# US 2013/0239877 A1 · Method and structure for nonlinear optics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0239877 A1
- Document ID: US20130239877A1
- Status: Published application
- Kind: A1
- Application number: 13/606,351
- Filed: 2012-09-07
- Published: 2013-09-19
- Earliest claimed: 2008-04-11
- Assignees: Deep Photonics Corporation
- Inventors: Theodore Alekel
- Web page: https://patentgrep.com/patent/US20130239877A1

## CPC

- C30B 9/12: Salt solvents, e.g. flux growth
- C04B 35/01: based on oxide ceramics
- C09K 11/778: {Borates}
- C30B 9/06: using as solvent a component of the crystal composition
- C30B 11/00: Single-crystal growth by normal freezing or freezing under temperature gradient, e.g. Bridgman-Stockbarger method (C30B13/00, C30B15/00, C30B17/00, C30B19/00 take precedence; under a protective fluid C30B27/00)
- C30B 29/22: Complex oxides
- G02F 1/3551: {Crystals}
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3227: Lanthanum oxide or oxide-forming salts thereof
- C04B 2235/3409: Boron oxide, borates, boric acids, or oxide forming salts thereof, e.g. borax
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

A nonlinear optical crystal having a chemical formula of YiLajAlkB16O48, where 2.8≦i≦3.2, 0.8≦j≦1.2, i and j sum to about four, and k is about 12 is provided. The nonlinear optical crystal is useful for nonlinear optical applications including frequency conversion. Nonlinear optical crystals in a specific embodiment are characterized by UV blocking materials (e.g., some transition metals and lanthanides) at concentrations of less than 1,000 parts per million, providing high transmittance over portions of the UV spectrum (e.g., 175-360 nm).

## Claims

### Claim 1

A method of growing one or more nonlinear crystals of a composition, the method comprising:
providing a set of constituent components of the composition including an yttrium source, a lanthanum source, a boron source, and an aluminum source;
mixing the set of constituent components of the composition to form a component mixture;
heating the component mixture to a predetermined temperature, thereby forming a resultant melt;
cooling the resultant melt; and
forming the one or more nonlinear crystals of the composition as a precipitate from the resultant melt, wherein the one or more nonlinear crystals have a chemical formula of YiLajAlkB16O48, where 2.0≦i≦3.6, 0.4≦j≦2.0, i and j sum to about four, and k is about 12.

### Claim 2 (depends on 1)

The method of claim 1 wherein the yttrium source comprises yttrium oxide, the lanthanum source comprises lanthanum oxide, and the aluminum source comprises aluminum oxide.

### Claim 3 (depends on 3)

The method of claim 3 wherein the boron source comprises at least one of boron oxide or boric acid.

### Claim 4 (depends on 3)

The method of claim 3 wherein the one or more nonlinear crystals are characterized by an optical transmittance of greater than 0.7 at 250 nm.

### Claim 5 (depends on 4)

The method of claim 4 wherein the optical transmittance is greater than 0.7 at 200 nm.

### Claim 6 (depends on 1)

The method of claim 1 wherein a concentration of at least one or more of elements 22-30, 40-48, and 72-80 in the one or more nonlinear crystals is less than 1,000 parts per million.

### Claim 7 (depends on 1)

The method of claim 1 wherein a concentration of molybdenum in the one or more nonlinear crystals is less than 50 parts per million.

### Claim 8 (depends on 1)

The method of claim 1 wherein a concentration of at least one or more of elements 58-70 in the one or more nonlinear crystals is less than 1,000 parts per million.

### Claim 9 (depends on 1)

The method of claim 1 wherein cooling the resultant melt is performed at a temperature rate of less than 20° K/hour.

### Claim 10 (depends on 1)

The method of claim 1 wherein the one or more nonlinear crystals are characterized by a volume between about 1.0 mm3 and about 10 cm3.