# US 2013/0230642 A1 · Method of manufacturing active retarder and method of manufacturing display apparatus having the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0230642 A1
- Document ID: US20130230642A1
- Status: Published application
- Kind: A1
- Application number: 13/783,802
- Filed: 2013-03-04
- Published: 2013-09-05
- Earliest claimed: 2012-03-05
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., Ltd.
- Inventors: HeeWook DO; Sang-Jae Kim; Soyoun Park; Hoyun Byun; Duck Jong Suh; SangHee Yu; SangGu Lee; Ji-Yoon Jung; MinOh Choi
- Web page: https://patentgrep.com/patent/US20130230642A1

## CPC

- G02F 1/133305: {Flexible substrates, e.g. plastics, organic film}
- G02B 5/3083: {Birefringent or phase retarding elements (G02B5/3008, G02B5/3016 take precedence; systems for polarisation control G02B27/286; manufacturing phase modulating patterns by lithographic processes G03F7/001)}
- G02B 30/25: using polarisation techniques
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A method of manufacturing an active retarder includes forming a first substrate, forming a second substrate, and forming a liquid crystal layer between the first substrate and the second substrate. The forming of the first and second substrates is performed by a roll-to-roll process.

## Claims

### Claim 1

A method of manufacturing an active retarder for a display apparatus, comprising:
forming a first substrate;
forming a second substrate; and
forming a liquid crystal layer between the first substrate and the second substrate, wherein the forming of the first and second substrates is performed by a roll-to-roll process.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming of the first substrate comprises:
preparing a first base film;
forming a first transparent conductive material on the first base film; and
patterning the first transparent conductive material to form a first electrode on the first base film, and wherein the forming of the second substrate comprises:
preparing a second base film; and
forming a second transparent conductive material on the second base film to form a second electrode on the second base film.

### Claim 3 (depends on 2)

The method of claim 2, wherein the first transparent conductive material and the second transparent conductive material are coated by a wet process.

### Claim 4 (depends on 2)

The method of claim 2, wherein each of the first transparent conductive material and the second transparent conductive comprises at least one of indium tin oxide (ITO), indium zinc oxide (IZO), or silver nanowire (AgNW).

### Claim 5 (depends on 4)

The method of claim 4, wherein the first transparent conductive material is patterned by a laser etching process.

### Claim 6 (depends on 2)

The method of claim 2, wherein the forming of the liquid crystal layer comprises:
forming a spacer on the first substrate;
forming a sealant on the first substrate;
dropping a liquid crystal on the first substrate;
positioning the second substrate to face the first substrate; and
curing the sealant.

### Claim 7 (depends on 6)

The method of claim 6, wherein the spacer is formed by scattering beads on the first substrate.

### Claim 8 (depends on 6)

The method of claim 6, wherein the spacer is formed by a gravure printing method.

### Claim 9 (depends on 6)

The method of claim 6, wherein the sealant is cured by an ultraviolet ray.

### Claim 10 (depends on 2)

The method of claim 2, further comprising forming a plurality of barrier layers on an upper surface and a lower surface of the first base film and on an upper surface and a lower surface of the second base film, respectively.

### Claim 11 (depends on 2)

The method of claim 2, wherein the forming of the first substrate comprises:
forming a first alignment layer on the first electrode, and
rubbing the first alignment layer, and wherein the forming of the second substrate comprises:
forming a second alignment layer on the second electrode, and
rubbing the second alignment layer.

### Claim 12 (depends on 2)

The method of claim 2, further comprising forming a wire part on the first substrate which connects the first and second electrodes to each other.

### Claim 13 (depends on 12)

The method of claim 12, wherein the wire part is formed by printing a metal layer.

### Claim 14 (depends on 1)

The method of claim 1, wherein each of the first substrate and the second substrate is a flexible substrate and the roll-to-roll process is performed under a temperature of about 160 degrees Celsius.

### Claim 15 (depends on 1)

A method of manufacturing a display apparatus, comprising:
preparing a display panel; and
attaching an active retarder manufactured by a method according to claim 1 to the display panel.

### Claim 16 (depends on 15)

The method of claim 15, wherein the attaching of the active retarder comprises:
attaching a release film on a surface of the active retarder while interposing an adhesive layer between the release film and the active retarder; and
removing the release film to attach the active retarder to the display panel.

### Claim 17 (depends on 16)

The method of claim 16, wherein the active retarder is attached on the display panel by:
positioning the active retarder on the display panel; and
applying a pressure on the active retarder toward the display panel using a roller.

### Claim 18

A method of manufacturing an active retarder for a display apparatus, comprising:
forming a first flexible substrate, wherein the forming of the first flexible substrate comprises:
preparing a first base film,
forming a first barrier layer on an upper surface of the first base film,
forming a first electrode on the first barrier layer, and
forming a first alignment layer on the first electrode; and
forming a second flexible substrate, wherein the forming of the second flexible substrate comprises:
preparing a second base film,
forming a second barrier layer on an upper surface of the second base film,
forming a second electrode on the second barrier layer,
forming a second alignment layer on the second electrode;
attaching a first retardation film on an upper surface of the second barrier layer using a first adhesive layer provided on the upper surface of the second barrier layer;
attaching a protective film onto an upper surface of the first retardation film using a second adhesive layer provided on the upper surface of the first retardation film;
providing liquid crystals on one of the first flexible substrate or the second flexible substrate; and
attaching the first flexible substrate and the second flexible substrate to each other with a liquid crystal layer disposed therebetween.

### Claim 19 (depends on 18)

The method of claim 18, wherein the forming of the first and second flexible substrates is performed by a roll-to-roll process.

### Claim 20 (depends on 18)

The method of claim 18, further comprising forming a wire part on the first base film which connects the first and second transparent electrodes to each other.

### Claim 21 (depends on 20)

The method of claim 20, wherein the wire part includes a flexible printed circuit board and a common line, wherein the flexible printed circuit board is electrically connected to first electrode and the common line and wherein the flexible printed circuit board directly contacts the first electrode and the common line via an anisotropic conductive film.

### Claim 22 (depends on 21)

The method of claim 21, wherein the second base film is smaller in size than the first base film and wherein a portion of the wire part formed on the first base film is exposed by the second base film.

### Claim 23 (depends on 20)

The method of claim 20, wherein the wire part includes a flexible printed circuit board, a connection line connected to the flexible printed circuit board though an anisotropic conductive film, a common line connected to the connection line and configured to apply a reference voltage to the second electrode and a contact pad connected to the connection line and which directly contacts with the first electrode and the common line.

### Claim 24 (depends on 18)

The method of claim 18, wherein the first and second alignment layers are formed by mixing an organic polymer having a glass transition temperature of no greater than about 200 degrees Celsius with a solvent.

### Claim 25 (depends on 24)

The method of claim 24, wherein the solvent is selected from the group consisting of acetone, gammabutyrolacetone (GBL), N-methylpyrrolidone (NMP), butylcellosolve (BC), and isopropylalcohol (IPA).

### Claim 26 (depends on 18)

The method of claim 18, wherein the first and second base films are each formed of a material selected from the group consisting of polyethylene terephthalate, polycarbonate, and polyetheretherketone.