Disclosed is a composition, useful for a coating material, comprising coal ash and latex polymer and optionally a hydraulic binder, a superplasticizer, a rheology modifier, a filler, an aggregate, a foaming agent, a de-foaming agent, an accelerant and/or a retardant. The composition possesses favorable physicochemical properties and a low carbon footprint.
Claims20
A composition, useful for a coating material, comprising:
- (a) no more than 75%, by weight, coal ash, wherein the loss on ignition of the coal ash is greater than 3%;
- (b) at least 25%, by weight, latex polymer;
- and optionally (c) a hydraulic binder, a superplasticizer, a rheology modifier, a filler, an aggregate, a foaming agent, a de-foaming agent, a reinforcing agent, an accelerant and/or a retardant.
A composition, useful for a coating material, consisting of:
- (a) no more than 75%, by weight, coal ash, wherein the loss on ignition of the coal ash is greater than 3%;
- and (b) at least 25%, by weight, latex polymer.
A coating material produced by admixing (a) no more than 75%, by weight, coal ash, wherein the loss on ignition of the coal ash is greater than 3%;
- (b) at least 25%, by weight, latex polymer;
- and optionally (c) a hydraulic binder, a superplasticizer, a rheology modifier, a filler, an aggregate, a foaming agent, a de-foaming agent, a reinforcing agent, an accelerant and/or a retardant.
An article, comprising a surface and a coating, the article manufactured by contacting, with a surface in need of coating, a coating comprising (a) no more than 75%, by weight, coal ash, wherein the loss on ignition of the coal ash is greater than 3%;
- and (b) at least 25%, by weight, latex polymer.
A consumable article, comprising a suitable container-closure system and a coating material, wherein the coating material is contained within the suitable container-closure system, and wherein the coating material is produced by admixing (a) no more than 75%, by weight, coal ash, wherein the loss on ignition of the coal ash is greater than 3%;
- and (b) at least 25%, by weight, latex polymer;
- and optionally (c) a hydraulic binder, a superplasticizer, a rheology modifier, a filler, an aggregate, a foaming agent, a de-foaming agent, a reinforcing agent, an accelerant and/or a retardant.
Dependencies are inferred from the claim text.