# US 2013/0158195 A1 · Delustrant Composed of Polyimide Powder, Polyimide Film Incorporating The Delustrant, and Manufacture Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0158195 A1
- Document ID: US20130158195A1
- Status: Published application
- Kind: A1
- Application number: 13/600,293
- Filed: 2012-08-31
- Published: 2013-06-20
- Earliest claimed: 2011-12-16
- Assignees: Taimide Technology Incorporation
- Inventors: Chung-Yi Chen; Sheng-Yu Huang; Wei-Dun Jhuang
- Web page: https://patentgrep.com/patent/US20130158195A1

## CPC

- C08J 5/18: Manufacture of films or sheets
- C08G 73/1046: {Polyimides containing oxygen in the form of ether bonds in the main chain}
- C09D 179/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08J 2379/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08J 2479/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A polyimide film with low gloss comprising a polyimide base polymer constituting the film, and a polyimide powder distributed in the film, the polyimide film having a 60° gloss value smaller or equal to about 50. The polyimide powder used as delustrant can have an average particle size between about 0.5 μm and about 15 μm. Embodiments described herein also include methods of preparing the polyimide film and the delustrant.

## Claims

### Claim 1

A polyimide film comprising:
a polyimide base polymer forming a main molecular structure of the film, the polyimide base polymer being obtained by reacting diamine with dianhydride components in substantially equal molar ratio; and
about 5 wt % to about 10 wt % of a polyimide powder distributed in the film;
wherein the film has a 60° gloss value less than or equal to about 50.

### Claim 2 (depends on 1)

The polyimide film according to claim 1, further comprising a color pigment.

### Claim 3 (depends on 2)

The polyimide film according to claim 2, wherein the color pigment has a weight ratio between about 2 wt % and about 10 wt % of the weight of the film.

### Claim 4 (depends on 2)

The polyimide film according to claim 2, wherein the color pigment is carbon black.

### Claim 5 (depends on 1)

The polyimide film according to claim 1, wherein the polyimide powder is obtained by reacting 4,4′-oxydianiline (4,4′-ODA) with pyromellitic dianhydride (PMDA).

### Claim 6 (depends on 5)

The polyimide film according to claim 5, wherein 4,4′-ODA and PMDA have a molar ratio of about 1:0.950 to 1:0.995.

### Claim 7 (depends on 1)

The polyimide film according to claim 1, wherein the polyimide powder has an average particle size between about 2 μm and about 10 μm.

### Claim 8

A method for preparing a polyimide film, comprising:
performing condensation polymerization of monomers including a diamine and a dianhydride to obtain a solution containing polyamic acid;
adding a polyimide powder into the solution;
adding a dehydrant and a catalyst into the solution to obtain a precursor solution;
coating a layer of the precursor solution on a support; and
baking the layer coated on the support to form a polyimide film;
wherein the polyimide powder is distributed in the polyimide film, and the film has a 60° gloss value less than or equal to about 50.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the polyimide powder is obtained by reacting 4,4′-oxydianiline (4,4′-ODA) with pyromellitic dianhydride (PMDA).

### Claim 10 (depends on 8)

The method according to claim 8, wherein the polyimide powder has an average particle size between about 2 μm and about 10 μm.

### Claim 11 (depends on 8)

The method according to claim 8, wherein the polyimide powder has a weight ratio between about 5 wt % and about 10 wt % of the weight of the film.

### Claim 12 (depends on 8)

The method according to claim 8, further comprising adding a color pigment into the solution containing the polyamic acid before coating a layer of the precursor solution on a support.

### Claim 13

A method of preparing a polyimide powder, comprising:
adding a diamine and a dianhydride at a molar ratio of about 1:0.950 to 1:0.995 into a solvent to obtain a reaction solution, wherein the sum of the diamine and the dianhydride has a weight ratio between about 2 wt % and about 20 wt % of the total weight of the reaction solution;
adding a dehydrant and a catalyst into the reaction solution to obtain a mixture; and
heating the mixture to obtain a precipitate of polyimide.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the diamine is 4,4′-oxydianiline (4,4′-ODA) and the dianhydride is pyromellitic dianhydride (PMDA).

### Claim 15 (depends on 13)

The method according to claim 13, wherein the total amount of the diamine and the dianhydride is between about 5 wt % and about 15 wt % of the total weight of the reaction solution.

### Claim 16 (depends on 13)

The method according to claim 13, further comprising rinsing, filtrating and drying the precipitate of polyimide.

### Claim 17

A polyimide powder having an average particle size between about 2 μm and about 10 μm, the polyimide powder being obtained by reacting 4,4′-oxydianiline (4,4′-ODA) with pyromellitic dianhydride (PMDA).