# US 2013/0199936 A1 · Methods and Electrolytes for Electrodeposition of Smooth Films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0199936 A1
- Document ID: US20130199936A1
- Status: Published application
- Kind: A1
- Application number: 13/495,727
- Filed: 2012-06-13
- Published: 2013-08-08
- Earliest claimed: 2012-02-07
- Assignees: Battelle Memorial Institute
- Inventors: Jiguang Zhang; Wu Xu; Gordon L. Graff; Xilin Chen; Fei Ding; Yuyan Shao
- Web page: https://patentgrep.com/patent/US20130199936A1

## CPC

- C25D 5/605: {Surface topography of the layers, e.g. rough, dendritic or nodular layers}
- C09D 5/4484: {Anodic paints (C09D5/4403 - C09D5/4476 take precedence)}
- C25D 3/02: from solutions (C25D5/34 - C25D5/46 take precedence)
- C25D 3/12: of nickel or cobalt
- C25D 3/20: of iron
- C25D 3/22: of zinc
- C25D 3/30: of tin
- C25D 3/38: of copper
- C25D 3/42: of light metals
- C25D 3/46: of silver
- C25D 3/48: of gold
- C25D 3/50: of platinum group metals
- C25D 3/56: of alloys
- C25D 13/22: Servicing or operating {apparatus or multistep processes}
- Y02E 60/10: Energy storage using batteries
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Electrodeposition involving an electrolyte having a surface-smoothing additive can result in self-healing, instead of self-amplification, of initial protuberant tips that give rise to roughness and/or dendrite formation on the substrate and/or film surface. For electrodeposition of a first conductive material (C1) on a substrate from one or more reactants in an electrolyte solution, the electrolyte solution is characterized by a surface-smoothing additive containing cations of a second conductive material (C2), wherein cations of C2 have an effective electrochemical reduction potential in the solution lower than that of the reactants.

## Claims

### Claim 1

An electrolyte solution for electrodeposition of a first conductive material (C1) on a substrate from one or more reactants in the electrolyte solution, the electrolyte solution characterized by a soluble, surface-smoothing additive comprising cations of a second conductive material (C2), wherein cations of C2 have an effective electrochemical reduction potential in the solution lower than that of the reactants.

### Claim 2 (depends on 1)

The electrolyte solution of claim 1, wherein C1 is a metallic material and the reactants comprise cations of C1.

### Claim 3 (depends on 2)

The electrolyte solution of claim 2, wherein C1 comprises a metal selected from the group consisting of Li, Na, Mg, Al, Sn, Ti, Fe, Ni, Cu, Zn, Ag, Pt, Au, and combinations thereof.

### Claim 4 (depends on 1)

The electrolyte solution of claim 1, wherein C1 comprises an electronic conductive polymer and the reactants comprise monomers of the polymer.

### Claim 5 (depends on 1)

The electrolyte solution of claim 1, wherein the cations of C2 are metal cations.

### Claim 6 (depends on 5)

The electrolyte solution of claim 5, wherein the cations of C2 comprise a metal selected from the group consisting of Cs, Rb, K, Ba, Sr, Ca, Li, and combinations thereof.

### Claim 7 (depends on 1)

The electrolyte solution of claim 1, wherein the cations of C2 have an activity in solution such that the effective electrochemical reduction potential of cations of C2 is lower than that of the reactants.

### Claim 8 (depends on 1)

The electrolyte solution of claim 1, wherein the cations of C2 have a concentration in solution such that the effective electrochemical reduction potential of cations of C2 is lower than that of the reactants.

### Claim 9 (depends on 1)

The electrolyte solution of claim 1, wherein the concentration of C2 cations is less than, or equal to, 30% of that of the reactants.

### Claim 10 (depends on 1)

The electrolyte solution of claim 1, wherein the concentration of C2 cations is less than, or equal to, 5% of that of the reactants.

### Claim 11 (depends on 1)

The electrolyte solution of claim 1, wherein the surface-smoothing additive comprises an anion selected from the group consisting of PF6−, AsF6−, BF4−, N(SO2CF3)2−, N(SO2O2−, CF3SO3−, ClO4−, I−, Cl−, OH−, NO3−, SO42− and combinations thereof.

### Claim 12 (depends on 1)

The electrolyte solution of claim 1, wherein the substrate is an electrode.

### Claim 13 (depends on 12)

The electrolyte solution of claim 12, wherein the electrode comprises lithium.

### Claim 14 (depends on 12)

The electrolyte solution of claim 12, wherein the electrode comprises carbon.

### Claim 15 (depends on 12)

The electrolyte solution of claim 12, wherein the electrode is an electrode in an energy storage device.

### Claim 16 (depends on 1)

The electrolyte solution of claim 1, wherein the cations of C2 are not chemically or electrochemically reactive with respect to C1 or the reactants.

### Claim 17

A method for improving surface smoothness during electrodeposition of a first conductive material (C1) on a substrate surface, the method comprising:
providing an electrolyte solution comprising reactants from which C1 is synthesized and a soluble, surface-smoothing additive comprising cations of a second conductive material (C2), wherein cations of C2 have an effective electrochemical reduction potential in the solution lower than that of the reactants; and
applying an electrical potential thereby reducing the reactants and forming C1 on the substrate surface.

### Claim 18 (depends on 17)

The method of claim 17, further comprising:
accumulating cations of C2 at protrusions on the substrate surface, thereby forming an electrostatically shielded region near each protrusion; and
temporarily repelling reactants from the electrostatically shielded regions.

### Claim 19 (depends on 17)

The method of claim 17, wherein C1 is a metallic material and the reactants comprise cations of C1.

### Claim 20 (depends on 19)

The method of claim 19, wherein C1 is selected from the group consisting of Na, K, Rb, Cs, Be, Mg, Ca, Sr, Ba, Al, Ga, In, Tl, Ge, Sn, Pb, As, Sb, Bi, Se, Te, Bi, Po, Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Y, Zr, Nb, Mo, Tc, Ru, Rh, Pd, Ag, Cd, W, Pt, Au, Hg, and combinations thereof.

### Claim 21 (depends on 19)

The method of claim 19, wherein C1 comprises Li.

### Claim 22 (depends on 17)

The method of claim 17, wherein C1 comprises an electronic conductive polymer and the reactants comprise monomers of the polymer.

### Claim 23 (depends on 17)

The method of claim 17, wherein the cations of C2 are metal cations.

### Claim 24 (depends on 23)

The method of claim 23, wherein the cations of C2 comprise a metal selected from the group consisting of Li, Cs, Rb, K, Ba, La, Sr, Ca, Ra, Zr, Te, B, Bi, Ta, Ga, Eu, S, Se, Nb, Na, Mg, Cu, Al, Fe, Zn, Ni, Ti, Sn, Sb, Mn, V, Ta, Cr, Au, Ge, Co, As, Ag, Mo, Si, W, Ru, I, Fc, Br, Re, Bi, Pt, Pd, and combinations thereof.

### Claim 25 (depends on 17)

The method of claim 17, wherein the cations of C2 have an activity in solution such that the effective electrochemical reduction potential of the cations of C2 is lower than that of the reactants.

### Claim 26 (depends on 17)

The method of claim 17, wherein the concentration of the cations of C2 is less than, or equal to, 30% of that of the reactants.

### Claim 27 (depends on 17)

The method of claim 17, wherein the concentration of the cations of C2 is less than, or equal to, 5% of that of the reactants.

### Claim 28 (depends on 17)

The method of claim 17, wherein the surface-smoothing additive comprises an anion selected from the group consisting of PF6−, AsF6−, BF4−, N(SO2CF3)2−, N(SO2F)2−, CF3SO3−, ClO4−, I−, Cl−, OH−, NO3−, SO42−, and combinations thereof.

### Claim 29 (depends on 17)

The method of claim 17, wherein the substrate is an electrode.

### Claim 30 (depends on 29)

The method of claim 29, wherein the electrode comprises lithium.

### Claim 31 (depends on 29)

The method of claim 29, wherein the electrode comprises carbon.

### Claim 32 (depends on 17)

The method of claim 17, wherein the electrical potential applied is less than the electrochemical reduction potential of the reactant and greater than the effective electrochemical reduction potential of the cations of C2.

### Claim 33

A method for improving surface smoothness during electrodeposition of lithium on a substrate surface, the method comprising:
providing an electrolyte solution comprising lithium cations and a soluble, surface-smoothing additive comprising cations of a second conductive material (C2) selected from the group consisting of cesium, rubidium, potassium, strontium, barium, calcium, and combinations thereof, wherein cations of C2 have an activity in solution such that the effective electrochemical reduction potential of the cations of C2 is lower than that of the lithium cations;
applying an electrical potential thereby reducing the lithium cations and forming lithium on the substrate surface;
accumulating cations of C2 at protrusions on the substrate surface, thereby forming an electrostatically shielded region near each protrusion; and
temporarily repelling the lithium cations from the electrostatically shielded regions.

### Claim 34 (depends on 33)

The method of claim 33, wherein the cations of C2 have a concentration in the electrolyte that is less than, or equal to, 30% of that of the lithium cations.

### Claim 35 (depends on 33)

The method of claim 33, wherein the cations of C2 have a concentration in the electrolyte that is less than, or equal to, 5% of that of the lithium cations.

### Claim 36 (depends on 33)

The method of claim 33, wherein the surface-smoothing additive comprises an anion comprising PF6− anion.

### Claim 37 (depends on 33)

The method of claim 33, wherein the substrate is a battery anode comprising lithium or a battery anode comprising carbon.

### Claim 38 (depends on 33)

The method of claim 33, wherein the electrical potential applied is less than the electrochemical reduction potential of the lithium cations and greater than the effective electrochemical reduction potential of the cations of C2.