# US 2013/0239874 A1 · Robust, ultraviolet-protected ambient condition history indicator and method of making same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0239874 A1
- Document ID: US20130239874A1
- Status: Published application
- Kind: A1
- Application number: 13/827,898
- Filed: 2013-03-14
- Published: 2013-09-19
- Earliest claimed: 2012-03-15
- Assignees: Temptime Corporation
- Applicants: Temptime Corporation
- Inventors: Dawn E. SMITH; Brian S. HUFFMAN; Frederick R. GRABINER; Jean-Paul Martin
- Web page: https://patentgrep.com/patent/US20130239874A1

## CPC

- G01N 31/229: {for investigating time/temperature history}
- Y10T 156/10: Methods of surface bonding and/or assembly therefor
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An optically readable ambient condition history indicator can have a substrate, an indicator agent on the substrate surface, and a transparent layer overlying the indicator agent. The indicator agent can be capable of changing appearance in response to exposure to an ambient condition and the transparent layer can be subject to exposure to environmental ultraviolet radiation. The indicator can also include a radiation-filtering adhesive layer overlying the indicator agent to secure the transparent layer to the indicator agent, which adhesive layer can include an adhesive and an ultraviolet radiation filter and can contact both the transparent layer and the indicator agent-bearing substrate. The radiation-filtering adhesive layer can protect the indicator agent from ultraviolet radiation transmitted through the transparent layer and provide a simple, robust construction that is easy to manufacture and resists delamination. The adhesive itself is also protected from ultraviolet radiation. A simplified manufacturing method is also disclosed.

## Claims

### Claim 1

An optically readable ambient condition history indicator comprising:
a substrate having a surface;
an indicator agent on the substrate surface, the indicator agent being capable of changing appearance irreversibly in response to historical exposure to an ambient condition;
a transparent layer overlying the indicator agent and at least a portion of the substrate surface, the transparent layer being subject to exposure to environmental ultraviolet radiation and the indicator appearance change being optically readable through the transparent layer;
a radiation-filtering adhesive layer overlying the indicator agent, wherein the radiation-filtering adhesive layer contacts the transparent layer, secures the transparent layer to the substrate surface, extends over the indicator agent, and comprises:
an adhesive; and
an ultraviolet radiation filter;
wherein the radiation-filtering adhesive layer can filter out ultraviolet radiation transmitted through the transparent layer.

### Claim 2 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the indicator agent occupies a portion of the substrate surface, the substrate surface has an unoccupied portion, and the radiation-filtering adhesive layer also overlies the unoccupied portion of the substrate surface.

### Claim 3 (depends on 2)

An ambient condition history indicator according to claim 2 comprising a contact area where the radiation-filtering adhesive layer contacts the transparent layer and contacts the indicator agent also wherein the contact area is at least coextensive with the occupied portion of the substrate surface.

### Claim 4 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the transparent layer and the radiation-filtering adhesive layer extend at least to the periphery of the substrate.

### Claim 5 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the transparent layer is transmissive to at least about 50 percent of ultraviolet radiation incident on the transparent layer.

### Claim 6 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the radiation-filtering adhesive layer can filter out at least about 70 percent of the ultraviolet energy incident on the radiation-filtering adhesive layer in a waveband of from about 200 nm to about 400 nm.

### Claim 7 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the transparent layer is transmissive to at least about 20 percent of light energy incident on the transparent layer in a waveband from about 400 nm to about 540 nm.

### Claim 8 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the radiation-filtering adhesive layer comprises a light filter to filter out short wavelength visible light.

### Claim 9 (depends on 8)

An ambient condition history indicator according to claim 8 wherein the light filter is transmissive to visible light having a longer wavelength than the filtered-out short wavelength visible light.

### Claim 10 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the radiation-filtering adhesive layer can transmit at least about 70 percent of the light energy reflected from the indicator agent in a waveband of from about 400 nm to about 700 nm.

### Claim 11 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the adhesive is selected from the group consisting of a synthetic monomer adhesive, a synthetic polymer adhesive, a solvent-based adhesive, a polymer dispersion adhesive, a pressure-sensitive adhesive, a contact adhesive, a hot-melt adhesive, a multi-component adhesive, a heat-curing adhesive, a moisture-curing adhesive, a mixture of any two or more compatible ones of the foregoing adhesives, or is selected from the group consisting of acrylonitrile, cyanoacrylate, acrylic, ethylene-vinyl acetate, polyvinyl alcohol, polyvinyl acetate, polyvinyl chloride, polyvinyl chloride emulsion, styrene acrylic copolymer, phenol formaldehyde resin, polyamide, polyester, epoxy, polyethylene, polypropylene, polysulfide, polyurethane, aliphatic resin, polyvinylpyrrolidone, urea-formaldehyde, starch, latex, resorcinol, and silicone adhesives, and mixtures of any two or more compatible ones of the foregoing adhesives.

### Claim 12 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the ultraviolet-radiation filter comprises a particulate dispersion of ultraviolet-filtering metal oxide particles.

### Claim 13 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the ultraviolet radiation filter is selected from the group consisting of zinc oxide, titanium dioxide, iron oxide, octylmethoxy cinnamate, octyl salicylate, octocrylene, oxybenzone, 2-ethylhexyl N,N-dimethylaminobenzoate, p-aminobenzoic acid, 2-phenyl-benzamidazole-5-sulfonic acid, homomethyl salicylate, avobenzone, DEA p-methoxycinnamate, octylmethoxy cinnamate, 4,4′-methoxy-t-butyldibenzoylmethane, 4-isopropyldibenzoylmethane, 3-(4-methylbenzylidene) camphor, 3-benzylidene camphor, 4-N,N-dimethylaminobenzoic acid ester, 2,4-dihydroxybenzophenone, 2-hydroxy-4-(2-hydroxyethoxy)benzophenone, 4-hydroxydibenzoyl-methane, 4-(2-hydroxyethoxy)dibenzoylmethane, 4-N,N-di(2-ethylhexyl)-aminobenzoic acid ester, 4-N,N-(2-ethylhexyl)methylaminobenzoic acid ester, 4-N,N-(2-hydroxyethoxy)benzophenone, and mixtures of two or more of the foregoing ultraviolet-radiation filters.

### Claim 14 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the indicator agent comprises a diacetylenic compound.

### Claim 15 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the transparent layer comprises a light filter to block blue light, the light filter being transmissive to red light.

### Claim 16 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the indicator agent comprises an active diacetylenic compound capable of changing appearance in response to cumulative exposure to temperature over time.

### Claim 17 (depends on 1)

An ambient condition history indicator according to claim 1 wherein the radiation-filtering adhesive layer can exhibit a peel value of at least about 16 g/mm as determined at an angle of 90° and a speed of 5 mm/s using a Cheminstruments AR1000 peel tester.

### Claim 18 (depends on 1)

An ambient condition history indicator according to claim 1 comprising a layer of an ultraviolet-absorbent ink extending over the indicator agent.

### Claim 19 (depends on 1)

An ambient condition history indicator according to claim 1 and a host product wherein the ambient condition history indicator is associated with the host product to monitor the exposure of the host product to an ambient condition.

### Claim 20

A method of making an optically readable ambient condition history indicator comprising:
applying an indicator agent to a substrate surface, the indicator agent being capable of changing appearance in response to exposure to an ambient condition,
applying a radiation-filtering adhesive to a transparent layer, the radiation-filtering adhesive comprising an adhesive component and an ultraviolet radiation filter wherein the adhesive component can filter out ultraviolet radiation transmitted by the transparent layer to protect the indicator agent from exposure to the ultraviolet radiation; and
overlaying the transparent layer bearing the radiation-filtering adhesive on the substrate surface bearing the indicator agent so that the radiation-filtering adhesive contacts the indicator agent.