# US 2013/0230709 A1 · Porous graphene material and preparation method and uses as electrode material thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0230709 A1
- Document ID: US20130230709A1
- Status: Published application
- Kind: A1
- Application number: 13/883,414
- Filed: 2010-12-29
- Published: 2013-09-05
- Earliest claimed: 2010-12-29
- Assignees: Ocean's King Lighting Science & Technology Co., Ltd.
- Inventors: Mingjie Zhou; Yaobing Wang
- Web page: https://patentgrep.com/patent/US20130230709A1

## CPC

- H01G 11/36: Nanostructures, e.g. nanofibres, nanotubes or fullerenes
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01B 32/192: starting from graphitic oxides
- H01M 4/587: for inserting or intercalating light metals
- C01P 2006/12: Surface area
- C01P 2006/16: Pore diameter
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- Y02E 60/10: Energy storage using batteries
- Y02E 60/13: Energy storage using capacitors
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A porous graphene material and preparation method thereof are provided. The pore diameter of the porous graphene material is 1 nm-10 μm and its specific surface area is 100 m2/g-2000 m2/g. The method for preparing the porous graphene material comprises the following steps: mixing graphene or graphene oxide with pore-forming agent, and pressing to obtain bulk or powder particle composite; heating the composite, and releasing gases from the pore-forming agent to obtain the porous graphene material. The porous graphene material can be used as electrode materials of supercapacitor and lithium ion battery.

## Claims

### Claim at position 1

1-10. (canceled)

### Claim 11

A porous graphene material, wherein the porous graphene material has a pore size of 1 nm to 10 μm and a specific surface area of 100 m2/g to 2000 m2/g.

### Claim 12 (depends on 11)

The porous graphene material according to claim 11, wherein the porous graphene material having a pore size of 50 nm to 10 μm represents 20% to 40% of the total volume; the porous graphene material having a pore size of 2 nm to 50 nm represents 35% to 55% of the total volume; and the porous graphene material having a pore size of 1 nm to 2 nm represents 20% to 25% of the total volume.

### Claim 13 (depends on 11)

The porous graphene material according to claim 11, wherein the porous graphene material has a pore size of 2 to 50 nm and a specific surface area of 150 m2/g to 1000 m2/g.

### Claim 14 (depends on 11)

The porous graphene material according to claim 11, wherein the porous graphene material has a pore specific surface area of 150 m2/g to 2500 m2/g.

### Claim 15

A method for preparing a porous graphene material, comprising the steps of:
mixing graphene or graphene oxide with a pore-forming agent which is capable of releasing a gas, and pressing into a composite in a form of blocks or powdered particles; and
heating the composite to release a gas from the pore-forming agent to give the porous graphene material.

### Claim 16 (depends on 15)

The method for preparing a porous graphene material according to claim 15, wherein the pore-forming agent is dry ice, which is heated to a temperature under which dry ice gasifies.

### Claim 17 (depends on 15)

The method for preparing a porous graphene material according to claim 15, wherein the pore-forming agent is an organic polymeric material or a small-molecular material which has a decomposition temperature of below 2000° C., and the procedure for releasing a gas from the pore-forming agent in the composite comprises: heating the composite to 500 to 2000° C. so that the organic polymeric material or the small-molecular material decomposes to release a gas.

### Claim 18 (depends on 17)

The method for preparing a porous graphene material according to claim 17, wherein the organic polymeric material is one or more of polycarbonate beads, polystyrene beads, polypropylene beads, polyacetylene beads, polyphenylene beads, polydimethylsiloxane beads, polycarbonate nanoparticles, polystyrene nanoparticles, polypropylene nanoparticles, polyacetylene nanoparticles, polyphenylene nanoparticles and polydimethylsiloxane nanoparticles; and
the small-molecular material is one or more of ammonium acetate, ammonium carbonate, tetramethyl ammonium acetate, ammonium nitrate, sodium bicarbonate, basic cupric carbonate and potassium permanganate.

### Claim 19 (depends on 18)

The method for preparing a porous graphene material according to claim 18, wherein the beads of the organic polymeric material have diameter of 10 nm to 1 μm.

### Claim 20 (depends on 11)

A supercapacitor or a lithium ion battery, comprising the porous graphene material according to claim 11 as an electrode material.