# US 2013/0158209 A1 · Method for producing polylactic acid block copolymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0158209 A1
- Document ID: US20130158209A1
- Status: Published application
- Kind: A1
- Application number: 13/819,199
- Filed: 2011-06-27
- Published: 2013-06-20
- Earliest claimed: 2010-08-31
- Assignees: Toray Industries, Inc.
- Inventors: Yoshitake Takahashi; Takuma Naotsuka; Ken Sudo; Hiroyuki Ome
- Web page: https://patentgrep.com/patent/US20130158209A1

## CPC

- C08G 63/80: Solid-state polycondensation
- C08G 63/06: derived from hydroxycarboxylic acids
- C08G 63/08: Lactones or lactides
- C08G 63/823: {for the preparation of polylactones or polylactides}
- C08G 63/912: {derived from hydroxycarboxylic acids}
- C08L 67/04: Polyesters derived from hydroxycarboxylic acids, e.g. lactones (C08L67/06 takes precedence)
- C08G 2261/126: block
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/05: containing polymer components which can react with one another
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A method of producing a polylactic acid block copolymer constituted of a segment(s) composed of L-lactic acid units and a segment(s) composed of D-lactic acid units, includes obtaining a mixture by mixing poly-L-lactic acid and poly-D-lactic acid one of which has a weight average molecular weight of 60,000 to 300,000 and the other of which has a weight average molecular weight of 10,000 to 50,000, the mixture having a weight average molecular weight of not less than 90,000 and a degree of stereocomplexation (Sc) satisfying: Sc=ΔHh/(ΔHl+ΔHh)×100>60 (wherein ΔHh represents the heat of fusion of stereocomplex crystals (J/g), and ΔHl represents the heat of fusion of crystals of poly-L-lactic acid alone and crystals of poly-D-lactic acid alone (J/g)); and subsequently subjecting the mixture to solid-phase polymerization at a temperature lower than the melting point of the mixture.

## Claims

### Claim at position 1

-13. (canceled)

### Claim 14

A method of producing a polylactic acid block copolymer comprising a segment(s) composed of L-lactic acid units and a segment(s) composed of D-lactic acid units, the method comprising:
obtaining a mixture by mixing poly-L-lactic acid and poly-D-lactic acid one of which has a weight average molecular weight of 60,000 to 300,000 and the other of which has a weight average molecular weight of 10,000 to 50,000, said mixture having a weight average molecular weight of not less than 90,000 and a degree of stereocomplexation (Sc) satisfying Inequality (1):
Sc=ΔHh/(ΔHl+ΔHh)×100>60 (1)
(wherein ΔHh represents heat of fusion of stereocomplex crystals (J/g), and ΔHl represents heat of fusion of crystals of poly-L-lactic acid alone and crystals of poly-D-lactic acid alone (J/g)); and
subsequently subjecting said mixture to solid-phase polymerization at a temperature lower than the melting point of said mixture.

### Claim 15

A method of producing a polylactic acid block copolymer, the method comprising:
obtaining a mixture by mixing poly-L-lactic acid and poly-D-lactic acid in which a ratio between weight average molecular weight of the polylactic acid having a higher weight average molecular weight and weight average molecular weight of the polylactic acid having a lower weight average molecular weight is not less than 2 and less than 30, said mixture having a weight average molecular weight of not less than 90,000 and a degree of stereocomplexation (Sc) satisfying Inequality (1):
Sc=ΔHh/(ΔHl+ΔHh)×100>60 (1)
(wherein ΔHh represents heat of fusion of stereocomplex crystals (J/g), and ΔHl represents heat of fusion of crystals of poly-L-lactic acid alone and crystals of poly-D-lactic acid alone (J/g)); and
subsequently subjecting said mixture to solid-phase polymerization at a temperature lower than the melting point of said mixture.

### Claim 16 (depends on 14)

The method according to claim 14, wherein one of said poly-L-lactic acid and said poly-D-lactic acid as raw materials has a weight average molecular weight of not less than 170,000 and the other has a weight average molecular weight of not less than 20,000.

### Claim 17 (depends on 14)

The method according to claim 14, wherein said mixture of poly-L-lactic acid and poly-D-lactic acid satisfies Inequality (2):
Sc=ΔHh/(ΔHl+ΔHh)×100>70 (2).

### Claim 18 (depends on 14)

The method according to claim 14, wherein the obtained polylactic acid block copolymer satisfies Inequality (3):
Sc=ΔHh/(ΔHl+ΔHh)×100>80 (3).

### Claim 19 (depends on 14)

The method according to claim 14, wherein, in DSC measurement of obtained polylactic acid block copolymer, the cooling crystallization temperature measured by increasing temperature of said polylactic acid block copolymer to 250° C. and keeping the temperature constant for 3 minutes, followed by decreasing the temperature at a cooling rate of 20° C./min. is not less than 130° C.

### Claim 20 (depends on 14)

The method according to claim 14, wherein polydispersity represented by a ratio between the weight average molecular weight and the number average molecular weight of the obtained polylactic acid block copolymer is not more than 2.7.

### Claim 21 (depends on 14)

The method according to claim 14, wherein a molded product comprising obtained polylactic acid block copolymer satisfies Inequality (4):
Relative degree of crystallinity=[(ΔHm−ΔHc)/ΔHm]×100>90 (4)
(wherein ΔHm represents melting enthalpy of crystals in a molded product (J/g), and ΔHc represents crystallization enthalpy of crystals in the molded product upon temperature increase (J/g)) and has a haze value of not more than 30% when thickness of said molded product is 100 μm.

### Claim 22 (depends on 14)

The method according to claim 14, wherein said mixture comprises a catalyst in an amount of 0.001 to 0.5 part by weight with respect to 100 parts by weight of said mixture.

### Claim 23 (depends on 22)

The method according to claim 22, wherein said catalyst contained in said mixture is at least one selected from the group consisting of tin compounds, titanium compounds, lead compounds, zinc compounds, cobalt compounds, iron compounds, lithium compounds, rare earth compounds and sulfonic acid compounds.

### Claim 24 (depends on 23)

The method according to claim 23, wherein said tin compounds are at least one selected from the group consisting of stannous acetate, stannous octoate, tin(II) chloride and tin(IV) chloride, and said sulfonic acid compounds are at least one selected from the group consisting of methanesulfonic acid, ethanesulfonic acid, propanesulfonic acid, propanedisulfonic acid, naphthalenedisulfonic acid and 2-aminoethanesulfonic acid.

### Claim 25 (depends on 14)

The method according to claim 14, wherein temperature during said solid-phase polymerization is increased stepwise or continuously.

### Claim 26 (depends on 14)

The method according to claim 14, wherein weight average molecular weight of the polylactic acid block copolymer is not less than 100,000.

### Claim 27 (depends on 15)

The method according to claim 15, wherein one of said poly-L-lactic acid and said poly-D-lactic acid as raw materials has a weight average molecular weight of not less than 170,000 and the other has a weight average molecular weight of not less than 20,000.

### Claim 28 (depends on 15)

The method according to claim 15, wherein said mixture of poly-L-lactic acid and poly-D-lactic acid satisfies Inequality (2):
Sc=ΔHh/(ΔHl+ΔHh)×100>70 (2).

### Claim 29 (depends on 16)

The method according to claim 16, wherein said mixture of poly-L-lactic acid and poly-D-lactic acid satisfies Inequality (2):
Sc=ΔHh/(ΔHl+ΔHh)×100>70 (2).

### Claim 30 (depends on 15)

The method according to claim 15, wherein the obtained polylactic acid block copolymer satisfies Inequality (3):
Sc=ΔHh/(ΔHl+ΔHh)×100>80 (3).

### Claim 31 (depends on 16)

The method according to claim 16, wherein the obtained polylactic acid block copolymer satisfies Inequality (3):
Sc=ΔHh/(ΔHl+ΔHh)×100>80 (3).

### Claim 32 (depends on 17)

The method according to claim 17, wherein the obtained polylactic acid block copolymer satisfies Inequality (3):
Sc=ΔHh/(ΔHl+ΔHh)×100>80 (3).