# US 2013/0240368 A1 · Low internal stress copper electroplating method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240368 A1
- Document ID: US20130240368A1
- Status: Published application
- Kind: A1
- Application number: 13/607,737
- Filed: 2012-09-09
- Published: 2013-09-19
- Earliest claimed: 2011-09-09
- Assignees: Rohm and Haas Electronic Material LLC
- Inventors: George R. Allardyce; Gary Hamm; Narsmoul Karaya
- Web page: https://patentgrep.com/patent/US20130240368A1

## CPC

- C25D 7/06: Wires; Strips; Foils
- C25D 3/38: of copper
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Copper electroplating methods provide low internal stress copper deposits. Concentrations of accelerators in the copper electroplating bath vary as a function of the plating current density and the low internal stress copper deposit is observed as a matt copper deposit.

## Claims

### Claim 1

A method comprises:
a) contacting a substrate with a composition comprising one or more sources of copper ions, one or more suppressors and one or more accelerators in sufficient amounts to provide a copper deposit of matt appearance; and
b) applying a current to the substrate to achieve a current density at or below MattCDmax throughout the substrate to deposit the copper of matt appearance on the substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the accelerator is chosen from one or more of 3-mercaptopropane-1-sulfonic acid, ethylenedithiodipropyl sulfonic acid, bis-(ω-sulfobutyl)-disulfide, methyl-(ω-sulfopropyl)-disulfide, N,N-dimethyldithiocarbamic acid (3-sulfopropyl) ester, (O-ethyldithiocarbonato)-S-(3-sulfopropyl)-ester, 3-[(amino-iminomethyl)-thiol]-1-propanesulfonic acid, 3-(2-benzylthiazolylthio)-1-propanesulfonic acid, bis-(sulfopropyl)-disulfide and alkali metal salts thereof.

### Claim 3 (depends on 2)

The method of claim 2, wherein the one or more accelerators are at concentrations of 1 ppm and greater.

### Claim 4 (depends on 3)

The method of claim 3, wherein the current density is 50 ASD and lower.

### Claim 5 (depends on 1)

The method of claim 1, wherein the one or more sources of copper ion are chosen from copper sulfate and copper alkane sulfonates.

### Claim 6 (depends on 1)

The method of claim 1, wherein the suppressors are chosen from one or more of polyoxyalkylene glycol, carboxymethylcellulose, nonylphenolpolyglycol ether, octandiolbis-(polyalkylene glycolether), octanolpolyalkylene glycolether, oleic acidpolyglycol ester, polyethylenepropylene glycol, polyethylene glycol, polyethylene glycoldimethylether, polyoxypropylene glycol, polypropylene glycol, polyvinylalcohol, stearic acidpolyglycol ester and stearyl alcoholpolyglycol ether.