# US 2013/0240128 A1 · Method for producing carbonized film and method for producing graphite film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240128 A1
- Document ID: US20130240128A1
- Status: Published application
- Kind: A1
- Application number: 13/583,572
- Filed: 2011-03-09
- Published: 2013-09-19
- Earliest claimed: 2010-03-10
- Assignees: Kaneka Corporation
- Inventors: Makoto Mishiro; Yasushi Nishikawa; yusuke Ohta; Takashi Inada
- Web page: https://patentgrep.com/patent/US20130240128A1

## CPC

- C01B 32/205: Preparation
- B32B 38/0036: {Heat treatment (for heating or cooling of layers during lamination B32B37/06, B32B37/08)}
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

Disclosed herein is a production method capable of efficiently producing a carbonized film wound into a roll without the occurrence of fusion bonding between the layers of the film. The method includes a carbonization step in which a polymer film wound around a core is placed in a heating furnace and carbonized by heat treatment to obtain a carbonized film wound around the core. The carbonization step is performed by increasing a temperature of the heat treatment from an initial temperature through a pyrolysis onset temperature to a pyrolysis end temperature. In the carbonization step, the heating furnace is decompressed when the temperature of the heat treatment is lower than the pyrolysis onset temperature, and after the temperature of the heat treatment reaches the pyrolysis onset temperature, the heating furnace is not decompressed or the heating furnace is decompressed so that an absolute pressure in the heating furnace is in a range of 21.3 kPa to 101.29 kPa.

## Claims

### Claim 1

A method for producing a carbonized film comprising:
a preparation step in which a polymer film wound around a core is prepared; and
a carbonization step in which the polymer film is placed in a heating furnace and carbonized by heat treatment to obtain a carbonized film wound around the core, wherein the carbonization step is performed by increasing a temperature of the heat treatment from an initial temperature through a pyrolysis onset temperature to a pyrolysis end temperature, and wherein the heating furnace is decompressed when the temperature of the heat treatment is lower than the pyrolysis onset temperature, and wherein the heating furnace is not decompressed after the temperature of the heat treatment reaches the pyrolysis onset temperature.

### Claim 2

A method for producing a carbonized film comprising:
a preparation step in which a polymer film wound around a core is prepared; and
a carbonization step in which the polymer film is placed in a heating furnace and carbonized by heat treatment to obtain a carbonized film wound around the core, wherein the carbonization step is performed by increasing a temperature of the heat treatment from an initial temperature through a pyrolysis onset temperature to a pyrolysis end temperature, and wherein the heating furnace is decompressed when the temperature of the heat treatment is lower than the pyrolysis onset temperature, and wherein, after the temperature of the heat treatment reaches the pyrolysis onset temperature, the heating furnace is decompressed so that an absolute pressure in the heating furnace is in a range of 21.3 kPa to 101.29 kPa.

### Claim 3 (depends on 1)

The method for producing a carbonized film according to claim 1 wherein an absolute pressure in the heating furnace during the decompression performed at lower than the pyrolysis onset temperature is 70 kPa or less.

### Claim 4 (depends on 3)

The method for producing a carbonized film according to claim 3, wherein the absolute pressure in the heating furnace during the decompression performed at lower than the pyrolysis onset temperature is 10 kPa or less.

### Claim 5 (depends on 1)

The method for producing a carbonized film according to claim 1, wherein the decompression at lower than the pyrolysis onset temperature is performed when the temperature of the heat treatment is in a range of 100 to 450° C.

### Claim 6 (depends on 1)

The method for producing a carbonized film according to claim 1, wherein a rate of temperature rise during the heat treatment is 5° C./min or less until the temperature of the heat treatment reaches the pyrolysis onset temperature.

### Claim 7 (depends on 1)

The method for producing a carbonized film according to claim 1, wherein an inert gas is introduced into the heating furnace after the temperature of the heat treatment reaches the pyrolysis onset temperature.

### Claim 8 (depends on 7)

The method for producing a carbonized film according to claim 7, wherein the inert gas is introduced into the heating furnace at a flow rate of 1 L/min or more after the temperature of the heat treatment reaches the pyrolysis onset temperature.

### Claim 9 (depends on 1)

The method for producing a carbonized film according to claim 1, wherein when subjected to the carbonization step, the polymer film wound around the core is housed in an external tube.

### Claim 10 (depends on 9)

The method for producing a carbonized film according to claim 9, wherein the external tube has gas permeability.

### Claim 11 (depends on 10)

The method for producing a carbonized film according to claim 10, wherein the external tube has a gas vent.

### Claim 12 (depends on 9)

The method for producing a carbonized film according to claim 9, wherein when a value obtained by dividing (inner diameter of the external tube−diameter of the core) by 2 is defined as a (mm) and a thickness of a roll of the polymer film is defined as b (mm), a ratio of a/b is 1.8 or more but 3.8 or less.

### Claim 13 (depends on 1)

The method for producing a carbonized film according to claim 1, wherein the preparation step is a step in which the polymer film is wound around the core while a tension of 40 N/m or more is applied to the polymer film.

### Claim 14 (depends on 13)

The method for producing a carbonized film according to claim 13, wherein the polymer film is wound around the core at a winding speed of 1 m/min or more.

### Claim 15 (depends on 13)

The method for producing a carbonized film according to claim 13, wherein when a tension applied to the polymer film at a point 3 m apart from an winding-start end of the film is defined as Ps and a tension applied to the polymer film at a point 3 m apart from a winding-end end of the film is defined as Pe, a tension ratio of Pe/Ps is 1.1 or more.

### Claim 16 (depends on 13)

The method for producing a carbonized film according to claim 13, wherein the step in which the polymer film is wound around the core is performed while the polymer film wound around the core is pressed at a pressure of 70 N/m or less by means of a nip roller.

### Claim 17 (depends on 13)

The method for producing a carbonized film according to claim 13, wherein the step in which the polymer film is wound around the core is performed without applying a pressure to the polymer film by means of a nip roller.

### Claim 18 (depends on 13)

The method for producing a carbonized film according to claim 13, wherein the step in which the polymer film is wound around the core is performed while static electricity of the polymer film is eliminated.

### Claim 19 (depends on 1)

A method for producing a graphite film comprising the steps of:
producing a carbonized film by the production method according to claim 1; and
producing a graphite film by graphitizing the carbonized film.