# US 2013/0221073 A1 · Method and system for retreading track wheel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0221073 A1
- Document ID: US20130221073A1
- Status: Published application
- Kind: A1
- Application number: 13/857,504
- Filed: 2013-04-05
- Published: 2013-08-29
- Earliest claimed: 2011-03-11
- Inventors: CRAIG MERCIER
- Web page: https://patentgrep.com/patent/US20130221073A1

## CPC

- B23K 31/02: relating to soldering or welding
- B23K 9/044: {Built-up welding on three-dimensional surfaces}
- B23K 9/186: {making use of a consumable electrodes}
- B23P 6/00: Restoring or reconditioning objects (straightening or restoring form of sheet metal, metal rods, metal tubes, metal profiles, or specific articles made therefrom B21D1/00, B21D3/00; repairing defective or damaged objects by casting techniques B22D19/10)
- B23K 2101/26: Railway- or like rails
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)

## Abstract

A wheel resurfacing method and system for resurfacing a worn track wheel to its original profile are disclosed. The system comprises a support for maintaining the worn railway wheel, a welding device, a controller, and a surface processing device. The worn railway wheel's circumferential surface defining a flange and a tread surface is reconstituted using a welding material. The welding device and the worn railway wheel rotate one relative to the other at a predetermined rate to adaptively aggregate annular welding beads along the circumferential surface to form a curvilinear profile slanted away from the flange. A surface processing device is then applied to the welded layer to form a substantially uniform surface to reconstitute the worn railway wheel to its original profile.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A method for resurfacing a worn railway wheel substantially to an original profile, comprising the steps of:
maintaining a welding device spaced from the worn railway wheel, the worn railway wheel defining an axis;
displacing at least one of the welding device and worn railway wheel about the axis for continuous revolving displacement therebetween at a predetermined rate;
adaptively aggregating annular beads formed from a welding material along a circumferential surface of the worn railway wheel, the welding material being applied during the continuous revolving displacement to form a welded layer, the circumferential surface having a flange and a tread surface, each annular bead extending to substantially encircle a portion of the circumferential surface, whereby the welded layer forms a curvilinear profile tapered away from the flange; and
surface processing the welded layer to form a substantially uniform surface to substantially reconstitute the worn railway wheel to the original profile.

### Claim 16 (depends on 15)

The method for resurfacing the worn railway wheel of claim 15, further comprising the step of mechanically disturbing the worn railway wheel to form a plurality of grooves into the circumferential surface before the step of adaptively aggregating the annular beads.

### Claim 17 (depends on 16)

The method for resurfacing the worn railway wheel of claim 16, wherein the plurality of grooves are each formed to extend transversely on the circumferential surface before the step of adaptively aggregating the annular beads.

### Claim 18 (depends on 15)

The method for resurfacing the worn railway wheel of claim 15, further comprising the step of preheating the worn railway wheel to a predetermined temperature before the step of adaptively aggregating the annular beads.

### Claim 19 (depends on 15)

The method for resurfacing the worn railway wheel of claim 15, further comprising the steps of determining a metallurgical composition of the worn railway wheel and imaging the worn railway wheel for detecting internal faults therein before the step of adaptively aggregating the annular beads.

### Claim 20 (depends on 15)

The method for resurfacing the worn railway wheel of claim 15, wherein the worn railway wheel is pre-conditioned before the step of adaptively aggregating the annular beads, the pre-conditioning including grinding and cleaning the worn railway wheel.

### Claim 21 (depends on 15)

The method for resurfacing the worn railway wheel of claim 15, wherein the worn railway wheel is thermally decompressed after weld-processing for progressively controlled cooling.

### Claim 22 (depends on 15)

The method for resurfacing the worn railway wheel of claim 15, wherein the welding material is applied onto welding points defined along the circumferential surface in cooperation with a flux material, the flux material establishing an airtight flux covering over the welding points during application.

### Claim 23 (depends on 22)

The method for resurfacing the worn railway wheel of claim 22, wherein the flux material includes a stream of solid granular composition.

### Claim 24

A method for resurfacing a worn railway wheel substantially to an original profile, comprising the steps of:
maintaining a welding device spaced from the worn railway wheel, the worn railway wheel defining an axis;
displacing at least one of the welding device and worn railway wheel about the axis for continuous revolving displacement therebetween at a predetermined rate;
adaptively aggregating along a circumferential surface of the worn railway wheel annular beads formed from a welding material, the welding material being applied during the continuous revolving displacement to form a welded layer, the circumferential surface having a flange and a tread surface, each annular bead extending to substantially encircle a portion of the circumferential surface, whereby the welded layer forms a curvilinear profile tapered away from the flange; and
surface processing the welded layer to form a substantially uniform surface to substantially reconstitute the worn railway wheel to the original profile;
wherein the welding material is applied onto welding points defined along the circumferential surface in cooperation with a flux material, the flux material establishing an airtight flux covering over the welding points during application.

### Claim 25 (depends on 24)

The method for resurfacing the worn railway wheel of claim 24, further comprising the step of mechanically disturbing the worn railway wheel to form a plurality of grooves into the circumferential surface before the step of adaptively aggregating the annular beads.

### Claim 26 (depends on 25)

The method for resurfacing the worn railway wheel of claim 25, wherein the plurality of grooves are each formed to extend transversely on the circumferential surface before the step of adaptively aggregating the annular beads.

### Claim 27 (depends on 24)

The method for resurfacing the worn railway wheel of claim 24, further comprising the step of preheating the worn railway wheel to a predetermined temperature before the step of adaptively aggregating the annular beads.

### Claim 28 (depends on 24)

The method for resurfacing the worn railway wheel of claim 24, further comprising the steps of determining a metallurgical composition of the worn railway wheel and imaging the worn railway wheel for detecting internal faults therein before the step of adaptively aggregating the annular beads.

### Claim 29 (depends on 24)

The method for resurfacing the worn railway wheel of claim 24, wherein the worn railway wheel is pre-conditioned before the step of adaptively aggregating the annular beads, the pre-conditioning including grinding and cleaning the worn railway wheel.

### Claim 30 (depends on 24)

The method for resurfacing the worn railway wheel of claim 24, wherein the worn railway wheel is thermally decompressed after weld-processing for progressively controlled cooling.

### Claim 31 (depends on 24)

The method for resurfacing the worn railway wheel of claim 24, wherein the flux material includes a stream of solid granular composition.

### Claim 32

A method for resurfacing a worn railway wheel substantially to an original profile, comprising the steps of:
supporting the worn railway wheel and a welding device;
actuating rotational displacement between the worn railway wheel and the welding device one relative to the other at a predetermined rate;
mechanically disturbing the worn railway wheel to form a plurality of grooves into the circumferential surface, each of the grooves being formed to extend transversely on the circumferential surface;
adaptively aggregating annular beads formed from a welding material along a circumferential surface of the worn railway wheel to form a welded layer, the circumferential surface having a flange and a tread surface, each annular bead extending to substantially encircle a portion of the circumferential surface, whereby the welded layer forms a curvilinear profile tapered away from the flange; and,