# US 2013/0230987 A1 · Flowable oxide film with tunable wet etch rate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0230987 A1
- Document ID: US20130230987A1
- Status: Published application
- Kind: A1
- Application number: 13/493,936
- Filed: 2012-06-11
- Published: 2013-09-05
- Earliest claimed: 2012-03-05
- Assignees: Novellus Systems, Inc.
- Inventors: Nerissa Draeger; Karena Shannon; Bart van Schravendijk; Kaihan Ashtiani
- Web page: https://patentgrep.com/patent/US20130230987A1

## CPC

- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6502: {of treatments performed before formation of the materials}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6534: {by exposure to a liquid}
- H10P 14/6538: {by exposure to UV light}
- H10P 14/6905: {being a silicon carbide or silicon carbonitride and not containing oxygen, e.g. SiC or SiC:H}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P 50/283: {by chemical means}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided herein are integration-compatible dielectric films and methods of depositing and modifying them. According to various embodiments, the methods can include deposition of flowable dielectric films targeting specific film properties and/or modification of those properties with an integration-compatible treatment process. In certain embodiments, methods of depositing and modifying flowable dielectric films having tunable wet etch rates and other properties are provided. Wet etch rates can be tuned during integration through am integration-compatible treatment process. Examples of treatment processes include plasma exposure and ultraviolet radiation exposure.

## Claims

### Claim 1

A method, comprising:
forming a flowable dielectric film on a substrate, wherein the flowable dielectric film has a first wet etch rate;
performing one or more integration processes on the substrate; and
after performing the one or more integration processes, modifying the wet etch rate of the flowable dielectric film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the flowable dielectric film is a silicon oxide, a silicon nitride, a silicon oxynitride, silicon carbide, or a silicon oxycarbide film.

### Claim 3 (depends on 1)

The method of claim 1, wherein the flowable dielectric film is a carbon-doped oxide, a boron-doped oxide, a phosphorous-doped oxide, or a nitrogen-doped oxide.

### Claim 4 (depends on 1)

The method of claim 1, wherein the modified wet etch rate is higher than the first wet etch rate.

### Claim 5 (depends on 1)

The method of claim 1, wherein the modified wet etch rate is lower than the first wet etch rate.

### Claim 6 (depends on 1)

The method of claim 1, wherein modifying the first wet etch rate comprises exposing the densified flowable dielectric film to ultraviolet radiation.

### Claim 7 (depends on 1)

The method of claim 1, wherein treating the densified flowable dielectric film comprises exposing the densified flowable dielectric film to species from an in situ or remote plasma and wherein treating the densified flowable film chemically and/or physically modifies the densified flowable dielectric film.

### Claim 8 (depends on 1)

The method of claim 1, wherein the one or more integration processes include at least one of an etch process, a deposition process, a planarization process, a photoresist strip process, a wet clean process, and a lithographic patterning process.

### Claim 9 (depends on 1)

The method of claim 1, wherein forming a flowable dielectric film on the substrate comprises depositing a flowable dielectric film and densifying the deposited film.

### Claim 10 (depends on 1)

The method of claim 1, comprising physically densifying the flowable film prior to performing the one or more integration process and chemically modifying the flowable film after performing the one or more integration processes.

### Claim 11

A method comprising:
depositing a flowable dielectric film on a substrate; and
densifying the flowable dielectric film, wherein the densified flowable dielectric film has a first wet etch rate, wherein said first wet etch rate is tunable such that it can be changed by a factor of at least 10.

### Claim 12 (depends on 11)

The method of claim 11, wherein the first wet etch rate is about zero.

### Claim 13 (depends on 11)

The method of claim 11, wherein the first wet etch rate at least about 10 nm/min.

### Claim 14 (depends on 11)

The method of claim 11, wherein the carbon concentration of the densified flowable dielectric film is less than about 5% atomic.

### Claim 15 (depends on 11)

The method of claim 11, wherein the carbon concentration of the densified flowable dielectric film is between 5 and 35% atomic.

### Claim 16 (depends on 11)

The method of claim 11, wherein depositing a flowable dielectric film on a substrate comprises exposing the substrate to a carbon-doped precursor.

### Claim 17 (depends on 11)

The method of claim 11, wherein depositing the flowable dielectric film on the substrate comprises reacting a non-hydroxyl-forming oxidant with a silicon-containing precursor.

### Claim 18 (depends on 17)

The method of claim 17, wherein depositing the silicon-containing precursor is an alkoxy compound.

### Claim 19

A method comprising:
after performing one or more integration operations on a substrate including a flowable dielectric film, treating the flowable dielectric film to modify a wet etch rate of the flowable dielectric film.

### Claim 20 (depends on 19)

The method of claim 19, wherein treating the flowable dielectric film comprises removing at least one of carbon, nitrogen or hydrogen from the flowable dielectric film.

### Claim at position 21

-25. (canceled)