# US 2013/0219800 A1 · Methods for Producing a Coated Abrasive Article for Polishing or Lapping Applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0219800 A1
- Document ID: US20130219800A1
- Status: Published application
- Kind: A1
- Application number: 13/862,592
- Filed: 2013-04-15
- Published: 2013-08-29
- Earliest claimed: 2008-11-04
- Inventors: Olivier L. Guiselin
- Web page: https://patentgrep.com/patent/US20130219800A1

## CPC

- C09D 7/45: Anti-settling agents
- B24D 3/00: Physical features of abrasive bodies, or sheets, e.g. abrasive surfaces of special nature; Abrasive bodies or sheets characterised by their constituents
- B24D 3/28: Resins {or natural or synthetic macromolecular compounds (B24D3/22 takes precedence)}
- B24D 11/00: Constructional features of flexible abrasive materials; Special features in the manufacture of such materials
- C09D 5/28: for wrinkle, crackle, orange-peel, or similar decorative effects
- C09D 7/62: modified by treatment with other compounds
- C09D 7/67: {Particle size smaller than 100 nm}
- C09D 7/68: {Particle size between 100-1000 nm}
- C09D 7/69: {Particle size larger than 1000 nm}
- C09K 3/1463: {Aqueous liquid suspensions}
- C08K 3/10: Metal compounds
- C08K 9/02: Ingredients treated with inorganic substances
- C08K 9/04: Ingredients treated with organic substances {(treated with macromolecular compounds C08K9/08)}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

Methods are provided for forming an abrasive coating on a surface of a backing. An abrasive slurry includes a continuous phase, a first discontinuous phase of abrasive particles dispersed in the continuous liquid phase, and a second discontinuous phase of binder precursor particles dispersed in the continuous liquid phase, so that the continuous liquid phase carries the first and second discontinuous phases. A coated abrasive article is formed by coating the abrasive slurry onto the surface of the backing, and then removing the continuous phase.

## Claims

### Claim 1

A method of manufacturing a coated abrasive article comprising:
(a) providing a flexible backing having a surface configured for being coated with an abrasive coating;
(b) providing an abrasive slurry including a continuous liquid phase, which comprises at least 50% per weight of water, and at least 0.001% per weight of fluorosurfactant;
a first discontinuous phase including abrasive particles dispersed in the continuous liquid phase; and
a second discontinuous phase including a waterborne binder precursor particle dispersion in the continuous liquid phase,
wherein the continuous liquid phase carries the first and second discontinuous phases,
wherein the volume ratio of abrasive particles to binder precursor particles is 0.05 to 3, and wherein the first and the second discontinuous phases comprise between 5% and 60% of the abrasive slurry by volume;
(c) coating the abrasive slurry onto the surface of the flexible backing;
(d) removing at least 50% per weight of the continuous liquid phase by evaporation; and
(e) coalescing the binder precursor particles at the surface of the flexible backing to form a coating with solid continuous binder phase disposed about the abrasive particles.

### Claim 2

A method of manufacturing a coated abrasive article comprising:
(a) providing a flexible backing having a surface configured for being coated with an abrasive coating;
(b) providing an abrasive slurry including
a continuous liquid phase, which comprises at least 60% per weight of water, and at least 0.001% per weight of fluorosurfactant;
a first discontinuous phase including abrasive particles dispersed in the continuous liquid phase; and
a second discontinuous phase including a waterborne binder precursor particle dispersion in the continuous liquid phase,
wherein the continuous liquid phase carries the first and second discontinuous phases, wherein the volume ratio of abrasive particles to binder precursor particles is 0.05 to 3, wherein the first and the second discontinuous phases comprise between 5% and 60% of the abrasive slurry by volume, and wherein the viscosity of the abrasive slurry is less than 100,000 cP;
(c) coating the abrasive slurry onto the surface of the flexible backing;
(d) removing at least 60% per weight of the continuous liquid phase by evaporation; and
(e) coalescing the binder precursor particles at the surface of the flexible backing.

### Claim 3 (depends on 2)

The method of claim 2, wherein the continuous liquid phase comprises at least about 90% per weight of water and wherein the abrasive and binder precursor particles comprise between 5% and 50% of the slurry by volume and the method comprises removing at least 90% per weight of the continuous liquid phase by evaporation.

### Claim 4 (depends on 2)

The method of claim 2, wherein the coalesced binder precursor particles form a continuous phase around the abrasive particles.

### Claim 5 (depends on 4)

The method of claim 4, wherein the continuous liquid phase comprises at least one coalescing agent configured to reduce the film forming temperature of the binder precursor particle dispersion.

### Claim 6 (depends on 5)

The method of claim 5, wherein the waterborne binder precursor particle dispersion is selected from the group consisting of waterborne acrylics emulsion, waterborne polyurethanes dispersion, waterborne urethane-acrylic copolymers dispersion, waterborne polyesters dispersion, waterborne alkyds dispersion, waterborne epoxies dispersion, waterborne phenoxy dispersion, waterborne melamine dispersion, waterborne polyamide dispersion, waterborne polyimide dispersion, waterborne cyanate esters dispersion, and combinations thereof.

### Claim 7 (depends on 2)

The method of claim 2 wherein the second discontinuous phase comprises a cross-linkable resin, the method comprising thermally curing the abrasive slurry coating using at least one energy source.

### Claim 8 (depends on 7)

The method of claim 7, comprising transmitting energy from the energy source by convection, conduction, radiation, or combinations thereof.

### Claim 9 (depends on 7)

The method of claim 7, the continuous liquid phase comprises a curing agent selected from the group consisting of metal ion crosslinkers, polyaldehydes, polyaziridines, polyisocyanates, polysulfides, imidazoles, dicyandiamines, polyamidoamines, polyamides, polyamines, functionalized silanes, functionalized siloxane, carbodiimides, peroxides, and combinations thereof.

### Claim 10 (depends on 2)

The method of claim 2, wherein the second discontinuous phase comprises binder precursor particles of:
at least about 5 nanometers in size; and
up to about 50 micrometers in size.

### Claim 11 (depends on 10)

The method of claim 10, wherein the second discontinuous phase comprises binder precursor particles of:
at least about 10 nanometers in size; and
up to about 10 micrometers in size.

### Claim 12 (depends on 11)

The method of claim 11, wherein the second discontinuous phase comprises binder precursor particles of:
at least about 50 nanometers in size; and
up to about 2 micrometers in size.

### Claim 13 (depends on 2)

The method of claim 2, wherein the abrasive particles are selected from the group consisting of natural diamond, synthetic diamond, cubic boron nitride, aluminum oxide, heat treated aluminum oxide, white fused aluminum oxide, black silicon carbide, green silicon carbide, titanium diboride, boron carbide, tungsten carbide, titanium carbide, garnet, fused alumina zirconia, sol gel abrasive material, silica, silicate, iron oxide, zirconium oxide, titanium dioxide, tin oxide, cerium oxide, rare earth containing ceramic materials, aluminum oxide containing ceramic material, zirconium oxide, chromium oxide, and mixtures thereof.

### Claim 14 (depends on 2)

The method of claim 2, wherein the abrasive slurry comprises at least one adhesion promoter selected from the group consisting of silanes, titanates, zirconates, phosphates, phosphonates, phosphinates, and combinations thereof.

### Claim 15 (depends on 2)

The method of claim 2, wherein the abrasive slurry further comprises a foam control agent.

### Claim 16 (depends on 2)

The method of claim 2, wherein the abrasive slurry further comprises a wetting agent.

### Claim 17 (depends on 2)

The method of claim 2, wherein the abrasive slurry comprises a rheology modifier and the weight ratio of the rheology modifier to the quantity of water in the slurry is between 0.0005 and 0.10 whereby the viscosity of the abrasive slurry is adjusted to a value between 10 cP and 50,000 cP.

### Claim 18 (depends on 2)

The method of claim 2, wherein the flexible backing is selected from the group consisting of plastic film, metallic foil, cloth, paper, foam and combinations thereof.

### Claim 19

A method of manufacturing a coated abrasive article comprising:
(a) providing a flexible backing having a surface configured for being coated with an abrasive coating,
wherein the flexible backing is selected from the group consisting of plastic film, metallic foil, cloth, paper, foam and combinations thereof;
(b) providing an abrasive slurry including a continuous liquid phase, which comprises at least 90% per weight of water, and at least 0.01% per weight of fluorosurfactant;
a first discontinuous phase including abrasive particles dispersed in the continuous liquid phase; and
a second discontinuous phase including a waterborne binder precursor particle dispersion in the continuous liquid phase,
wherein the continuous liquid phase carries the first and second discontinuous phases, wherein the volume ratio of abrasive particles to binder precursor particles is 0.05 to 2, and wherein the first and the second discontinuous phases comprise between 10% and 40% of the abrasive slurry by volume;
wherein the waterborne binder precursor particle dispersion is selected from the group consisting of waterborne acrylics emulsion, waterborne polyurethanes dispersion, waterborne urethane-acrylic copolymers dispersion, waterborne polyesters dispersion, waterborne alkyds dispersion, waterborne epoxies dispersion, waterborne phenoxy dispersion, waterborne melamine dispersion, waterborne polyamide dispersion, waterborne polyimide dispersion, waterborne cyanate esters dispersion, and combinations thereof;
wherein the continuous liquid phase comprises a curing agent selected from the group consisting of metal ion crosslinkers, polyaldehydes, polyaziridines, polyisocyanates, polysulfides, imidazoles, dicyandiamines, polyamidoamines, polyamides, polyamines, functionalized silanes, functionalized siloxane, carbodiimides, peroxides, and combinations thereof.
(c) coating the abrasive slurry onto the surface of the flexible backing;
(d) removing at least 90% per weight of the continuous liquid phase by evaporation;
(e) coalescing the binder precursor particles at the surface of the flexible backing to form a coating with solid continuous binder phase disposed about the abrasive particles; and
(f) thermally curing the coating using at least one energy source.

### Claim 20 (depends on 19)

The method of claim 19, wherein the continuous liquid phase comprises at least 0.02% per weight of fluorosurfactant.