# US 2013/0239848 A1 · Calcium Sulphate-Based Products and Methods for the Manufacture Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0239848 A1
- Document ID: US20130239848A1
- Status: Published application
- Kind: A1
- Application number: 13/988,845
- Filed: 2011-11-23
- Published: 2013-09-19
- Earliest claimed: 2010-11-23
- Assignees: Saint-Gobain Placo
- Inventors: Robin Daniel Fisher; Jan Rideout
- Web page: https://patentgrep.com/patent/US20130239848A1

## CPC

- C04B 14/00: Use of inorganic materials as fillers, e.g. pigments, for mortars, concrete or artificial stone; Treatment of inorganic materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone (expanding or defibrillating materials C04B20/00)
- C04B 28/14: containing calcium sulfate cements {(gypsum-paper plates E04C)}
- C04B 2111/28: Fire resistance, i.e. materials resistant to accidental fires or high temperatures
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The invention provides a calcium sulphate-based product comprising a phosphate as additive for increased fire resistance. Particularly preferred phosphate additives may be those containing aluminium or ammonium ions.

## Claims

### Claim 1

A method of manufacture of a calcium sulphate-based product having increased fire resistance, comprising the steps of:
providing a stucco slurry comprising a mixture of stucco, water, and at least one phosphate additive; and
allowing the stucco in the mixture to hydrate and set.

### Claim 2 (depends on 1)

A method of manufacture according to claim 1, wherein the phosphate additive is present in an amount of at least 2 weight % of the dry weight of the slurry.

### Claim 3 (depends on 1)

A method of manufacture according to claim 1, wherein the phosphate additive is selected from a group comprising sodium phosphate, potassium phosphate, lithium phosphate, calcium phosphate (e.g. calcium pyrophosphate, monetite, or brushite (calcium phosphate dihydrate)), magnesium phosphate, magnesium phosphate dibasic trihydrate, magnesium phosphate hydrate, zinc phosphate, aluminium phosphate, diammonium hydrogen phosphate, ammonium dihydrogen phosphate, ammonium magnesium phosphate, ammonium aluminium phosphate, ammonium polyphosphate, potassium aluminium phosphate, sodium aluminium phosphate, aluminium metaphosphate, copper hydroxide phosphate, and boron phosphate.

### Claim 4 (depends on 1)

A method of manufacture according to claim 1 wherein the phosphate additive is selected from a group comprising aluminium phosphate, diammonium hydrogen phosphate, ammonium aluminium phosphate, ammonium polyphosphate, ammonium dihydrogen phosphate, potassium aluminium phosphate, and sodium aluminium phosphate.

### Claim 5 (depends on 1)

A method of manufacture according to claim 1, wherein the phosphate additive includes aluminium.

### Claim 6 (depends on 5)

A method of manufacture according to claim 5, wherein the phosphate additive is aluminium phosphate.

### Claim 7 (depends on 6)

A method of manufacture according to claim 6, wherein the aluminium phosphate is Al(H2PO4)3.

### Claim 8 (depends on 1)

A method of manufacture according to claim 1, wherein the phosphate additive includes ammonium ions.

### Claim 9 (depends on 1)

A method of manufacture according to claim 1, wherein the phosphate additive is provided in a liquid solution.

### Claim 10 (depends on 10)

A method of manufacture according to claim 10, wherein the liquid solution is an aqueous solution.

### Claim 11 (depends on 1)

A method of manufacture according to claim 1, wherein the phosphate additive is substantially insoluble in water.

### Claim 12 (depends on 1)

A method of manufacture according to claim 1, comprising the further step, before allowing the stucco to hydrate and set, of adding an accelerator to increase the rate of hydration of the stucco.

### Claim 13 (depends on 12)

A method according to claim 12, wherein the accelerator is Ground Mineral NANSA.

### Claim 14 (depends on 13)

A method according to claim 13, wherein the Ground Mineral NANSA is added to the stucco slurry in a quantity of 1-5 wt %, relative to the dry weight of the slurry.

### Claim 15

A method of manufacture of a treated calcium sulphate-based product having increased fire resistance, comprising the steps of:
causing a stucco slurry to hydrate, to provide a set calcium sulphate-based product; and
impregnating the set calcium sulphate-based product with a solution comprising a phosphate additive.

### Claim 16 (depends on 15)

A method of manufacture according to claim 15, wherein the phosphate additive is a compound other than aluminium phosphate.

### Claim 17

A calcium sulphate-based product having increased fire resistance comprising a phosphate additive.

### Claim 18 (depends on 17)

A calcium sulphate-based product according to claim 17, wherein the phosphate additive is a compound other than aluminium phosphate.