# US 2013/0220078 A1 · Method for leaching of copper and molybdenum

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0220078 A1
- Document ID: US20130220078A1
- Status: Published application
- Kind: A1
- Application number: 13/819,148
- Filed: 2011-08-29
- Published: 2013-08-29
- Earliest claimed: 2010-08-27
- Assignees: Metaleach Limited
- Inventors: Nicholas James Welham; Garry Mervyn Johnston; Matthew Leslie Sutcliffe
- Web page: https://patentgrep.com/patent/US20130220078A1

## CPC

- C22B 15/0078: {with ammoniacal solutions, e.g. ammonium hydroxide}
- C22B 15/0069: {containing halogen}
- C22B 34/34: Obtaining molybdenum {(treatment or purification of solutions by adsorption on solids C22B3/24, by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42; preparation of molybdenum involving liquid-liquid extraction, adsorption or ion-exchange C01G39/003)}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for leaching copper and molybdenum from an ore, residue and/or concentrate containing such, in which more than 1% of the total molybdenum is present as a sulfide and in which more than 1% of the total copper is present as an oxide, the method comprising the steps of: Exposing the ore, residue and/or concentrate to an aqueous solution of chlorine (I)-based oxidising species of a p H of at least 3.0; Allowing and/or facilitating the oxidation of the molybdenum by the chlorine-based oxidising species thereby providing a treated ore, residue and/or concentrate and a reduced aqueous solution of chlorine-based oxidising species; and Leaching the treated ore, residue and/or concentrate by exposing the treated ore, residue and/or concentrate to an aqueous ammoniacal ammonium carbonate solution to form a pregnant leach solution containing both copper and molybdenum; Passing the pregnant leach solution containing both copper and molybdenum to a means for metal recovery.

## Claims

### Claim 1

A method for leaching copper and molybdenum from an ore, residue and/or concentrate containing such, in which more than 1% of the total molybdenum is present as a sulfide and in which more than 1% of the total copper is present as an oxide, the method comprising the steps of:
Exposing the ore, residue and/or concentrate to an aqueous solution of chlorine (I)-based oxidising species of a pH of at least 3.0;
Allowing and/or facilitating the oxidation of the molybdenum by the chlorine-based oxidising species thereby providing a treated ore, residue and/or concentrate and a reduced aqueous solution of chlorine-based oxidising species; and
Leaching the treated ore, residue and/or concentrate by exposing the treated ore, residue and/or concentrate to an aqueous ammoniacal ammonium carbonate solution to form a pregnant leach solution containing both copper and molybdenum;
Passing the pregnant leach solution containing both copper and molybdenum to a means for metal recovery.

### Claim 2 (depends on 1)

The method according to claim 1 wherein more than 20% of the total molybdenum is present as a sulfide.

### Claim 3 (depends on 1)

The method according to claim 1 wherein more than 20% of the total copper is present as an oxide.

### Claim 4 (depends on 1)

The method according to claim 1 wherein the ore, residue and/or concentrate is a porphyry float concentrate.

### Claim 5 (depends on 1)

The method according to claim 1 wherein the mixture comprising the treated ore, residue and/or concentrate and at least a residue from the reduced aqueous solution of chlorine-based oxidising species, and the step of:
leaching the treated ore, residue and/or concentrate by exposing the treated ore, residue and/or concentrate to an aqueous ammoniacal ammonium carbonate solution to form a pregnant leach solution containing both copper and molybdenum;
more specifically comprises
exposing the mixture to the aqueous ammoniacal ammonium carbonate solution to form the pregnant leach solution containing both copper and molybdenum.

### Claim 6 (depends on 5)

The method according to claim 5 wherein the mixture comprises the treated ore, residue and/or concentrate and the majority of the reduced aqueous solution of chlorine-based oxidising species.

### Claim 7 (depends on 6)

The method according to claim 6 wherein the mixture comprises the treated ore, residue and/or concentrate and substantially all of the reduced aqueous solution of chlorine-based oxidising species.

### Claim 8 (depends on 1)

The method according to claim 1 wherein the method does not employ any solid-liquid separation step prior to the exposure of the treated ore residue and/or concentrate to the ammoniacal ammonium carbonate solution.

### Claim 9 (depends on 1)

The method according to claim 1 wherein the pH of the reduced aqueous solution of chlorine-based oxidising species is neutral or basic.

### Claim 10 (depends on 9)

The method according to claim 9 wherein the pH of the reduced aqueous solution of chlorine-based oxidising species is between 7 and 10.

### Claim 11 (depends on 10)

The method according to claim 10 wherein the pH of the reduced aqueous solution of chlorine-based oxidising species is between 8 and 9.5.

### Claim 12 (depends on 1)

The method according to claim 1 wherein the pH of the aqueous solution of chlorine (I)-based oxidising species is at least 3.5.

### Claim 13 (depends on 1)

The method according to claim 1 wherein the predominant chlorine (I)-based oxidising species present in the aqueous solution of chlorine-based oxidising species is hypochlorite ion.

### Claim 14 (depends on 1)

The method according to claim 1 wherein the steps of:
Exposing the ore, residue and/or concentrate to an aqueous solution of chlorine (I)-based oxidising species of a pH of at least 3.0;
Allowing and/or facilitating the oxidation of the molybdenum by the chlorine-based oxidising species thereby providing a treated ore, residue and/or concentrate and a reduced aqueous solution of chlorine-based oxidising species; and
Leaching the treated ore, residue and/or concentrate by exposing the treated ore, residue and/or concentrate to an aqueous ammoniacal ammonium carbonate solution to form a pregnant leach solution containing both copper and molybdenum;
Passing the pregnant leach solution containing both copper and molybdenum to a means for metal recovery;
are performed at ambient temperature.

### Claim 15 (depends on 1)

The method according to claim 1 wherein the steps of:
Exposing the ore, residue and/or concentrate to an aqueous solution of chlorine (I)-based oxidising species of a pH of at least 3.0;
Allowing and/or facilitating the oxidation of the molybdenum by the chlorine-based oxidising species thereby providing a treated ore, residue and/or concentrate and a reduced aqueous solution of chlorine-based oxidising species; and
Leaching the treated ore, residue and/or concentrate by exposing the treated ore, residue and/or concentrate to an aqueous ammoniacal ammonium carbonate solution to form a pregnant leach solution containing both copper and molybdenum;
Passing the pregnant leach solution containing both copper and molybdenum to a means for metal recovery;
are performed at atmospheric pressure.

### Claim 16 (depends on 1)

The method according to claim 1 wherein the molybdenum content of the ore, residue and/or concentrate is less than 5% w/w.

### Claim 17 (depends on 1)

The method according to claim 1 wherein the copper content of the ore, residue and/or concentrate is less than 10% w/w.

### Claim 18 (depends on 1)

The method according to claim 1 wherein the ore, residue and/ore concentrate exposed to the aqueous solution of chlorine (I)-based oxidising species of a pH of at least 3.0 is previously unleached.

### Claim 19 (depends on 1)

The method according to claim 1 wherein the ore and/ore concentrate exposed to the aqueous solution of chlorine (I)-based oxidising species of a pH of at least 3.0 is previously unroasted.