# US 2013/0158213 A1 · Process for the preparation of a polyolefin polymer with improved wax deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0158213 A1
- Document ID: US20130158213A1
- Status: Published application
- Kind: A1
- Application number: 13/818,845
- Filed: 2011-08-30
- Published: 2013-06-20
- Earliest claimed: 2010-08-31
- Assignees: Basell Polyolefine GmbH
- Inventors: Gerhardus Meier; Reinhard Kuehl; Harald Prang; Michael Aulbach
- Web page: https://patentgrep.com/patent/US20130158213A1

## CPC

- C08F 2/04: Polymerisation in solution (C08F2/32 takes precedence)
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Process for the preparation of a polyolefin polymer by continuously polymerizing one or more olefin monomers in suspension at temperatures of from 40° C. to 120° C. and pressures of from 0.1 to 10 MPa in the presence of a polymerization catalyst in at least one polymerization reactor, comprising a) withdrawing a suspension of solid polyolefin particles in a suspension medium from the polymerization reactor, wherein the suspension has a temperature of from 65° C. to 120° C.; b) feeding the suspension withdrawn from the polymerization reactor to a moderating vessel; c) keeping the suspension in the moderating vessel at a temperature of from 60° C. to 85° C. for a time sufficiently long that the mean residence time of the suspension in the moderating vessel is at least 5 min; d) withdrawing suspension from the moderating vessel; e) cooling the suspension withdrawn from the moderating vessel to a temperature of from 20° C. to 55° C.; and f) mechanically separating the solid polyolefin particles from the liquid suspension medium, and method for controlling the content of hydrocarbons with from 14 to 300 carbon atoms in a polyolefin polymer prepared by polymerizing one or more olefin monomers in suspension.

## Claims

### Claim 1

A process for the preparation of a polyolefin polymer by continuously polymerizing one or more olefin monomers in suspension at temperatures of from 40° C. to 120° C. and pressures of from 0.1 to 10 MPa in the presence of a polymerization catalyst in at least one polymerization reactor, comprising
a) withdrawing a suspension of solid polyolefin particles in a suspension medium from the polymerization reactor, wherein the suspension has a temperature of from 65° C. to 120° C.;
b) feeding the suspension withdrawn from the polymerization reactor to a moderating vessel;
c) keeping the suspension in the moderating vessel at a temperature of from 60° C. to 85° C. for a time sufficiently long that the mean residence time of the suspension in the moderating vessel is at least 5 min;
d) withdrawing suspension from the moderating vessel;
e) cooling the suspension withdrawn from the moderating vessel to a temperature of from 20° C. to 55° C.; and
f) mechanically separating the solid polyolefin particles from the liquid suspension medium.

### Claim 2 (depends on 1)

A process according to claim 1, wherein the polymerization reactor from which the suspension is withdrawn in step a) is the last polymerization reactor of a series of polymerization reactors.

### Claim 3 (depends on 1)

A process according to claim 1, wherein the moderating vessel is operated at a pressure of from 0.101 MPa to 1.0 MPa.

### Claim 4 (depends on 1)

A process according to any of claims 1, wherein the suspension in the moderating vessel is cooled by returning a part of the suspension cooled in step e) to the moderating vessel.

### Claim 5 (depends on 1)

A process according to any of claims 1, wherein the suspension in the moderating vessel is cooled by vaporizing a part of the liquid suspension medium in the moderating vessel.

### Claim 6 (depends on 1)

A process according to any of claims 1, wherein the suspension is fed after cooling step e) to a collecting vessel.

### Claim 7 (depends on 6)

A process according to claim 6, wherein the suspension is kept in the collecting vessel at a temperature of from 20° C. to 55° C. sufficiently long that the mean residence time of the suspension in the collecting vessel is at least 5 min.

### Claim 8 (depends on 1)

A process according to any of claims 1, wherein the separation of solid polyolefin particles and the liquid suspension medium takes place in a centrifuge.

### Claim 9 (depends on 1)

A process according to any of claims 1, wherein the liquid suspension medium separated from the polyolefin particles in step f) comprises less than 3 wt.-% of solved waxy components, which content is determined by passing the suspension medium at a temperature of 60° C. through a filter, evaporating the liquid by heating till 120° C. at 40 kPa for 30 min, and weighting the residue.

### Claim 10 (depends on 1)

A process according to any of claims 1, wherein the liquid suspension medium separated from the polyolefin particles in step f) is fed to one or more of the polymerization reactors, in which the polyolefin polymer is prepared.

### Claim 11

A method for controlling the content of hydrocarbons with from 14 to 300 carbon atoms in a polyolefin polymer prepared by continuously polymerizing one or more olefin monomers in suspension at temperatures of from 40° C. to 120° C. and pressures of from 0.1 to 10 MPa in the presence of a polymerization catalyst in at least one polymerization reactor, comprising
a) withdrawing a suspension of solid polyolefin particles in a suspension medium from the polymerization reactor, wherein the suspension has a temperature of from 65° C. to 120° C.;
b) feeding the suspension withdrawn from the polymerization reactor to a moderating vessel;
c) withdrawing suspension from the moderating vessel;
d) cooling the suspension withdrawn from the moderating vessel to a temperature of from 20° C. to 55° C.; and
e) mechanically separating the solid polyolefin particles from the liquid suspension medium,
wherein the content of hydrocarbons with from 14 to 300 carbon atoms in the polyolefin polymer is controlled by setting the temperature of the suspension in the moderating vessel and/or the mean residence time of the suspension in the moderating vessel to predefined values.