# US 2013/0221464 A1 · Reduced light degradation due to low power deposition of buffer layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0221464 A1
- Document ID: US20130221464A1
- Status: Published application
- Kind: A1
- Application number: 13/407,006
- Filed: 2012-02-28
- Published: 2013-08-29
- Earliest claimed: 2012-02-28
- Assignees: International Business Machines Corporation
- Inventors: Keith E. Fogel; Augustin J. Hong; Jeehwan Kim; Devendra K. Sadana
- Web page: https://patentgrep.com/patent/US20130221464A1

## CPC

- H10F 77/1668: {presenting light-induced characteristic variations, e.g. Staebler-Wronski effect}
- H10F 10/17: Photovoltaic cells having only PIN junction potential barriers
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 77/244: {made of transparent conductive layers, e.g. transparent conductive oxide [TCO] layers}
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02E 10/548: Amorphous silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Methods for forming a photovoltaic device include forming a buffer layer between a transparent electrode and a p-type layer. The buffer layer includes a work function that falls substantially in a middle of a barrier formed between the transparent electrode and the p-type layer to provide a greater resistance to light induced degradation. An intrinsic layer and an n-type layer are formed over the p-type layer.

## Claims

### Claim 1

A method for forming a photovoltaic device, comprising:
forming a buffer layer between a transparent electrode and a p-type layer, the buffer layer including a work function that falls substantially in a middle of a barrier formed between the transparent electrode and the p-type layer to provide a greater resistance to light induced degradation; and
forming an intrinsic layer and an n-type layer over the p-type layer.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein forming the buffer layer includes depositing an amorphous form of germanium.

### Claim 3 (depends on 1)

The method as recited in claim 1, wherein forming the buffer layer includes depositing a germanium containing material at a deposition power of less than about 0.50 Watts per square centimeter.

### Claim 4 (depends on 3)

The method as recited in claim 3, wherein the deposition power includes a power of less than about 0.05 Watts per square centimeter.

### Claim 5 (depends on 1)

The method as recited in claim 1, wherein forming the buffer layer includes reducing initial photovoltaic device efficiency to provide improved long-term efficiency of the photovoltaic device.

### Claim 6 (depends on 1)

The method as recited in claim 1, wherein the buffer layer includes a Fermi level aligned with the transparent electrode.

### Claim 7 (depends on 1)

The method as recited in claim 1, wherein forming a buffer layer includes forming the buffer layer with a plasma enhanced chemical vapor deposition process.

### Claim 8 (depends on 1)

The method as recited in claim 1, wherein the p-type layer includes a form of silicon.

### Claim 9 (depends on 8)

The method as recited in claim 8, wherein the p-type layer includes at least one of amorphous silicon, amorphous silicon carbide, hydrogenated amorphous silicon, or hydrogenated amorphous silicon carbide.

### Claim 10

A method for forming a photovoltaic device, comprising:
forming a transparent electrode on a transparent substrate;
depositing a buffer layer on the transparent electrode, the buffer layer being deposited at a deposition power to provide an amorphous germanium layer with a work function that falls substantially in a middle of a barrier formed between adjacent layers to the buffer layer to provide a greater resistance to light induced degradation;
depositing a p-type layer on the buffer layer;
forming an intrinsic layer on the p-type layer; and
forming an n-type layer on the intrinsic layer.

### Claim 11 (depends on 10)

The method as recited in claim 10, wherein depositing the buffer layer includes depositing at least one of a hydrogenated amorphous silicon germanium alloy, or a hydrogenated amorphous germanium.

### Claim 12 (depends on 10)

The method as recited in claim 10, wherein the deposition power includes a power of less than about 0.50 Watts per square centimeter.

### Claim 13 (depends on 10)

The method as recited in claim 10, wherein the deposition power includes a power of less than about 0.050 Watts per square centimeter.

### Claim 14 (depends on 10)

The method as recited in claim 10, wherein depositing the buffer layer includes reducing initial efficiency to provide improved long-term efficiency of the photovoltaic device.

### Claim 15 (depends on 10)

The method as recited in claim 10, wherein the buffer layer includes a Fermi level aligned with the transparent electrode.

### Claim 16 (depends on 10)

The method as recited in claim 10, wherein depositing a buffer layer includes depositing the buffer layer with a plasma enhanced chemical vapor deposition process.

### Claim 17 (depends on 10)

The method as recited in claim 10, wherein the p-type layer includes at least one of amorphous silicon, amorphous silicon carbide, hydrogenated amorphous silicon, or hydrogenated amorphous silicon carbide.

### Claim 18

A method for forming a photovoltaic device, comprising:
forming a transparent conductive oxide on a transparent substrate;
depositing a buffer layer including germanium on the transparent conductive oxide, the buffer layer being deposited at a deposition power of less than about 0.05 Watts per square centimeter to adjust a work function of the buffer layer;
depositing a p-type amorphous silicon carbide layer on the buffer layer such that the work function of the buffer layer falls substantially in a middle of a barrier between the transparent electrode and the p-type layer to provide a greater resistance to light induced degradation;
forming an amorphous silicon intrinsic layer on the p-type layer;
forming an amorphous silicon n-type layer on the intrinsic layer; and
forming a back reflector on the n-type layer.

### Claim 19 (depends on 18)

The method as recited in claim 18, wherein depositing the buffer layer includes depositing at least one of a hydrogenated amorphous silicon germanium alloy, or a hydrogenated amorphous germanium.

### Claim 20 (depends on 10)

The method as recited in claim 10, wherein depositing the buffer layer includes reducing initial efficiency to provide improved long term efficiency of the photovoltaic device.

### Claim 21

A photovoltaic device, comprising:
a transparent conductive oxide formed on a transparent substrate;
a buffer layer including germanium formed on the transparent conductive oxide;
a p-type layer formed on the buffer layer such that the work function of buffer layer falls substantially in a middle of a barrier formed between the transparent electrode and the p-type layer to provide a greater resistance to light induced degradation;
an intrinsic layer formed on the p-type layer;
an n-type layer formed on the intrinsic layer; and
a back reflector formed on the n-type layer.

### Claim 22 (depends on 21)

The device as recited in claim 21, wherein the buffer layer includes at least one of a hydrogenated amorphous silicon germanium alloy, or a hydrogenated amorphous germanium.

### Claim 23 (depends on 21)

The device as recited in claim 21, wherein the work function includes a value within about ±10% of the middle of the barrier.

### Claim 24 (depends on 21)

The device as recited in claim 21, wherein the buffer layer includes a Fermi level aligned with the transparent electrode.

### Claim 25 (depends on 21)

The method as recited in claim 21, wherein the p-type layer includes at least one of amorphous silicon, amorphous silicon carbide, hydrogenated amorphous silicon, or hydrogenated amorphous silicon carbide.