# US 2013/0220974 A1 · Microporous carbons with aligned pores for supercapacitors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0220974 A1
- Document ID: US20130220974A1
- Status: Published application
- Kind: A1
- Application number: 13/781,429
- Filed: 2013-02-28
- Published: 2013-08-29
- Earliest claimed: 2012-02-28
- Assignees: Sila Nanotechnologies, Inc.
- Inventors: Gleb Nikolayevich Yushin
- Web page: https://patentgrep.com/patent/US20130220974A1

## CPC

- H01G 13/00: Apparatus specially adapted for manufacturing capacitors; Processes specially adapted for manufacturing capacitors not provided for in groups H01G4/00 - H01G11/00
- H01G 11/26: characterised by their structure, e.g. multi-layered, porosity or surface features
- H01G 11/32: Carbon-based
- H01G 11/86: specially adapted for electrodes (carbonisation or activation of carbon for the manufacture of electrodes H01G11/34)
- Y02E 60/13: Energy storage using capacitors
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A microporous carbon matrix material composition for use in supercapacitor electrodes may be produced by depositing carbon on a sacrificial zeolite template via one of several methods (e.g., hydrothermal or solvo-thermal deposition, sub-atmospheric vapor phase deposition, or high-pressure infiltration of hydrocarbon vapors). The deposition produces a carbon-coated zeolite intermediary. A surface layer of carbon formed on the carbon-coated zeolite intermediary may then be refined and the refined carbon-coated zeolite intermediary may be etched to produce a microporous carbon matrix having a substantially uniform structure and substantially aligned pores. In some embodiments, the carbon-coated zeolite intermediary may be annealed after deposition.

## Claims

### Claim 1

A method of producing a microporous carbon matrix material composition for use in supercapacitor electrodes, comprising:
depositing carbon on a sacrificial zeolite template via hydrothermal or solvo-thermal deposition to produce a carbon-coated zeolite intermediary;
refining a surface layer of carbon formed on the carbon-coated zeolite intermediary; and
etching the refined carbon-coated zeolite intermediary to produce a microporous carbon matrix having a substantially uniform structure and substantially aligned pores.

### Claim 2 (depends on 1)

The method of claim 1, further comprising annealing the carbon-coated zeolite intermediary after deposition.

### Claim 3 (depends on 1)

The method of claim 1, wherein the refining comprises physical activation of the surface layer to enlarge pores present therein.

### Claim 4 (depends on 3)

The method of claim 3, wherein the physical activation comprises heating the carbon-coated zeolite intermediary to a temperature in the range of about 700° C. to about 900° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the refining comprises milling the carbon-coated zeolite intermediary to remove at least a portion of the surface layer.

### Claim 6 (depends on 5)

The method of claim 5, wherein the milling comprises ball milling.

### Claim 7 (depends on 6)

The method of claim 6, further comprising annealing the carbon-coated zeolite intermediary at a temperature in the range of about 750° C. to about 1000° C. prior to the ball milling to improve pore alignment in the microporous carbon matrix.

### Claim 8 (depends on 6)

The method of claim 6, further comprising annealing the carbon-coated zeolite intermediary at a temperature in the range of about 750° C. to about 1000° C. after the ball milling to improve pore alignment in the microporous carbon matrix.

### Claim 9 (depends on 1)

The method of claim 1, wherein the refining comprises:
physical activation of the surface layer to enlarge pores present therein; and
ball milling the carbon-coated zeolite intermediary to remove at least a portion of the surface layer.

### Claim 10 (depends on 9)

The method of claim 9, further comprising annealing the carbon-coated zeolite intermediary prior to or after the ball milling to improve pore alignment in the microporous carbon matrix.

### Claim 11 (depends on 10)

The method of claim 10, wherein the annealing is performed after the physical activation.

### Claim 12 (depends on 1)

The method of claim 1, further comprising preparing a supercapacitor from the microporous carbon matrix and an organic electrolyte.

### Claim 13

A method of producing a microporous carbon matrix material composition for use in supercapacitor electrodes, comprising:
depositing carbon on a sacrificial zeolite template via sub-atmospheric vapor phase deposition to produce a carbon-coated zeolite intermediary;
refining a surface layer of carbon formed on the carbon-coated zeolite intermediary; and
etching the refined carbon-coated zeolite intermediary to produce a microporous carbon matrix having a substantially uniform structure and substantially aligned pores.

### Claim 14 (depends on 13)

The method of claim 13, wherein the refining comprises physical activation of the surface layer to enlarge pores present therein and/or ball milling the carbon-coated zeolite intermediary to remove at least a portion of the surface layer.

### Claim 15 (depends on 13)

The method of claim 13, further comprising preparing a supercapacitor from the microporous carbon matrix and an organic electrolyte.

### Claim 16

A method of producing a microporous carbon matrix material composition for use in supercapacitor electrodes, comprising:
depositing carbon on a sacrificial zeolite template via high-pressure infiltration of hydrocarbon vapors to produce a carbon-coated zeolite intermediary;
refining a surface layer of carbon formed on the carbon-coated zeolite intermediary; and
etching the refined carbon-coated zeolite intermediary to produce a microporous carbon matrix having a substantially uniform structure and substantially aligned pores.

### Claim 17 (depends on 16)

The method of claim 16, wherein the depositing is performed at or above three atmospheres of pressure.

### Claim 18 (depends on 16)

The method of claim 16, wherein the depositing comprises:
flowing a hydrocarbon gas over the sacrificial zeolite template at a substantially low temperature and elevated pressure to liquefy the hydrocarbon gas in the pores of the sacrificial zeolite template; and
carbonizing the carbon-coated zeolite intermediary after flowing the hydrocarbon gas.

### Claim 19 (depends on 16)

The method of claim 16, wherein the refining comprises physical activation of the surface layer to enlarge pores present therein and/or ball milling the carbon-coated zeolite intermediary to remove at least a portion of the surface layer.

### Claim 20 (depends on 16)

The method of claim 16, further comprising preparing a supercapacitor from the microporous carbon matrix and an organic electrolyte.
