## CPC

- C03C 3/247: containing fluorine and phosphorus
- C03C 17/42: at least one coating of an organic material and at least one non-metal coating
- C03C 2217/948: Layers comprising indium tin oxide [ITO]
- H10K 59/8731: {multilayered coatings having a repetitive structure, e.g. having multiple organic-inorganic bilayers}
- H10K 71/421: {using coherent electromagnetic radiation, e.g. laser annealing}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

A method of preparing an organic light-emitting device including: forming an organic emission unit on a substrate; and forming a thin film encapsulation layer including at least one inorganic layer including a low temperature viscosity transition (LVT) inorganic material, the forming the thin film encapsulation layer including forming the at least one inorganic layer, and the forming the at least one inorganic layer including: forming a pre-inorganic layer including the LVT inorganic material on the organic emission unit by heating a source including the LVT inorganic material using plasma in a vacuum and depositing the LVT inorganic material or ions of the LVT inorganic material separated from the source on the organic emission unit; and applying a healing process to the pre-inorganic layer at a temperature greater than a viscosity transition temperature of the LVT inorganic material.

## Claims

### Claim 1

A method of preparing an organic light-emitting device, the method comprising:
forming an organic emission unit on a substrate; and
forming a thin film encapsulation layer including at least one inorganic layer including a low temperature viscosity transition (LVT) inorganic material, the forming the thin film encapsulation layer comprising forming the at least one inorganic layer,
wherein the forming the at least one inorganic layer comprises:
forming a pre-inorganic layer including the LVT inorganic material on the organic emission unit by heating a source comprising the LVT inorganic material using plasma in a vacuum and depositing the LVT inorganic material or ions of the LVT inorganic material separated from the source on the organic emission unit; and
applying a healing process to the pre-inorganic layer at a temperature greater than a viscosity transition temperature of the LVT inorganic material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the viscosity transition temperature of the LVT inorganic material is a minimum temperature capable of providing fluidity to the LVT inorganic material.

### Claim 3 (depends on 1)

The method of claim 1, wherein the viscosity transition temperature of the LVT inorganic material is less than a lowest temperature of denaturation temperatures of materials contained in the organic emission unit.

### Claim 4 (depends on 1)

The method of claim 1, wherein the LVT inorganic material comprises a tin oxide.

### Claim 5 (depends on 4)

The method of claim 4, wherein the LVT inorganic material further comprises at least one selected from the group consisting of phosphorus oxide, boron phosphate, tin fluoride, niobium oxide, and tungsten oxide.

### Claim 6 (depends on 1)

The method of claim 1, wherein the LVT inorganic material comprises SnO; SnO and P2O5; SnO and BPO4; SnO, SnF2, and P2O5; SnO, SnF2, P2O5, and NbO; or SnO, SnF2, P2O5, and WO3.

### Claim 7 (depends on 1)

The method of claim 1, wherein the applying the healing process is performed by heat-treating the pre-inorganic layer at a temperature from the viscosity transition temperature of the LVT inorganic material to a lowest temperature of denaturation temperatures of materials contained in the organic emission layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the applying the healing process is performed by heat-treating the pre-inorganic layer at a temperature of 80° C. to 132° C. for 1 to 3 hours.

### Claim 9 (depends on 1)

The method of claim 1, wherein the applying the healing process is performed in a vacuum or in an inert gas atmosphere.

### Claim 10 (depends on 1)

The method of claim 1, wherein the applying the healing process comprises scanning the pre-inorganic layer while irradiating a laser beam to the pre-inorganic layer.

### Claim 11 (depends on 1)

The method of claim 1, wherein the forming the thin film encapsulation layer further comprises forming at least one organic layer of the thin film encapsulation layer, the at least one organic layer including a polymer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the forming the at least one organic layer comprises providing a curable precursor, and curing the curable precursor.

### Claim 13 (depends on 12)

The method of claim 12, wherein the providing the curable precursor is performed by using a flash evaporator.

### Claim 14 (depends on 12)

The method of claim 12, wherein the curing the curable precursor is performed by using at least one of UV rays, infrared rays, or laser beams.

### Claim 15 (depends on 11)

The method of claim 11, wherein the thin film encapsulation layer comprises one organic layer and one inorganic layer, wherein the organic layer and the inorganic layer are sequentially stacked on the organic emission unit.

### Claim 16 (depends on 11)

The method of claim 11, wherein the thin film encapsulation layer comprises one organic layer and one inorganic layer, wherein the inorganic layer and the organic layer are sequentially stacked on the organic emission unit.

### Claim 17 (depends on 11)

The method of claim 11, wherein the thin film encapsulation layer comprises two organic layers including first and second organic layers, and one inorganic layer, wherein the first organic layer, the inorganic layer, and the second organic layer are sequentially stacked on the organic emission unit.

### Claim 18 (depends on 11)

The method of claim 11, wherein the thin film encapsulation layer comprises one organic layer, and two inorganic layers including first and second inorganic layers, wherein the first inorganic layer, the organic layer, and the second inorganic layer are sequentially stacked on the organic emission unit,

### Claim 19 (depends on 1)

The method of claim 1, wherein the forming the pre-inorganic layer comprises applying a negative potential to the substrate.

### Claim 20 (depends on 1)