# US 2013/0158214 A1 · Catalyst components for the polymerization of olefins

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0158214 A1
- Document ID: US20130158214A1
- Status: Published application
- Kind: A1
- Application number: 13/818,626
- Filed: 2011-08-10
- Published: 2013-06-20
- Earliest claimed: 2010-08-24
- Assignees: Basell Pollolefine Italia s.r.l.
- Inventors: Joachim T.M. Pater; Dario Liguori; Gianni Vitale; Gianni Collina; Diego Brita; Tiziano Dall'Occo; Giampiero Morini
- Web page: https://patentgrep.com/patent/US20130158214A1

## CPC

- C08F 4/46: selected from alkali metals
- C08F 10/00: Homopolymers and copolymers of unsaturated aliphatic hydrocarbons having only one carbon-to-carbon double bond
- C08F 4/6494: {containing oxygen}
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A solid catalyst component for olefin polymerization, and in particular for the preparation of LLDPE, comprising Mg, Ti, halogen and an electron donor compound (ID) belonging to cyclic ethers having 3-6 carbon atoms, characterized by having the molar ratio Mg/Ti higher than 5, the molar ratio Mg/ID lower than 3, and by a specific X-ray diffraction spectrum.

## Claims

### Claim 1

A solid catalyst component for olefin polymerization, comprising Mg, Ti, halogen and an electron donor compound (ID) belonging to cyclic ethers having 3-6 carbon atoms, characterized by a molar ratio Mg/Ti higher than 5, a molar ratio Mg/ID lower than 3, and by a X-ray diffraction spectrum, in which, in the range of 2θ diffraction angles between 5.0° and 20.0°, at least three main diffraction peaks are present at diffraction angles 2θ of 7.2±0.2°, and 11.5±0.2° and 14.5±0.2° said peak at 2θ of 7.2±0.2° being the most intense one and the peak at 11.5±0.2° having an intensity less than 0.9 times the intensity of the most intense peak.

### Claim 2 (depends on 1)

The solid catalyst component according to claim 1 in which in the X-ray diffraction spectrum, the intensity of the peak at 11.5° has an intensity less than 0.8 times the intensity of the diffraction peak at 2θ diffraction angles of 7.2±0.2°.

### Claim 3 (depends on 1)

The solid catalyst component according to claim 1 in which in the X-ray diffraction spectrum another diffraction peak is present at diffraction angles 2θ of 8.2±0.2° having intensity less than 0.9 times the intensity of the diffraction peak at 2θ diffraction angles of 7.2±0.2°.

### Claim 4 (depends on 1)

The solid catalyst component according to claim 1 in which in the X-ray diffraction spectrum, is present also an additional broad peak at diffraction angles 2θ of 18.2±0.2° having intensity less than 0.5 times the intensity of the diffraction peak at 2θ diffraction angles of 7.2±0.2°.

### Claim 5 (depends on 1)

The solid catalyst component according to claim 1 in which the ID compound is selected among cyclic ethers having 3-5 carbon atoms.

### Claim 6 (depends on 5)

The solid catalyst component according to claim 5 in which the ID compound is tetrahydrofurane.

### Claim 7 (depends on 1)

The solid catalyst component according to claim 1 in which the Mg/ID molar ratio is lower than 2.9

### Claim 8 (depends on 1)

The solid catalyst component according to claim 1 in which Mg/Ti molar ratio ranges from 7 to 50.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

Process for the preparation of the solid catalyst component according to any of the claim 1-8 comprising the following steps: (a) contacting a titanium tetrahalide or a titanium compound of formula TiXn(OR1)4-n, where 0≦n≦3, X is halogen, and R1 is C1-C10 hydrocarbon group with a MgX2(R″OH)m adduct in which R″ groups are C1-C20 hydrocarbon groups and X is halogen, in order to prepare an intermediate product, containing a titanium compound supported on Mg dichloride; (b) contacting an internal donor compound (ID) selected from cyclic ethers having 3-6 carbon atoms with the intermediate product, coming from (a) under conditions to have on the resulting solid an Mg/ID molar ratio lower than 3 and (c) subjecting the solid catalyst component coming from (b) to a thermal treatment carried out at a temperature from 70 to 150° C.

### Claim 10 (depends on 9)

The process according to claim 9 in which the thermal treatment is carried out at temperature ranging from 80 to 130° C.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

A catalyst for the polymerization of olefins comprising the product obtained by contacting:
A a solid catalyst component according to anyone of the claims 1-8;
B one or more aluminum alkyl compounds and, optionally,
C an external electron donor compound.

### Claim 12 (depends on 11)

The catalyst according to claim 11, in which the aluminum alkyl compound is an Al trialkyl.

### Claim 13 (depends on 11)

The catalyst according to claim 11 in which the alkylaluminum compound is the product obtained by mixing one or more trialkylaluminum compound with an alkylaluminum halide.

### Claim 14 (depends on 11)

The catalyst according to claim 11, characterized by further comprising a halogenated compound (D) as activity enhancer.

### Claim 15 (depends on 11)

A process for the (co)polymerization of olefins CH2=CHR, wherein R is hydrogen or a hydrocarbon radical having 1-12 carbon atoms, carried out in the presence of a catalyst according to claim 11.