# US 2013/0240350 A1 · Electronic device housing and method for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240350 A1
- Document ID: US20130240350A1
- Status: Published application
- Kind: A1
- Application number: 13/893,584
- Filed: 2013-05-14
- Published: 2013-09-19
- Earliest claimed: 2009-12-28
- Assignees: FIH (Hong Kong) Limited; Shenzhen Futaihong Precision Industry Co., Ltd.
- Applicants: Shenzhen Futaihong Precision Industry Co., Ltd.; Fih (Hong Kong) Limited
- Inventors: CHWAN-HWA CHIANG; QI-JIAN DU
- Web page: https://patentgrep.com/patent/US20130240350A1

## CPC

- C09D 5/00: Coating compositions, e.g. paints, varnishes or lacquers, characterised by their physical nature or the effects produced {(electrically insulating plastics, resins or waxes H01B3/30)}; Filling pastes
- C03C 17/2456: {Coating containing TiO2}
- C04B 41/009: {characterised by the material treated}
- C04B 41/5041: {Titanium oxide or titanates}
- C04B 41/52: Multiple coating or impregnating {multiple coating or impregnating with the same composition or with compositions only differing in the concentration of the constituents, is classified as single coating or impregnation}
- C04B 41/87: Ceramics
- C04B 41/89: for obtaining at least two superposed coatings having different compositions
- C23C 14/083: {of refractory metals or yttrium}
- H05K 5/0243: {for decorative purposes}
- B82Y 99/00: Subject matter not provided for in other groups of this subclass
- C03C 2217/212: TiO2
- C03C 2217/71: Photocatalytic coatings
- C03C 2218/155: by reactive sputtering
- C04B 2111/00853: {in electrochemical cells or batteries, e.g. fuel cells}
- C04B 2111/2061: {Materials containing photocatalysts, e.g. TiO2, for avoiding staining by air pollutants or the like}
- Y10T 428/131: Glass, ceramic, or sintered, fused, fired, or calcined metal oxide or metal carbide containing [e.g., porcelain, brick, cement, etc.]
- Y10T 428/1317: Multilayer [continuous layer]
- Y10T 428/2495: Thickness [relative or absolute]
- Y10T 428/265: 1 mil or less
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An electronic device housing includes a substrate and a nano titanium dioxide coating formed on the substrate. The nano titanium dioxide coating has a thickness of about 10-100 nm. The nano titanium dioxide coating is formed of rutile crystals or composite crystals formed of rutile and anatase. A method for making the electronic device is also described.

## Claims

### Claim 1

A method for making electronic device housing, comprising:
providing a substrate;
vacuum sputtering a nano titanium dioxide coating on the substrate, the nano titanium dioxide coating being formed of rutile crystals or composite crystals formed of rutile and anatase, and having a thickness of about 10 nm to about 100 nm.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein vacuum sputtering the nano titanium dioxide coating is carried out by using oxygen gas and argon gas, the oxygen gas and the argon gas having a total pressure of about 0.05 Pa to about 0.29 Pa.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein the oxygen gas has a pressure of about 0.01 Pa to about 0.225 Pa.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein vacuum sputtering the nano titanium dioxide coating is carried out by using a titanium target, the titanium target is set with an output power of about 3000 W to about 4000 W.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the nano titanium dioxide coating is vacuum sputtered at a rate of about 0.3 nm/s to about 0.5 nm/s.

### Claim 6 (depends on 1)

The method as claimed in claim 1, further comprising a step of spraying a base paint coating on the substrate before forming the nano titanium dioxide coating.

### Claim 7 (depends on 6)

The method as claimed in claim 6, wherein spraying the base paint coating is carried out by using acrylic resin paint, epoxy resin paint, polyurethane resin paint, or phenolic resin paint.

### Claim 8 (depends on 6)

The method as claimed in claim 6, wherein the base paint coating has a thickness of about 1 μm to about 30 μm.