 19 (depends on 7)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 7, wherein the acidic solution used in the treatment of ion exchange with protons is an acidic solution with pH 1-3 comprised of at least one of hydrochloric acid, nitric acid and acetic acid.

### Claim 20 (depends on 8)

The method for manufacturing the separation membrane for dehydrating an aqueous organic acid solution according claim 8, wherein the acidic solution used in the treatment of ion exchange with protons is an acidic solution with pH 1-3 comprised of at least one of hydrochloric acid, nitric acid and acetic acid.