# US 2013/0240033 A1 · Method for producing counter electrode based on electrophoretic deposition of graphene, counter electrode produced by the method and dye-sensitized solar cell including the counter electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0240033 A1
- Document ID: US20130240033A1
- Status: Published application
- Kind: A1
- Application number: 13/880,739
- Filed: 2011-05-06
- Published: 2013-09-19
- Earliest claimed: 2010-10-22
- Assignees: Inje University Industry-Academic Cooperation Foundation
- Inventors: Min-Hyon Jeon; Hyon-Kwang Choi; Sook-Hyun Hwang; Hyun-Kook Kim
- Web page: https://patentgrep.com/patent/US20130240033A1

## CPC

- H01G 9/2022: {characterized by he counter electrode}
- C25D 13/02: with inorganic material
- C25D 13/12: characterised by the article coated
- C25D 13/22: Servicing or operating {apparatus or multistep processes}
- F27D 7/06: Forming or maintaining special atmospheres or vacuum within heating chambers (supplying steam, vapour, gases or liquids F27D7/02)
- H01G 9/04: Electrodes {or formation of dielectric layers thereon}
- H01G 9/2031: {comprising titanium oxide, e.g. TiO2 (H01G9/2036 takes precedence)}
- H01G 9/2059: {comprising an organic dye as the active light absorbing material, e.g. adsorbed on an electrode or dissolved in solution}
- Y02E 10/542: Dye sensitized solar cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed is a method for producing a counter electrode based on electrophoretic deposition of graphene. The method includes: adding graphene to a dispersion medium to prepare a graphene dispersion; dipping a transparent electrode in the graphene dispersion and applying a voltage to the transparent electrode for 5 seconds to 5 minutes to deposit the graphene on the transparent electrode; and annealing the graphene-adsorbed transparent electrode at 350 to 600° C. under a nitrogen atmosphere. Also disclosed are a counter electrode produced by the method and a dye-sensitized solar cell including the counter electrode.

## Claims

### Claim 1

A method for producing a counter electrode, comprising:
adding graphene to a dispersion medium to prepare a graphene dispersion;
dipping a transparent electrode in the graphene dispersion and applying a voltage to the transparent electrode for 5 seconds to 5 minutes to deposit the graphene on the transparent electrode; and
annealing the graphene-adsorbed transparent electrode at 350 to 600° C. under a nitrogen atmosphere.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the graphene is present in an amount of 0.00001 to 0.25% by weight, based on the weight of the graphene dispersion.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the deposition voltage is from 10 to 30 V.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the graphene is produced by a chemical synthesis process.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the dispersion medium is a mixed solution of an alcohol and magnesium nitrate.

### Claim 6

A counter electrode produced by adding graphene to a dispersion medium, dipping a transparent electrode in the graphene dispersion, applying a voltage to the transparent electrode to deposit the graphene on the transparent electrode, and annealing the graphene-adsorbed transparent electrode at 350 to 600° C. under a nitrogen atmosphere.

### Claim 7 (depends on 6)

The counter electrode according to claim 6, wherein the counter electrode has a transmittance of at least 60% in the visible region in a state in which the counter electrode is attached to a transparent substrate.

### Claim 8 (depends on 6)

The counter electrode according to claim 6, wherein the counter electrode has a current density of 10 to 15 mA/cm2.

### Claim 9 (depends on 6)

A dye-sensitized solar cell fabricated using the counter electrode according to claim 6.