# US 2013/0230446 A1 · Method for producing a coarse-grained ammonium sulfate product via crystallization and installation for operating the method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0230446 A1
- Document ID: US20130230446A1
- Status: Published application
- Kind: A1
- Application number: 13/780,297
- Filed: 2013-02-28
- Published: 2013-09-05
- Earliest claimed: 2012-03-01
- Assignees: GEA Messo GmbH
- Applicants: Gea Messo GmbH
- Inventors: Guenter Hofmann; Holger Leptien; Johannes Widua
- Web page: https://patentgrep.com/patent/US20130230446A1

## CPC

- B01D 9/0036: {Crystallisation on to a bed of product crystals; Seeding}
- B01D 9/0022: {by reducing pressure}
- B01D 9/0031: {by heating (B01D9/0022, B01D9/0027 take precedence)}
- B01D 9/0059: {General arrangements of crystallisation plant, e.g. flow sheets}
- C01C 1/248: Preventing coalescing or controlling form or size of the crystals
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C01C: AMMONIA; CYANOGEN; COMPOUNDS THEREOF ({metal hydrides, monoborane, diborane or addition complexes thereof C01B6/00}; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; azides C01B21/08; {compounds other than ammonia or cyanogen, containing nitrogen, non-metals and optionally metals C01B21/082}; metal imides or amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; compounds containing silicon C01B33/00; compounds containing boron C01B35/00)

## Abstract

Method for the production of a coarse-grained ammonium sulphate product by crystallization and installation for carrying out the method. A method for the continuous production of a coarse-grained ammonium sulphate product from an ammonium sulphate solution in a crystallizer operates in accordance with the DTB principle and has an internal suspension circuit and a clarifying zone, from which a clarified partial flow of solution is constantly drawn off into an external circuit, is heated in a heat exchanger so as to dissolve the solids contained therein and is then guided back as a clear solution into the lower region of the crystallizer. In order to ensure production of a product crystallizate with a grain coarseness which is practically constant over time, a fine crystal suspension flow may be drawn off from the clarifying zone as a further partial flow and guided back into the internal circuit of the crystallization stage without any previous dissolution of the solid proportion contained therein.

## Claims

### Claim 1

Method for continuous production of a coarse-grained ammonium sulphate product of a grain size in the range of approximately 2.0-3.0 mm by crystallization of an ammonium sulphate solution in a crystallization stage which is operated in accordance with a draft tube baffled (DTB) principle, said method comprising:
constantly circulating a suspension of mother solution and ammonium sulphate crystals in an internal circuit while evaporating water from the solution;
drawing off a clarified partial flow of solution from a clarifying zone in an upper region of the crystallization stage into an external circuit;
heating the solution so as to dissolve the solids contained therein and then guiding the solution back as a clear solution into a lower region of the crystallization stage, and continuously drawing off vapours from a head of the crystallization stage;
supplying new ammonium sulphate solution from outside and drawing off a suspension flow containing the coarse-grained ammonium sulphate product from the lower region of the crystallization stage; and
drawing off as a further partial flow a fine crystal suspension flow from the clarifying zone and guiding the fine crystal suspension flow back into the internal circuit of the crystallization stage without any previous dissolution of the solid proportion contained therein.

### Claim 2 (depends on 1)

Method as claimed in claim 1, including recirculating the fine crystal suspension flow in a continuous manner.

### Claim 3 (depends on 2)

Method as claimed in claim 2, including recirculating the fine crystal suspension flow with a constant flow volume, said flow dependent upon the production output of the crystallization stage, per unit of time.

### Claim 4 (depends on 1)

Method as claimed in claim 1 wherein the fine crystal suspension flow is branched off from the partial flow of the clarified solution of the external circuit prior to heating thereof.

### Claim 5 (depends on 1)

Method as claimed in claim 1 wherein the flow volume of the fine crystal suspension flow is adjusted such that the solid proportion contained therein corresponds per unit of time to a quantity in the range of 0.2-0.3% of the quantity of product crystallizate in the suspension flow drawn off from the lower region of the crystallization stage.

### Claim 6 (depends on 5)

Method as claimed in claim 5, wherein the solids quantity in the guided-back fine crystal suspension flow is in the range of 0.8-1.5% of the product crystallizate quantity.

### Claim 7 (depends on 1)

Method as claimed in claim 1 wherein the fine crystal suspension flow in the close range of the liquid level of the crystallization stage is fed back into the internal suspension circuit.

### Claim 8

Installation for continuous production of a coarse-grained ammonium sulphate product of a grain size in the range of approximately 2.0-3.0 mm by crystallization of an ammonium sulphate solution in a crystallization stage, said installation comprising:
a crystallizer which operates in accordance with the draft tube baffled (DTB) principle and has an inner suspension circuit with a flow guide pipe and which has an external circuit line for clarified solution;
a heat exchanger which is connected into the external circuit line and having a vapour discharge line which is disposed at a head of the crystallizer;
a solution supply line for external supply of new ammonium sulphate solution and having a suspension discharge line which leads from a base region of the crystallizer; and
a fine crystal suspension return line connected to a clarifying zone of the crystallizer issues into the region of the inner suspension circuit of the crystallizer.

### Claim 9 (depends on 8)

Installation as claimed in claim 8, wherein the fine crystal suspension return line has a valve for adjusting flow volume.

### Claim 10 (depends on 8)

Installation as claimed in claim 8, wherein the fine crystal suspension return line branches off from the external circuit line upstream of the heat exchanger downstream of a circulating pump.

### Claim 11 (depends on 8)

Installation as claimed in claim 8, wherein the fine crystal suspension return line issues into the crystallizer in the region of the height level of the upper end of the flow guide pipe.

### Claim 12 (depends on 9)

Installation as claimed in claim 9, wherein the fine crystal suspension return line branches off from the external circuit line upstream of the heat exchanger downstream of a circulating pump.

### Claim 13 (depends on 12)

Installation as claimed in claim 12, wherein the fine crystal suspension return line issues into the crystallizer in the region of the height level of the upper end of the flow guide pipe.

### Claim 14 (depends on 6)

Method as claimed in claim 6, wherein the solids quantity in the guided-back fine crystal suspension flow is approximately 1% of the product crystallizate quantity.

### Claim 15 (depends on 2)

Method as claimed in claim 2, wherein the fine crystal suspension flow is branched off from the partial flow of the clarified solution of the external circuit prior to heating thereof.

### Claim 16 (depends on 3)

Method as claimed in claim 3, wherein the fine crystal suspension flow is branched off from the partial flow of the clarified solution of the external circuit prior to heating thereof.

### Claim 17 (depends on 2)

Method as claimed in claim 2, wherein the flow volume of the fine crystal suspension flow is adjusted such that the solid proportion contained therein corresponds per unit of time to a quantity in the range of 0.2-0.3% of the quantity of product crystallizate in the suspension flow drawn off from the lower region of the crystallization stage.

### Claim 18 (depends on 17)

Method as claimed in claim 17, wherein the solids quantity in the guided-back fine crystal suspension flow is in the range of 0.8-1.5% of the product crystallizate quantity.

### Claim 19 (depends on 2)

Method as claimed in claim 2, wherein the fine crystal suspension flow in the close range of the liquid level of the crystallization stage is fed back into the internal suspension circuit.

### Claim 20 (depends on 3)

Method as claimed in claim 3, wherein the fine crystal suspension flow in the close range of the liquid level of the crystallization stage is fed back into the internal suspension circuit.